Electrochemical reconstruction: a new perspective on Sn metal-organic complex microbelts as robust anode for lithium storage AITranslate
Abstract AITranslate
Tin-based materials with high theoretical capacity and suitable working voltage are ideal anode materials for lithium-ion batteries(LIBs). However, to overcome their shortcomings(volume expansion and inferior stability), the preparation processes are usually complicated and expensive. Herein, a tin-based metal-organic complex(tin 1,2-benzenedicarboxylic acid, Sn-BDC)with one-dimensional microbelt morphology is synthesized by a facile, rapid and low-cost co-precipitation method, and served as anode material for LIBs without any post-treatment. Sn-BDC exhibits a high reversible capacity with609/440 m Ah·g-1 at 50/2000 m A·g-1, and robust cycling stability of 856 m Ah·g-1 after 200 cycles at 200 m A·g-1,which are obviously superior to that of the Sn Ox/C counterparts. Moreover, an electrochemical reconstruction perspective on the lithium storage mechanism of Sn-BDC is proposed by systematic ex-situ characterizations. The reconstructed SnO2 replaces Sn-BDC and becomes the active material in the subsequent cycles. As the by-product of the lithiation reaction, the formed Li-based metal-organic complex(Li-BDC, wrapped around the reconstructed SnO2) plays an important role in alleviating volume expansion and accelerating the charge transfer kinetics.This work is beneficial to design and construct the new electrode materials based on the electrochemical reconstruction for advanced LIBs.
KeyWords AITranslate
1文刚,谭亮,兰雪侠,张涵茵,胡仁宗,袁斌,刘军,朱敏.Li_(2)CO_(3)诱导生长稳定SEI膜:提升SnO_(2)储锂可逆性和稳定性的有效策略[J].Science China Materials,2021,64(11):2683-2696. 被引量:1
2Pan Deng,Jing Yang,Shengyang Li,Tian-E Fan,Hong-Hui Wu,Yun Mou,Hui Huang,Qiaobao Zhang,Dong-Liang Peng,Baihua Qu.High Initial Reversible Capacity and Long Life of Ternary SnO_(2)-Co-carbon Nanocomposite Anodes for Lithium-Ion Batteries[J].Nano-Micro Letters,2019,11(1):326-338. 被引量:3
3Ting-Ting Wei,Panpan Peng,Yu-Rui Ji,Yan-Rong Zhu,Ting-Feng Yi,Ying Xie.Rational construction and decoration of Li_(5)Cr_(7)Ti_(6)O_(25)@Cnanofibers as stable lithium storage materials[J].Journal of Energy Chemistry,2022,31(8):400-410. 被引量:5
4伊廷锋,仇立英,梅杰,齐思雨,崔平,罗绍华,朱彦荣,谢颖,贺艳兵.纳米结构的多孔球形NiO@NiMoO4@PPy作为先进的电化学赝电容器材料[J].Science Bulletin,2020,65(7):546-556. 被引量:6
5Xue-Zhong Li,Nan Zhang,Yu-Rong Wu,Qin-Zhi Lai,Yan-Rong Zhu,Jun-Hong Zhang,Ping Cui,Ting-Feng Yi.Interconnected Bi_(5)Nb_(3)O_(15)@CNTs network as high-performance anode materials of Li-ion battery[J].Rare Metals,2022,41(10):3401-3411. 被引量:3
6Su Hyun Yang,Seung‑Keun Park,Yun Chan Kang.MOF‑Derived CoSe2@N‑Doped Carbon Matrix Confined in Hollow Mesoporous Carbon Nanospheres as High‑Performance Anodes for Potassium‑Ion Batteries[J].Nano-Micro Letters,2021,13(1):123-137. 被引量:6
7Huan Liu,Xin Zhang,Yifan Zhu,Bin Cao,Qizhen Zhu,Peng Zhang,Bin Xu,Feng Wu,Renjie Chen.Electrostatic Self-assembly of 0D–2D SnO_(2) Quantum Dots/Ti_(3)C_(2)T_(x) MXene Hybrids as Anode for Lithium-Ion Batteries[J].Nano-Micro Letters,2019,11(4):161-172. 被引量:14
8Hongyi Xu,Chengxin Peng,Yuhua Yan,Fei Dong,Hao Sun,Junhe Yang,Shiyou Zheng.“All‐In‐One” integrated ultrathin SnS2@3D multichannel carbon matrix power high‐areal–capacity lithium battery anode[J].Carbon Energy,2019,1(2):276-288. 被引量:5
9Jian-Guo Zhao,Hong-Yan Zhou,Zhuan Hu,Ya-Wen Wu,Hong Jia,Xian-Ming Liu.Sn-MOFs/G composite materials for long cycling performance lithium ion batteries[J].Rare Metals,2022,41(5):1504-1511. 被引量:1
10Guan-Li Xu,Yu-Dong Gong,Chang Miao,Qing Wang,Shu-Qing Nie,Yu Xin,Min-Yue Wen,Jian Liu,Wei Xiao.Sn nanoparticles embedded into porous hydrogel-derived pyrolytic carbon as composite anode materials for lithium-ion batteries[J].Rare Metals,2022,41(10):3421-3431. 被引量:3
1Shuqing Nie,Yu Xin,Qiuyun Wang,Chengjin Liu,Chang Miao,Limin Yu,Wei Xiao.Three-dimensional structural Cu^(6)Sn_(5)/carbon nanotubes alloy thin-film electrodes fabricated by in situ electrodeposition from the leaching solution of waste-printed circuit boards[J].International Journal of Minerals,Metallurgy and Materials,2023,30(6):1171-1180.
