Influence of Active Spheroidization Agent on the Morphology of Cobalt Oxalate AITranslate
Abstract AITranslate
Study is made of the influence of active spheroidization agent on the morphology of the cobalt oxalate.Analysis is made of the microstructures of industrial cobalt oxalate and spheroidial cobalt oxalate by X-diffractmeter and their morphology is observed under scanning eletron microscope.The experiment results showed addition of active spheroidization agent can result in distinct morphology change with better physical properties on the prerequisite of unchanged crystalline structure of the cobalt oxalate.
KeyWords AITranslate
1代云,徐远志,刁微之,左以专.氧化钴生产过程的非草酸盐沉钴工艺研究之一碳铵(反加)法自氯化钴溶液中沉钴[J].云南冶金,2007,36(3):32-36. 被引量:2
2罗崇玲,易茂中,谭兴龙.碳酸钴制备超细球形钴粉的工艺探讨[J].硬质合金,2007,24(2):84-87. 被引量:9
3刁微之,徐远志,代云,左以专.氧化钴生产过程的非草酸盐沉钴工艺研究之二 碳铵(反加)法自硫酸钴溶液中沉钴[J].云南冶金,2007,36(5):29-33. 被引量:3
4谭兴龙,易茂中,罗崇玲.球形钴粉的制备及其在超细晶粒硬质合金中的应用[J].中国有色金属学报,2008,18(2):209-214. 被引量:15
5张太全.分解还原法制备超细球形钴粉的过程机理[J].粉末冶金材料科学与工程,2010,15(6):593-596. 被引量:3
6邓莹,熊翔,邓玲,张艳华,涂铭旌.碳酸盐体系固相化学反应法制备纳米钴粉及其反应热力学[J].粉末冶金材料科学与工程,2014,19(2):205-210.
7高晋,王洪军.前驱物颗粒的形貌对钴粉形貌的影响[J].稀有金属与硬质合金,2002,30(2):15-18. 被引量:18
8刘诚.电池级氧化钴的研制[J].有色金属,2002,54(4):25-29. 被引量:20
1廖春发,梁勇,陈辉煌.由草酸钴热分解制备Co_3O_4及其物性表征[J].中国有色金属学报,2004,14(12):2131-2136. 被引量:16
2周健,宁顺明,习小明.电子级Co_3O_4制备方法及其进展[J].矿冶工程,2005,25(2):39-42. 被引量:5
3陈培荣,俞志敏.类球状Co_3O_4粉料的制备研究[J].新技术新工艺,2006(6):59-62.
4樊玉川.电池级Co_3O_4的制备[J].稀有金属,2006,30(3):282-286. 被引量:5
5肖劲,王剑锋,刘永东,李劼,刘业翔.Preparation of spherical cobalt carbonate powder with high tap density[J].中南工业大学学报:英文版,2006,13(6):642-646.
6曹钦存,张战营.沉淀法制备纳米Co_3O_4前驱体的研究[J].洛阳工业高等专科学校学报,2007,17(3):5-7. 被引量:1
7柳松,古国榜.微细氧化钴粉的研制[J].矿冶工程,2007,27(3):69-71. 被引量:4
8代云,徐远志,刁微之,左以专.氧化钴生产过程的非草酸盐沉钴工艺研究之一碳铵(反加)法自氯化钴溶液中沉钴[J].云南冶金,2007,36(3):32-36. 被引量:2
9罗崇玲,易茂中,谭兴龙.碳酸钴制备超细球形钴粉的工艺探讨[J].硬质合金,2007,24(2):84-87. 被引量:9
10刘宇慧,汪礼敏,张景怀.液相沉淀法制备超细Co_3O_4粉体的研究[J].粉末冶金工业,2007,17(4):14-18. 被引量:6
1梁志方,胡栋泉,陈丽萍.烧结矿中FeO含量测量中X衍射仪的应用[J].中国化工贸易,2013,5(4):263-263.
2高晋,王洪军.前驱物颗粒的形貌对钴粉形貌的影响[J].稀有金属与硬质合金,2002,30(2):15-18. 被引量:18
3陈喜平,李旺兴.废槽衬的性能研究[J].有色金属:冶炼部分,2003(6):35-37. 被引量:4
4E.Keulen,Almelo,薛福庭.工业X射线衍射仪在铝厂的应用[J].轻金属,1993(11):40-41.
5屈广林,颜练武,张卫兵,何惧.碳化钨和碳化钒在固相钴中的固溶研究[J].硬质合金,2014,31(1):8-14. 被引量:6
6王梅生,张琼,姜继森.α-Fe_2O_3的晶粒度与晶格畸变的测定[J].应用科学学报,1994,12(3):307-310.
7张鹏,赖桂华,衷水平,张兴勋,康锦程,伍赠玲,王韬.高电流密度电积技术在铜冶炼厂的现场应用[J].湿法冶金,2017,36(2):148-150. 被引量:4
8谢建军,韩秀丽,鲍彦丽,高永会,冯帅.MnO_2对高炉喷吹煤粉助燃机制的研究[J].中国冶金,2013,23(11):16-20. 被引量:2
9黄有国,李庆余,王红强.低温电解质熔体中NiFe_2O_4基惰性阳极电解腐蚀初探[J].有色冶金设计与研究,2010,31(4):7-9.
10李文化,李彩珍,郭晋梅.砂状氧化铝比表面积的测定[J].世界有色金属,2006(5):22-23.
Basic Information:
DOI:
Chinese Library Classification Number:TF123.24[冶金工程—粉末冶金];TF125.3[冶金工程—粉末冶金]
Citation Information:
Study is made of the influence of active spheroidization agent on the morphology of the cobalt oxalate.Analysis is made of the microstructures of industrial cobalt oxalate and spheroidial cobalt oxalate by X-diffractmeter and their morphology is observed under scanning eletron microscope.The experiment results showed addition of active spheroidization agent can result in distinct morphology change with better physical properties on the prerequisite of unchanged crystalline structure of the cobalt oxalate.
quote
| GB/T 7714-2015 | [1] GAO Jin, CHEN Qing-lin. Influence of Active Spheroidization Agent on the Morphology of Cobalt Oxalate[J]. Rare Metals and Cemented Carbides, 2001(3): 20-22. |
| MLA | [1] GAO Jin, and CHEN Qing-lin. "Influence of Active Spheroidization Agent on the Morphology of Cobalt Oxalate." Rare Metals and Cemented Carbides, no. 3, 2001, pp. 20-22. |
| APA | [1] GAO Jin, & CHEN Qing-lin. (2001). Influence of Active Spheroidization Agent on the Morphology of Cobalt Oxalate. Rare Metals and Cemented Carbides(3), 20-22. |
| IEEE | [1] GAO Jin and CHEN Qing-lin, "Influence of Active Spheroidization Agent on the Morphology of Cobalt Oxalate," Rare Metals and Cemented Carbides, no. 3, pp. 20-22, 2001. keywords: {active spheroidization agent;cobalt oxalate;morphology} |