daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Development of lithium-free P2-type high-sodium content cathode materials with enhanced cycle and air stability for sodium-ion batteries AITranslate

College of Chemical Engineering and Technology;College of Chemical Engineering and Technology;College of Chemical Engineering and Technology;College of Chemical Engineering and Technology;College of Chemical Engineering and Technology;College of Chemical Engineering and Technology;College of Chemical Engineering and Technology
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effect of partial substitution of Mg for Ni on a high-sodium and lithium-free layered P2-type Na45/54Mg6/54Ni12/54Mn34/54O2 cathode with high initial Coulombic efficiency and excellent cyclic stability has been investigated in this study.Based on the crystal structural analysis,the Mg doping can retain the P2 structure up to 4.3 V,thus restraining the detrimental phase transformation of P2-02during the Na-ion intercalation/deintercalation process.Therefore,the obtained Mg-doped P2-type cathode exhibits a reversible specific capacity of 109 mAh·g-1 at 0.1C between 2.0 and 4.3 V and a retention rate of 81.5% after 200cycles at 1C.In addition,the full cell consisting of Mg-doped P2-type cathode and hard carbon anode shows a capacity retention rate of 85.6% after 100 cycles.This study provides new insight into the development of durable cathode materials for sodium-ion batteries.

KeyWords AITranslate

Sodium-ion batteries Cathode material High sodium content Air stability

1孙媛媛,李思卿,王成儒,钱昱骁,郑时有,袁涛.钠离子电池层状过渡金属氧化物正极材料的研究进展[J].稀有金属,2022,46(6):776-795. 被引量:12

2Wen-Bin Li,Kang Wu,Hao Feng,Ni Wang,Jiang-Hua Zhang,Jing-Jing Wang,Xi-Fei Li.Atomic layer deposition of ultrafine Pd nanoparticles for enhancing the rate capability of LiNi_(0.8)Co_(0.1)Mn_(0.1)O_(2) cathode[J].Tungsten,2022,4(4):346-355. 被引量:4

3Kun-Qi Geng,Meng-Qian Yang,Jun-Xia Meng,Ling-Fei Zhou,Yu-Qin Wang,Sydorov Dmytro,Qian Zhang,Sheng-Wen Zhong,Quan-Xin Ma.Engineering layered/spinel heterostructure via molybdenum doping towards highly stable Li-rich cathodes[J].Tungsten,2022,4(4):323-335. 被引量:5

4王玉琪,蓝海航,侯琼,曾荣华,高进伟.蒽醌类有机电极材料在新型二次电池中的应用研究进展[J].稀有金属,2022,46(2):238-253. 被引量:4

5Jianyue Jiao,Kang Wu,Na Li,Enyue Zhao,Wen Yin,Zhongbo Hu,Fangwei Wang,Jinkui Zhao,Xiaoling Xiao.Tuning anionic redox activity to boost high-performance sodium-storage in low-cost Na_(0.67)Fe_(0.5)Mn_(0.5)O_(2) cathode[J].Journal of Energy Chemistry,2022,31(10):214-222. 被引量:2

6Guo-Qiang Liu,Yue Li,Yu-Long Du,Lei Wen.Synthesis and properties of Na_(0.8)Ni_(0.4)Mn_(0.6)O_2 oxide used as cathode material for sodium ion batteries[J].Rare Metals,2017,36(12):977-980. 被引量:4

7Zhao Fang,Xing-Liang Zhang,Xue-Yang Hou,Wen-Long Huang,Lin-Bo Li.Submicron single-crystalline LiNi_(0.5)Mn_(1.5)O_(4) cathode with modulated Mn^(3+) content enabling high capacity and fast lithium-ion kinetics[J].Rare Metals,2022,41(7):2268-2279. 被引量:3

1Haixia Zhang,Kuangshi Yu,Zhiping Zhu.Steam gasification reactivity of a high-sodium coal fly ash obtained from a pilot scale CFB gasifier[J].International Journal of Coal Science & Technology,2018,5(2):244-252. 被引量:4

2Bin Liu,Jie Liu,Cheng Zhong,Wenbin Hu.Mg-doped,carbon-coated,and prelithiated SiO_(x) as anode materials with improved initial Coulombic efficiency for lithium-ion batteries[J].Carbon Energy,2024,6(3):204-214.

3Shuhei Nomura,Aya Ishizuka,Shiori Tanaka,Daisuke Yoneoka,Hisayuki Uneyama,Kenji Shibuya.Umami: An Alternative Japanese Approach to Reducing Sodium While Enhancing Taste Desirability[J].Health,2021,13(6):629-636.

