Simultaneously enhanced electrochemical performance and air stability of Ni-rich cathode with a modified washing process AITranslate
Abstract AITranslate
Water washing has been regarded as one of the most effective strategies to remove surface residual lithium of nickel-rich layered oxides for lithium-ion batteries(LIBs).However,the loss of lattice lithium during the water washing process deteriorates the electrochemical performances and air stability.Herein,washing the LiNi0.90Co0.05Al0.02O2(NCA) with ammonium dihydrogen phosphate(NH4H2PO4) solution has been proposed to simultaneously enhance electrochemical performances and air stability,in which in-situ generated Li3PO4 coating layer on surface of NCA can suppress the loss of lattice lithium.Besides,as a fast ionic conductor,Li3PO4 coating layer on NCA can prevent the direct contact with electrolyte/air.As a result,the NH4H2PO4 solution washed NCA cathode can deliver a high capacity of131.9 mAh·g-1 at 10.0C rate as well as impressive cycle stability with a capacity retention of 83.1% after 100 cycles at 1.0C,much higher than those of water washed NCA(WS-NCA) electrode.After exposed in air for 7 days,the NH4H2PO4 solution washed NCA electrode can more effectively maintain the structural integrity as well as the electrochemical performances than water-washed NCA.This work provides a simple and effective approach to enhance the cycle stability and air stability of Nickel-rich cathode materials.
KeyWords AITranslate
1Xiaobo Ding,Huiying Huang,Qianhui Huang,Benrui Hu,Xiaokang Li,Xiangdong Ma,Xunhui Xiong.Doping sites modulation of T-Nb_(2)O_(5) to achieve ultrafast lithium storage[J].Journal of Energy Chemistry,2023(2):280-289. 被引量:1
2吴锋,李晴,陈来,王紫润,陈刚,包丽颖,卢赟,陈实,苏岳锋.高镍正极材料中钴元素的替代方案及其合成工艺优化[J].物理化学学报,2022,38(5):60-69. 被引量:7
3Xiao-Feng Zhu,Xiu Li,Tian-Quan Liang,Xin-Hua Liu,Jian-Min Ma.Electrolyte perspective on stabilizing LiNi_(0.8)Co_(0.1)Mn_(0.1)O_(2)cathode for lithium-ion batteries[J].Rare Metals,2023,42(2):387-398. 被引量:4
4Tian-Yi Zeng,Xiao-Yun Zhang,Xing-Yu Qu,Mei-Qing Li,Pan-Pan Zhang,Ming-Ru Su,Ai-Chun Dou,Ahmad Naveed,Yu Zhou,Yun-Jian Liu.Mechanism exploration of enhanced electrochemical performance of single-crystal versus polycrystalline LiNi_(0.8)Mn_(0.1)Co_(0.1)O_(2)[J].Rare Metals,2022,41(11):3783-3794. 被引量:3
5Zi-Wei Lan,Jian-Ru Zhang,Yuan-Yuan Li,Ru-Heng Xi,Yong-Xiang Yuan,Lei Zhao,Xiao-Yi Hou,Jia-Tai Wang,Dickon H.L.Ng,Cai-Hong Zhang.LiFePO_(4)and LiMn_(2)O_(4)nanocomposite coating of LiNi_(0.815)Co_(0.15)Al_(0.035)O_(2)cathode material for high-performance lithium-ion battery[J].Rare Metals,2022,41(8):2560-2566. 被引量:2
6Chu Wang,Lei Tan,Hongling Yi,Zixiang Zhao,Xiaoli Yi,Youyuan Zhou,Junchao Zheng,Jiexi Wang,Lingjun Li.Unveiling the impact of residual Li conversion and cation ordering on electrochemical performance of Co-free Ni-rich cathodes[J].Nano Research,2022,15(10):9038-9046. 被引量:3
1Yuchuan Feng,Minghui Wang,Lina Gao,Zhaoling He,Kai Chen,Zheng Li,Hongcai He,Yuanhua Lin.Novel fast ionic conductor ceramic composite separator for highperformance safe Li-ion power batteries[J].Journal of Materiomics,2022,8(6):1184-1190.
2Huanhuan Jia,Linfeng Peng,Zhuoran Zhang,Tao An,Jia Xie.Na3.8[Sn0.67Si0.33]0.8Sb0.2S4:A quinary sodium fast ionic conductor for all-solid-state sodium battery[J].Journal of Energy Chemistry,2020,29(9):102-106. 被引量:1
3Yang Hua,Wei Bai,Sheng Wang,Yunbo Wu,Shengtao Cui,Zhe Sun,Chong Xiao.Tuning the electric transport behavior of AgCrSe_(2) by intrinsic defects[J].Science China Chemistry,2021,64(11):1970-1975.
