Catalytic Synthesis of DOP,DOM and DOA with Ln_2O_3/ZrO_2 Catalyst AITranslate
Abstract AITranslate
The catalytic synthesis of DOP,DOM and DOA with catalyst Ln 2O 3/ZrO 2 (Ln=Nd,Sm,Er),prepared by coprecipitation-calcination method,has resulted in distinct efficiency improvement and due to its larger specific surface area and better dispersion by~60% less carrier Ln 2O 3 consumption compared with pure Ln 2O 3.
KeyWords AITranslate
1陈其瑞,张凤美,罗明润,焦肇林.Ln_2O_3/Al_2O_3催化酯化合成邻苯二甲酸二辛酯[J].催化学报(英文),1994,15(3):236-238. 被引量:20
2陈其瑞,焦肇林,罗明润,潘慧芳.混合镨钕氧化物作为酯化催化剂的研究[J].稀土,1990,11(5):66-68. 被引量:13
3陈其瑞,孟菁,张凤美,焦肇林.内增塑剂DOM制备方法的改进[J].化学试剂,1995,17(3):187-188. 被引量:5
4陈其瑞,邵明霞.Ln_2O_3/X-13分子筛作酯化反应催化剂的研究[J].稀有金属与硬质合金,1997,25(4):11-14. 被引量:3
5陈其瑞.Ln_2O_3/Al_2O_3催化合成内增塑剂DOM[J].稀有金属与硬质合金,1999,27(4):24-26. 被引量:1
6廖世军,杨兆禧,张小玲,刘莹,王乐夫,黄仲涛.SO_4^(2-)/ZrO_2-SiO_2催化剂的制备及其对乙酸/丁醇酯化反应的催化作用[J].分子催化,1998,12(1):53-58. 被引量:43
1陈其瑞.Ln_2O_3/MgO催化合成增塑剂IOP的研究[J].稀有金属与硬质合金,2003,31(4):16-17.
1陈其瑞.Ln_2O_3/Al_2O_3催化合成内增塑剂DOM[J].稀有金属与硬质合金,1999,27(4):24-26. 被引量:1
2陈其瑞,邵明霞.Ln_2O_3/MgO(Ln=Nd、Sm、Er)催化合成DOP、DOM和DOA[J].稀土,1998,19(4):8-10. 被引量:3
3关玉德.制备催化剂的新方法——醇盐法[J].天然气化工—C1化学与化工,1993,18(4):39-41. 被引量:2
4吕布,吴培云.Ln_2O_3/x-13分子筛担载型催化剂在合成DOP中的催化活性[J].安徽化工,2000,26(2):21-22.
5芳族尿烷在担载钌催化剂的存在下的氢化[J].精细化工原料及中间体,2005(1):42-42.
6姚楠,熊国兴,杨维慎,何鸣元.硅铝催化材料合成的新进展[J].化学进展,2000,12(4):376-384. 被引量:9
7孟玲,徐淑娟,桂玉梅.高岭土细粉原位晶化合成NaY分子筛[J].中国西部科技,2012,11(8):13-15. 被引量:3
8戈军,石斌,郭龙德,郭智慧,田华,张建芳.同步溶胀-担载催化剂对烟煤-重油共炼的影响[J].煤炭转化,2011,34(3):1-6.
9徐龙伢,王清遐,林励吾,梁东白,徐奕德.CO_2加氢制低碳烯烃Fe/Silicalite-2催化剂研究 Ⅲ.K-Fe-MnO/Silicalite-2催化剂性能考察[J].天然气化工—C1化学与化工,1997,22(4):14-17. 被引量:5
10康瑞雪,张志芳,尹文梅,王爱娣,马国富.AlPO_4-5负载溴化铝催化酮的Baeyer-Villiger氧化反应[J].精细化工,2012,29(10):942-946.
Basic Information:
DOI:
Chinese Library Classification Number:TQ414[化学工程];TQ320.4[化学工程—合成树脂塑料工业]
Citation Information:
The catalytic synthesis of DOP,DOM and DOA with catalyst Ln 2O 3/ZrO 2 (Ln=Nd,Sm,Er),prepared by coprecipitation-calcination method,has resulted in distinct efficiency improvement and due to its larger specific surface area and better dispersion by~60% less carrier Ln 2O 3 consumption compared with pure Ln 2O 3.
quote
| GB/T 7714-2015 | [1] CHEN Qi-rui, SHAO Ming-xia. Catalytic Synthesis of DOP,DOM and DOA with Ln_2O_3/ZrO_2 Catalyst[J]. Rare Metals and Cemented Carbides, 2001(3): 23-26. |
| MLA | [1] CHEN Qi-rui, and SHAO Ming-xia. "Catalytic Synthesis of DOP,DOM and DOA with Ln_2O_3/ZrO_2 Catalyst." Rare Metals and Cemented Carbides, no. 3, 2001, pp. 23-26. |
| APA | [1] CHEN Qi-rui, & SHAO Ming-xia. (2001). Catalytic Synthesis of DOP,DOM and DOA with Ln_2O_3/ZrO_2 Catalyst. Rare Metals and Cemented Carbides(3), 23-26. |
| IEEE | [1] CHEN Qi-rui and SHAO Ming-xia, "Catalytic Synthesis of DOP,DOM and DOA with Ln_2O_3/ZrO_2 Catalyst," Rare Metals and Cemented Carbides, no. 3, pp. 23-26, 2001. keywords: {rare earth oxides;supported catalyst;catalytic esterification} |