Nitrogen–sulfur co-doped porous carbon derived from asphalt as efficient catalyst for oxygen reduction AITranslate

Key Laboratory of Structure and Functional Regulation of Hybrid Materials;Key Laboratory of Structure and Functional Regulation of Hybrid Materials;Key Laboratory of Structure and Functional Regulation of Hybrid Materials;Key Laboratory of Structure and Functional Regulation of Hybrid Materials;Key Laboratory of Structure and Functional Regulation of Hybrid Materials
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

As an environment-friendly and low-cost petrochemical by-product, asphalt has great potential in the preparation of metal-free oxygen reduction electrocatalysts with excellent performance and outstanding stability. In this paper, we converted asphalt into porous carbon nanosheets by a simple activation method, using potassium citrate as the swelling agent.

KeyWords AITranslate

stability POROUS CATALYST

1甘億,王聪,李敬迎,郑俊杰,万厚钊,王浩.水系锌离子电池的稳定性优化策略[J].稀有金属,2022,46(6):753-775. 被引量:6

2王亚雄,钟顺彬,孙逢春.车载高质量密度固态储氢材料研究进展[J].稀有金属,2022,46(6):796-812. 被引量:9

3Jing-Jing Chen,Shuai Gu,Rui Hao,Zhen-Yu Wang,Mu-Qing Li,Zhi-Qiang Li,Kun Liu,Ke-Meng Liao,Zhi-Qiang Wang,He Huang,Ying-Zhi Li,Kai-Li Zhang,Zhou-Guang Lu.Co single atoms and nanoparticles dispersed on N-doped carbon nanotube as high-performance catalysts for Zn-air batteries[J].Rare Metals,2022,41(6):2055-2062. 被引量:3

4Chen Sun,Yong-Jie Zhao,Xuan-Yi Yuan,Jing-Bo Li,Hai-Bo Jin.Bimetal nanoparticles hybridized with carbon nanotube boosting bifunctional oxygen electrocatalytic performance[J].Rare Metals,2022,41(8):2616-2623. 被引量:1

1Rui Ma,Zixing Wang,Qingfeng Fu,Wang Zhou,Ying Mo,Jian Tu,Zhiyong Wang,Peng Gao,Changling Fan,Jilei Liu.Dual-salt assisted synergistic synthesis of Prussian white cathode towards high-capacity and long cycle potassium ion battery[J].Journal of Energy Chemistry,2023(8):16-23.

2Xiaofeng Lin,Xiaoxin Li,Beichi Luo,Dingshan Yu.Black-phosphorus-based materials for application in solar cells[J].Chinese Journal of Structural Chemistry,2023,42(7):34-46.

3Jiachen Zhao,Deshuai Yu,Jianmin Chen,Shihao Lin,Yonghua Tang,Chaoyu Fan,Dongfang Zhou,Youhui Lin.Deciphering the high-carbonization-temperature triggered enzymatic activity of wool-derived N,S-co-doped carbon nanosheets[J].Chinese Chemical Letters,2024,35(3):182-188.

4Yingqiao Jiang,Yinhui Wang,Gang Cheng,Yuehua Li,Lei Dai,Jing Zhu,Wei Meng,Jingyu Xi,Ling Wang,Zhangxing He.Multiple-dimensioned defect engineering for graphite felt electrode of vanadium redox flow battery[J].Carbon Energy,2024,6(2):143-153.

5付鑫.一种新型钻孔密封材料的研究与应用[J].煤,2024,33(4):59-61.

6Donghui Li,Wenzhe Wu,Xue Ren,Xixi Zhao,Hongbing Song,Meng Xiao,Quanhong Zhu,Hengjun Gai,Tingting Huang.Enhanced activation of peroxymonosulfate by Fe/N co-doped ordered mesoporous carbon with dual active sites for efficient removal of m-cresol[J].Chinese Journal of Chemical Engineering,2024,65(1):130-144.

7贾华,牛建瑞,高玮,芮遨宇,余铭浩,陈梦,郭延凯.电子转移主导的载钴生物炭活化PMS降解四环素[J].环境科学学报,2024,44(3):51-60.

8Yuqiao Dong,Guang-Ling Song,Yuqing Xu,Dajiang Zheng.Bio-inhibitive effect of an algal symbiotic bacterium on corrosion of magnesium in marine environment[J].Journal of Magnesium and Alloys,2023,11(12):4603-4618.

9Kaisheng Sun,Zemao Xiao,Yunfei Shen,Heng Lv,Jianpeng Zhu,Jianxiang Pang,Yang Zheng,Wenwen Kong,Long Chen.MOF-derived Se doped MnS/Ti_(3)C_(2)T_(x) as cathode and Zn-Ti_(3)C_(2)T_(x) membrane as anode for rocking-chair zinc-ion battery[J].Nano Research,2024,17(4):2781-2789.

10Qingye Meng,Shuangling Zhong,Jingfei Wang,Zhenqian Zhang,Yan Gao,Xuejun Cui.Sono-assembly of folate-decorated curcumins/alginate core-shell microcomplex and its targeted delivery and pH/reduction dual-triggered release[J].Particuology,2024,84(1):168-177.

Basic Information:

DOI:

Chinese Library Classification Number:O643.36[理学—物理化学]

Citation Information:

As an environment-friendly and low-cost petrochemical by-product, asphalt has great potential in the preparation of metal-free oxygen reduction electrocatalysts with excellent performance and outstanding stability. In this paper, we converted asphalt into porous carbon nanosheets by a simple activation method, using potassium citrate as the swelling agent.

quote

GB/T 7714-2015 [1] Jing-Sheng Ma, Ming-Zai Wu, Ling Chen, et al. Rare Metals, 2024(1): 380-388.
MLA [1] Jing-Sheng Ma, et al., Rare Metals, no. 1, 2024, pp. 380-388.
APA [1] Jing-Sheng Ma, Ming-Zai Wu, Ling Chen, Li-Xing Zhang, & Ying Xiong. (2024). Rare Metals(1), 380-388.
IEEE [1] Jing-Sheng Ma, Ming-Zai Wu, Ling Chen, Li-Xing Zhang, and Ying Xiong, Rare Metals, no. 1, pp. 380-388, 2024.