Boost VS2 electrochemical reactive kinetics by regulating crystallographic planes and coupling carbon matrix for high performance sodium-ion storage AITranslate
Abstract AITranslate
Vanadium disulfide(VS2) as a typical two-dimensional transition metal chalcogenide has excellent competitiveness for sodium-ion storage due to its wide layer spacing(0.575 nm),high theoretical capacity of 932mAh·g-1 originating from multi-electron electrochemical redox.However,continuous sodiation process accompanied by crystal structural evolution and collapse cause rapid capacity decaying.Herein,novel few-layer VS2nanosheets with open(001) crystal planes are in-situ constructed on reduced graphene oxide to solve these issues mentioned above.It indicates that few-layer VS2provides more Na+ storage activity due to the low Na+surface migration energy barrier on exposed crystal(001)planes.The flexible and high electronic conductivity of carbon matrix also effectively builds multi-level buffer structure and electron transport kinetics to boost the Na+insertion/conversion reactive activity on VS2 as well as Na+ pseudocapacitance storage kinetics on edges and defects of nano sheets.Those coupling effects result in high rate capability and long cycling stability as a battery/capacitor anode.It delivers conspicuous high energy density of 81 and 40 Wh·kg-1 at power density of 118 and 10,286W·kg-1,as well as 80% energy retention rate after 5000cycles,confirming its great application potential in sodiumbased storage devices.
KeyWords AITranslate
1Yan-Fang Zhu,Yao Xiao,Shi-Xue Dou,Yong-Mook Kang,Shu-Lei Chou.Spinel/Post-spinel engineering on layered oxide cathodes for sodium-ion batteries[J].eScience,2021,1(1):13-27. 被引量:17
2Mou-Ping Fan,You-Chen Chen,Yuan-Mao Chen,Ze-Xi Huang,Wen-Li Wu,Pan Wang,Xi Ke,Shu-Hui Sun,Zhi-Cong Shi.NiS_(2) nanosheet arrays on stainless steel foil as binder-free anode for high-power sodium-ion batteries[J].Rare Metals,2022,41(4):1294-1303. 被引量:3
3K.Ramachandran,Gokila Subburam,Xian-Hu Liu,Ming-Gang Huang,Chun Xu,Dickon H.L.Ng,Ying-Xue Cui,Guo-Chun Li,Jing-Xia Qiu,Chuan Wang,Jia-Biao Lian.Nitrogen-doped porous carbon nanofoams with enhanced electrochemical kinetics for superior sodium-ion capacitor[J].Rare Metals,2022,41(7):2481-2490. 被引量:3
4Hong-Yan Liang,Zhi-Wen Zhang,Xiao-Bin Zhong,Yao-Hui Zhang,Meng-Yao Tang,Shu-Xian Li,Huan-Huan Zhang,Peng-Fei Hu,Jun-Fei Liang.Scalable synthesis of mesoporous FeS_(2) nanorods as highperformance anode materials for sodium-ion batteries[J].Rare Metals,2022,41(1):21-28. 被引量:4
5Xiaosa Xu,Fei Xu,Xiuhai Zhang,Changzhen Qu,Jinbo Zhang,Yuqian Qiu,Rong Zhuang,Hongqiang Wang.Laser-Derived Interfacial Confinement Enables Planar Growth of 2D SnS_(2) on Graphene for High-Flux Electron/Ion Bridging in Sodium Storage[J].Nano-Micro Letters,2022,14(6):65-80. 被引量:1
6Wen-Bei Yu,Zhi-Yi Hu,Jun Jin,Min Yi,Min Yan,Yu Li,Hong-En Wang,Huan-Xin Gao,Li-Qiang Mai,Tawfique Hasan,Bai-Xiang Xu,Dong-Liang Peng,Gustaaf Van Tendeloo,Bao-Lian Su.Unprecedented and highly stable lithium storage capacity of(001)faceted nanosheet-constructed hierarchically porous TiO2/rGO hybrid architecture for high-performance Li-ion batteries[J].National Science Review,2020,7(6):1046-1058. 被引量:2
7Daxiong Wu,Caiyun Wang,Mingguang Wu,Yunfeng Chao,Pengbin He,Jianmin Ma.Porous bowl-shaped VS2 nanosheets/graphene composite for high-rate lithium-ion storage[J].Journal of Energy Chemistry,2020,29(4):24-32. 被引量:13
8Fengyi He,Cheng Tang,Guanjia Zhu,Yadong Liu,Aijun Du,Qiaobao Zhang,Minghong Wu,Haijiao Zhang.Leaf-inspired design of mesoporous Sb_(2)S_(3)/N-doped Ti_(3)C_(2)T_(x) composite towards fast sodium storage[J].Science China Chemistry,2021,64(6):964-973. 被引量:5
1Longsheng Zhong,Hongneng Chen,Yanzhe Sheng,Yiting Sun,Yanhe Xiao,Baochang Cheng,Shuijin Lei.Two-dimensional layered In_(2)P_(3)S_(9): A novel superior anode material for sodium-ion batteries[J].Journal of Energy Chemistry,2024,90(3):294-304.
2Jianhua PAN,Luxin Li.Third-order unconditional positivity-preserving schemes for reactive flows keeping both mass and mole balance[J].Chinese Journal of Aeronautics,2023,36(11):24-41.