2Lianyu Zhao,Yishan Wang,Chuncheng Wei,Xiaoxiao Huang,Xueqian Zhang,Guangwu Wena.MoS2-based anode materials for lithium-ion batteries:Developments and perspectives[J].Particuology,2024,87(4):240-270.
3Kaisi Liu,Jiabin Wu,Qun Li,Hongrun Jin,Yongxin Luo,Bei Qi,Simin Dai,Jianquan Zhao,Liang Huang,Jun Zhou.Molten metal-organic complex to synthesize versatile ultrathin nonlayered oxides[J].Nano Research,2024,17(4):3147-3155. 被引量:1
4Qiao Cu,Chao-Qun Shang,Guo-Fu Zhou,Xin Wang.Freestanding MoSe_(2)nanoflowers for superior Li/Na storage properties[J].Tungsten,2024,6(1):238-247.
5Yajie Han,Shujie Jiao,Jiangcheng Jing,Lei Chen,Ping Rong,Shuai Ren,Dongbo Wang,Shiyong Gao,Jinzhong Wang.A self-powered solar-blind UV-enhanced Bi_(2)Se_(3)/a-Ga_(2)O_(3)/p-Si heterojunction photodetector for full spectral photoresponse and imaging[J].Nano Research,2024,17(4):2960-2970.
6Jing-Sheng Ma,Ming-Zai Wu,Ling Chen,Li-Xing Zhang,Ying Xiong.Nitrogen–sulfur co-doped porous carbon derived from asphalt as efficient catalyst for oxygen reduction[J].Rare Metals,2024,43(1):380-388.
7Lin Yang,Zhong Zhang,Chao-Nan Zhang,Xiu-Li Wang.A bifunctional POM-based Cu-viologen complex with mixed octamolybdate clusters for rapid oxidation desulfurization and effective photogeneration of hydrogen[J].Rare Metals,2024,43(1):236-246.
8YANG Yinze,ZHANG Liyan,ZHOU Leilei,CHENG Haiyang,ZHAO Fengyu.A Highly Efficient Ni/Al_(2)O_(3)-LaO_(x) Catalyst for the Reductive Amination of Furfural to Furfurylamine:the Promoting Effect of La[J].Chemical Research in Chinese Universities,2024,40(1):36-46.
9Jie Fu,Dong Wang,Yan Li,Xianzheng Liu,Rui Zhang,Zhiyuan Liu,Pengdong Liu,Lijuan Zhang,Xuefei Li,Guangwu Wen.3D printed silicon-based micro-lattices with ultrahigh areal/gravimetric capacities and robust structural stability for lithium-ion batteries[J].Nano Research,2024,17(4):2693-2703.
10Zhen Wang,Yuan Cheng,Kewei Li,Tianxu Wang,Mengen Hu,Chunxue Zheng,Xinyang Li,Zhulin Huang,Xiaoye Hu,Yue Li,Xinghong Zhang.Synthesis and formation mechanism of HfB_(2) ultrafine powders with low oxygen via flocculating settling assisted process and carbo/borothermal reduction[J].Journal of Materials Science & Technology,2023(33):229-239.
Basic Information:
DOI:
Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动];O641.4[理学—物理化学]
Citation Information:
Tin-based materials with high theoretical capacity and suitable working voltage are ideal anode materials for lithium-ion batteries(LIBs). However, to overcome their shortcomings(volume expansion and inferior stability), the preparation processes are usually complicated and expensive. Herein, a tin-based metal-organic complex(tin 1,2-benzenedicarboxylic acid, Sn-BDC)with one-dimensional microbelt morphology is synthesized by a facile, rapid and low-cost co-precipitation method, and served as anode material for LIBs without any post-treatment. Sn-BDC exhibits a high reversible capacity with609/440 m Ah·g-1 at 50/2000 m A·g-1, and robust cycling stability of 856 m Ah·g-1 after 200 cycles at 200 m A·g-1,which are obviously superior to that of the Sn Ox/C counterparts. Moreover, an electrochemical reconstruction perspective on the lithium storage mechanism of Sn-BDC is proposed by systematic ex-situ characterizations. The reconstructed SnO2 replaces Sn-BDC and becomes the active material in the subsequent cycles. As the by-product of the lithiation reaction, the formed Li-based metal-organic complex(Li-BDC, wrapped around the reconstructed SnO2) plays an important role in alleviating volume expansion and accelerating the charge transfer kinetics.This work is beneficial to design and construct the new electrode materials based on the electrochemical reconstruction for advanced LIBs.
quote
| GB/T 7714-2015 | [1] Jin-Ke Shen, Nai-Teng Wu, Li-Yuan Wang, et al. Rare Metals, 2024(1): 76-86. |
| MLA | [1] Jin-Ke Shen, et al., Rare Metals, no. 1, 2024, pp. 76-86. |
| APA | [1] Jin-Ke Shen, Nai-Teng Wu, Li-Yuan Wang, Gang Jiang, Dong-Lei Guo, Jin Li, Gui-Long Liu, Hong-Yu Mi, Huan Pang, & Xian-Ming Liu. (2024). Rare Metals(1), 76-86. |
| IEEE | [1] Jin-Ke Shen, Nai-Teng Wu, Li-Yuan Wang, Gang Jiang, Dong-Lei Guo, Jin Li, Gui-Long Liu, Hong-Yu Mi, Huan Pang, and Xian-Ming Liu, Rare Metals, no. 1, pp. 76-86, 2024. |