4Wenyun Wang,Chao Yang,Shangjing Yu,Daotong Han,Wentao Qi,Rui Ling,Guangqiang Liu.Defect engineering on BiFeO_(3) through Na and V codoping for aqueous Na-ion capacitors[J].Journal of Energy Chemistry,2024,90(3):453-463.

5Zhijia Zhang,Yuwen Zhao,Yanhao Wei,Mengmeng Zhang,Chunsheng Li,Yan Sun,Jianmin Ma,Yong Jiang.Modulating the p-band center of carbon nanofibers derived from Co spin state as anode for high-power sodium storage[J].Chinese Chemical Letters,2024,35(1):537-541.

6Dai-Hai YU,De-Pei LIU,Lai-Yuan WANG,Jing CHEN,Cashell E.JAQUISH,Dabeeru C.RAO,James E.HIXSON,Jian-Feng HUANG,Chung-Shiuan CHEN,Charles GU,Ji-Chun CHEN,Jie CAO,Shu-Feng CHEN,Paul K.WHELTON,Jiang HE,Dong-Feng GU.Genetic variants in the ADD1 and GNB3 genes and bloodpressure response to potassium supplementation[J].Frontiers of Medicine,2010,4(1):59-66.

7Xinyan Li,Ang Gao,Qinghua Zhang,Hao Yu,Pengxiang Ji,Dongdong Xiao,Xuefeng Wang,Dong Su,Xiaohui Rong,Xiqian Yu,Hong Li,Yong-Sheng Hu,Lin Gu.Cationic ordering transition in oxygen-redox layered oxide cathodes[J].Carbon Energy,2024,6(1):197-206.

8Bo Mai,Boyu Xing,Yunfan Yue,Nianyao Cai,Congcong Cai,Sitian Lian,Hao Fan,Mengyu Yan,Ting Zhu,Ping Hu,Xuewen Wang,Liqiang Mai.Cr-doped Na_(3)V_(2)(PO_(4))_(3)@C enables high-capacity with V^(2+)/V^(5+)reaction and stable sodium storage[J].Journal of Materials Science & Technology,2023(34):1-7.

9Haixiang Xiu,Wanqiang Liu,Dongming Yin,Nan Ding,Wenfeng Qiao,Shaolei Zhao,Long Liang,Cong Liu,Shaohua Wang,Qingshuang Wang,Bingbing Chen,Limin Wang,Yong Cheng.Multidimensional regulation of Ti-Zr-Cr-Mn hydrogen storage alloys via Y partial substitution[J].Nano Research,2024,17(5):4211-4220.

10刘雅文,刘义亭,郁汉琪,李佩娟.基于轻量化卷积神经网络的苹果目标检测算法[J].南京工程学院学报(自然科学版),2023,21(4):14-22.

Basic Information:

DOI:

Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动]

Citation Information:

The effect of partial substitution of Mg for Ni on a high-sodium and lithium-free layered P2-type Na45/54Mg6/54Ni12/54Mn34/54O2 cathode with high initial Coulombic efficiency and excellent cyclic stability has been investigated in this study.Based on the crystal structural analysis,the Mg doping can retain the P2 structure up to 4.3 V,thus restraining the detrimental phase transformation of P2-02during the Na-ion intercalation/deintercalation process.Therefore,the obtained Mg-doped P2-type cathode exhibits a reversible specific capacity of 109 mAh·g-1 at 0.1C between 2.0 and 4.3 V and a retention rate of 81.5% after 200cycles at 1C.In addition,the full cell consisting of Mg-doped P2-type cathode and hard carbon anode shows a capacity retention rate of 85.6% after 100 cycles.This study provides new insight into the development of durable cathode materials for sodium-ion batteries.

quote

GB/T 7714-2015 [1] Jin-Lv Tian, Lin-Rong Wu, Hai-Jun Zhao, et al. Rare Metals, 2024(1): 113-123.
MLA [1] Jin-Lv Tian, et al., Rare Metals, no. 1, 2024, pp. 113-123.
APA [1] Jin-Lv Tian, Lin-Rong Wu, Hai-Jun Zhao, Shou-Dong Xu, Liang Chen, Ding Zhang, & Xiao-Chuan Duan. (2024). Rare Metals(1), 113-123.
IEEE [1] Jin-Lv Tian, Lin-Rong Wu, Hai-Jun Zhao, Shou-Dong Xu, Liang Chen, Ding Zhang, and Xiao-Chuan Duan, Rare Metals, no. 1, pp. 113-123, 2024.