Sol-Gel Process and Its Application for Preparation of Metallic Oxide Powder and the Coating AITranslate
Abstract AITranslate
Three types of Sol-Gel methods used in manufacturing metallic oxides were analyzed in this paper: gelation Sol-Gel method, organo-metal polyment Gel method and organo-polymer Silica-Gel method,their suitable applications were also reviewed.The paper focused on the discussion on powder agglomeration and coating crack propagation during oxide ceramic manufacturing.
KeyWords AITranslate
1丁子上,翁文剑,杨娟.化学络合法在溶胶-凝胶过程中的应用[J].硅酸盐学报,1995,23(5):571-579. 被引量:38
2孙继红,范文浩,吴东,孙予罕.溶胶-凝胶(Sol-gel)化学及其应用[J].材料导报,2000,14(4):25-29. 被引量:45
3王歆,庄志强,齐雪君.金属氧化物溶胶-凝胶法制备技术及其应用[J].材料导报,2000,14(11):42-44. 被引量:16
1亢占英,陈文革,丁秉钧.溶胶-凝胶法制备纳米MoCu复合粉体[J].稀有金属材料与工程,2005,34(6):990-993. 被引量:4
2王静,冯玉杰.溶胶-凝胶法制备稀土Gd掺杂SnO_2电催化电极的实验研究[J].环境污染治理技术与设备,2005,6(7):19-24. 被引量:10
3余火根,余家国,郭瑞,赵修建.溶胶-凝胶薄膜的制备和应用[J].材料导报,2003,17(6):31-33. 被引量:29
1方俊,王秀峰.化学修饰溶胶-凝胶法制备功能薄膜微细图形[J].微细加工技术,2006(5):24-26.
2孙尚梅,赵莲花,康振晋,陈志彬.溶胶-凝胶技术及其在绿色无机合成化学与新型材料制备中的近期应用进展[J].延边大学学报:自然科学版,2005,31(1):42-48. 被引量:3
3抓住机遇 争取支持——上海市档案部门积极参与政府信息公开工作[J].中国档案,2005(9):18-19. 被引量:1
4沈毅,吴国友,张青龙,李真.超细WO_3粉体的制备现状及表征方法[J].光谱实验室,2005,22(6):1121-1126. 被引量:3
5方俊,杨万莉.溶胶-凝胶法制备ZnO:Al透明导电膜正交试验的灰色关联分析[J].江苏陶瓷,2006,39(3):27-29.
6郑国华,罗新乐.无支撑体SiO_2膜的制备及其表征[J].新疆大学学报:自然科学版,2006,23(4):437-440. 被引量:1
7于志伟,谈国强.溶胶-凝胶法制备薄膜[J].陶瓷,2006(10):39-42. 被引量:7
8刘文武,涂学炎,王伟,张世鸿,潘媛.两种DSA电极的制备及其对有机废水降解的电催化性能[J].环境化学,2007,26(2):152-156. 被引量:10
9胡静,吕凤婷,房喻.光学薄膜氧气传感器研究进展[J].化学研究与应用,2007,19(5):457-464. 被引量:7
10陈南春,韦翠美.溶胶-凝胶法制备纳米TiO_2薄膜[J].稀有金属材料与工程,2007,36(A01):973-976. 被引量:3
1罗电宏,马荣骏.对超细粉末团聚问题的探讨[J].湿法冶金,2002,21(2):57-61. 被引量:20
2姚敏琪,卫英慧,胡兰青,许并社.溶胶-凝胶法制备纳米粉体[J].稀有金属材料与工程,2002,31(5):325-329. 被引量:30
3黄坚.高纯铜加工方法综述[J].湖南有色金属,1996,12(6):36-39. 被引量:1
4曹瑞军,林晨光,孙兰,赵诣林,刘总,贾成厂.超细粉末的团聚及其消除方法[J].粉末冶金技术,2006,24(6):460-466. 被引量:21
5王东,阎圣刚,张爱丽,周科衍.二烯丙基硒的研制[J].低温与特气,1994,12(4):56-57.
6高杨,栾春晖,薛永强.改进的溶胶-凝胶法制备超细铜粉[J].太原理工大学学报,2000,31(3):271-273. 被引量:7
7范景莲,黄伯云,汪登龙.PCA对机械合金化纳米粉末的SEM结构与成分分布均匀性的影响[J].中国有色金属学报,2003,13(1):116-121. 被引量:11
8田庆华,王恒利,辛云涛,郭学益.臭氧在湿法冶金领域的研究进展[J].有色金属科学与工程,2014,5(6):8-13. 被引量:4
9范景莲,黄伯云,汪登龙.过程控制剂对机械合金化过程与粉末特征的影响[J].粉末冶金工业,2002,12(2):7-12. 被引量:23
10谈国强,苗鸿雁.氮化钛粉体制备及反应机理的研究[J].云南大学学报:自然科学版,2005,27(S3):414-417. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TF123[冶金工程—粉末冶金]
Citation Information:
Three types of Sol-Gel methods used in manufacturing metallic oxides were analyzed in this paper: gelation Sol-Gel method, organo-metal polyment Gel method and organo-polymer Silica-Gel method,their suitable applications were also reviewed.The paper focused on the discussion on powder agglomeration and coating crack propagation during oxide ceramic manufacturing.
quote
| GB/T 7714-2015 | [1] QIN Pei-yu, ZHOU Shi-quan. Sol-Gel Process and Its Application for Preparation of Metallic Oxide Powder and the Coating[J]. Rare Metals and Cemented Carbides, 2001(3): 30-33. |
| MLA | [1] QIN Pei-yu, and ZHOU Shi-quan. "Sol-Gel Process and Its Application for Preparation of Metallic Oxide Powder and the Coating." Rare Metals and Cemented Carbides, no. 3, 2001, pp. 30-33. |
| APA | [1] QIN Pei-yu, & ZHOU Shi-quan. (2001). Sol-Gel Process and Its Application for Preparation of Metallic Oxide Powder and the Coating. Rare Metals and Cemented Carbides(3), 30-33. |
| IEEE | [1] QIN Pei-yu and ZHOU Shi-quan, "Sol-Gel Process and Its Application for Preparation of Metallic Oxide Powder and the Coating," Rare Metals and Cemented Carbides, no. 3, pp. 30-33, 2001. keywords: {Sol-Gel method of metallic oxides;oxide ceramic;powder agglomeration;coating crackpropagatoin} |