4EFFECT OF DISPERSED PHASE PARTICLES ON ELECTRICAL CONDUCTION OF PEO-NaSCN[J].Chemical Research in Chinese Universities,1986,4(1):97-101.
5Yibo Deng,Xiaoguang Xu,Lu Zhang,Fei Du,Qi Liu,Jikun Chen,Kangkang Meng,Yong Wu,Ming Yang,Yong Jiang.Lithium incorporation enhanced resistive switching behaviors in lithium lanthanum titanium oxide-based heterostructure[J].Journal of Materials Science & Technology,2022(33):142-147.
6Pengfei Li,Takayuki Shimaoka.Assessing the Metal Recovery Value of Municipal Solid Waste Incineration Residues: Impact of Pretreatment on Fly Ash and Bottom Ash[J].Journal of Geoscience and Environment Protection,2023,11(10):79-86.
7Haibo Xu,Qingmei Lu,Lichao Yu,Liying Cong,Haowen Tian,Weiqiang Liu,Youhao Liu,Yunqiao Wang,Jingwu Chen,Xiaofei Yi,Qiong Wu,Ming Yue.A facile process to optimize performance of regenerated Nd-Fe-B sintered magnets:Chemo-selective dissolution washing[J].Journal of Rare Earths,2023,41(12):1976-1983.
8Shi-Ju Chen,Da-Ya Zhang,Xia Wu,Fa-Ming Zhang,Bo-Ta Cui,Yi-Hao Huang,Zu-Lun Zhang,Rui Wang,Fei-Hu Bai.Washed microbiota transplantation for Crohn’s disease:A metagenomic,metatranscriptomic,and metabolomic-based study[J].World Journal of Gastroenterology,2024,30(11):1572-1587.
9Zheng Bo,Qian Jianguo,Shi Peng,Pan Zhiyong,Qie Siyuan,Zhang Yueqin,Fei Jianqi,Qiao Liang,Zong Baoning.Pilot Test of Preparing 2-Alkylanthraquinone Using Alkylation-Oxidation Technology[J].China Petroleum Processing & Petrochemical Technology,2024,26(1):88-97.
10Xi Wang,Asif Hussain,Qingqing Li,Mingyu Ma,Juan Wu,Mingqiang Deng,Jie Yang,Dengxin Li.Core-shell design of UiO66-Fe_(3)O_(4) configured with EDTA-assisted washing for rapid adsorption and simple recovery of heavy metal pollutants from soil[J].Journal of Environmental Sciences,2024(5):556-568. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动]
Citation Information:
Water washing has been regarded as one of the most effective strategies to remove surface residual lithium of nickel-rich layered oxides for lithium-ion batteries(LIBs).However,the loss of lattice lithium during the water washing process deteriorates the electrochemical performances and air stability.Herein,washing the LiNi0.90Co0.05Al0.02O2(NCA) with ammonium dihydrogen phosphate(NH4H2PO4) solution has been proposed to simultaneously enhance electrochemical performances and air stability,in which in-situ generated Li3PO4 coating layer on surface of NCA can suppress the loss of lattice lithium.Besides,as a fast ionic conductor,Li3PO4 coating layer on NCA can prevent the direct contact with electrolyte/air.As a result,the NH4H2PO4 solution washed NCA cathode can deliver a high capacity of131.9 mAh·g-1 at 10.0C rate as well as impressive cycle stability with a capacity retention of 83.1% after 100 cycles at 1.0C,much higher than those of water washed NCA(WS-NCA) electrode.After exposed in air for 7 days,the NH4H2PO4 solution washed NCA electrode can more effectively maintain the structural integrity as well as the electrochemical performances than water-washed NCA.This work provides a simple and effective approach to enhance the cycle stability and air stability of Nickel-rich cathode materials.
quote
| GB/T 7714-2015 | [1] Ben-Rui Hu, Ying-Yi Yuan, Yu-Cheng Wang, et al. Rare Metals, 2024(1): 87-97. |
| MLA | [1] Ben-Rui Hu, et al., Rare Metals, no. 1, 2024, pp. 87-97. |
| APA | [1] Ben-Rui Hu, Ying-Yi Yuan, Yu-Cheng Wang, & Xun-Hui Xiong. (2024). Rare Metals(1), 87-97. |
| IEEE | [1] Ben-Rui Hu, Ying-Yi Yuan, Yu-Cheng Wang, and Xun-Hui Xiong, Rare Metals, no. 1, pp. 87-97, 2024. |