3Yi Zhang,Zhen Zhang,Sheng Yu,Hannah M.Johnson,De-Cheng Zhao,Su-Chong Tan,Zheng-Dao Pan,Zhou-Lu Wang,Yu-Tong Wu,Xiang Liu.Three-dimensional nanostructured Co_(2)VO_(4)-decorated carbon nanotubes for sodium-ion battery anode materials[J].Rare Metals,2023,42(12):4060-4069.
4Chen Zhu,Yanfeng Shi,Jing Yu,Wenhao Zhao,Lingqiao Li,Jingxi Liang,Xiaolin Yang,Bing Zhang,Yao Zhao,Yan Gao,Xiaobo Chen,Xiuna Yang,Lu Zhang,Luke W.Guddat,Lei Liu,Haitao Yang,Zihe Rao,Jun Li.Cryo-EM structures of a prokaryotic heme transporter CydDC[J].Protein & Cell,2023,14(12):919-923.
5Xiaofeng He,Xiang-Yu Kong,Liping Wen.A promising solution for highly reversible zinc metal anode chemistry:Functional gradient interphase[J].Nano Research Energy,2024,3(2):3-6.
6Sukanya Pothaya,Chatwarin Poochai,Nantikan Tammanoon,Yaowamarn Chuminjak,Tanaporn Kongthong,Tanom Lomas,Chakrit Sriprachuabwong,Adisorn Tuantranont.Bamboo-derived hard carbon/carbon nanotube composites as anode material for long-life sodium-ion batteries with high charge/discharge capacities[J].Rare Metals,2024,43(1):124-137. 被引量:1
7Baixin Peng,Tianxun Cai,Shaoning Zhang,Yuqiang Fang,Zhuoran Lv,Yusha Gao,Fuqiang Huang.Unlocking efficient energy storage via regulating ion and electron-active subunits:an(SbS)_(1.15)TiS_(2)superlattice for large and fast Na^(+)storage[J].Science China Chemistry,2024,67(1):336-342.
8Fengyang Jing,Chade Lv,Liangliang Xu,Yaru Shang,Jian Pei,Pin Song,Yuanheng Wang,Gang Chen,Chunshuang Yan.An amorphous manganese iron oxide hollow nanocube cathode for aqueous zinc ion batteries[J].Journal of Energy Chemistry,2023(12):314-321.
9Tufail Mustafa,Yongping Liu,Jie Gao,Peng Yan,Qi Ding,Yuchi Fan,Wan Jiang.Highly aligned reduced graphene oxide in alumina composites for strengthening,toughening,and electromagnetic interference shielding[J].Journal of Materiomics,2023,9(6):993-1003.
10Tao Jin,Long Yang,Xinyue Zhang,Wen Li,Yanzhong Pei.Close-packed layer spacing as a practical guideline for structure symmetry manipulation of IV-VI/I-V-VI_(2) thermoelectrics[J].InfoMat,2024,6(2):99-106.
Basic Information:
DOI:
Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动];TM53[电气工程—电器];O643.1[理学—物理化学]
Citation Information:
Vanadium disulfide(VS2) as a typical two-dimensional transition metal chalcogenide has excellent competitiveness for sodium-ion storage due to its wide layer spacing(0.575 nm),high theoretical capacity of 932mAh·g-1 originating from multi-electron electrochemical redox.However,continuous sodiation process accompanied by crystal structural evolution and collapse cause rapid capacity decaying.Herein,novel few-layer VS2nanosheets with open(001) crystal planes are in-situ constructed on reduced graphene oxide to solve these issues mentioned above.It indicates that few-layer VS2provides more Na+ storage activity due to the low Na+surface migration energy barrier on exposed crystal(001)planes.The flexible and high electronic conductivity of carbon matrix also effectively builds multi-level buffer structure and electron transport kinetics to boost the Na+insertion/conversion reactive activity on VS2 as well as Na+ pseudocapacitance storage kinetics on edges and defects of nano sheets.Those coupling effects result in high rate capability and long cycling stability as a battery/capacitor anode.It delivers conspicuous high energy density of 81 and 40 Wh·kg-1 at power density of 118 and 10,286W·kg-1,as well as 80% energy retention rate after 5000cycles,confirming its great application potential in sodiumbased storage devices.
quote
| GB/T 7714-2015 | [1] Min Zeng, Ming-Shan Wang, Lin Chen, et al. Rare Metals, 2024(1): 98-112. |
| MLA | [1] Min Zeng, et al., Rare Metals, no. 1, 2024, pp. 98-112. |
| APA | [1] Min Zeng, Ming-Shan Wang, Lin Chen, En-Zhi Li, Zhen-Liang Yang, Dan Zhou, Hai-Jiao Xie, Jun-Chen Chen, Zhi-Yuan Ma, Bing-Shu Guo, Bo Yu, & Xing Li. (2024). Rare Metals(1), 98-112. |
| IEEE | [1] Min Zeng, Ming-Shan Wang, Lin Chen, En-Zhi Li, Zhen-Liang Yang, Dan Zhou, Hai-Jiao Xie, Jun-Chen Chen, Zhi-Yuan Ma, Bing-Shu Guo, Bo Yu, and Xing Li, Rare Metals, no. 1, pp. 98-112, 2024. |