Attaining synergetic equilibrium of electrical conductivity and tensile strength in GQDs@GN/Cu composites through multi-scale intragranular and intergranular reinforcements AITranslate

Faculty of Materials Science and Engineering;Faculty of Materials Science and Engineering;Faculty of Materials Science and Engineering;Faculty of Materials Science and Engineering;Faculty of Materials Science and Engineering
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The configuration and quality of reinforcements, as well as the robustness of interfacial bonding,holding a critical significance in determining the concurrence between electrical conductivity and mechanical strength in metal matrix composites. In this study, citric acid was employed as the precursor for synthesizing multiscale carbon nanomaterials(graphene quantum dots and graphene, abbreviated as GQDs and GN). The GQDs@GN/Cu composites were fabricated through a segmented ball milling process in conjunction with subsequent spark plasma sintering(SPS). The intragranular GQDs and intergranular GQDs@GN had synergistically reinforced Cu composites through Orowan strengthening, load transfer strengthening and refinement strengthening. Furthermore,the robust interface bonding between GQDs@GN and Cu effectively mitigated interfacial impedance stemming from electron-boundary scattering. The yield strength and ultimate tensile strength of the GQDs@GN/Cu composites were recorded as 270 and 314 MPa, respectively, representing an improvement of 92 and 28% over pure Cu, while maintaining electrical conductivity at a level comparable to that of pure Cu. This study advances the understanding of the possibility of realizing a synergistic compatibility between electrical conductivity and mechanical strength in Cu composites.

KeyWords AITranslate

Cu matrix composites Interface bonding Mechanical property Graphene quantum dots(GQDs) Electrical conductivity

1Zi-Hao Chen,Han-Yu Hui,Cheng-Lin Li,Feng Chen,Xin-Ming Mei,Ye Ma,Ju-Ying Li,Seong-Woo Choi,Qing-Song Mei.GNPs/Al nanocomposites with high strength and ductility and electrical conductivity fabricated by accumulative roll-compositing[J].Rare Metals,2021,40(9):2593-2601. 被引量:3

2Ke-Chao Zhou,Hai-Long Pei,Jin-Kun Xiao,Lei Zhang.Micro-scratch behavior of WC particle-reinforced copper matrix composites[J].Rare Metals,2022,41(7):2337-2342. 被引量:2

3Hongbin Shi,Qing Liu,Xiaofeng Dai,Teng Zhang,Yuling Shi,Tao Wang.Magnetic graphene oxide-anchored Ni/Cu nanoparticles with a Cu-rich surface for transfer hydrogenation of nitroaromatics[J].Chinese Journal of Chemical Engineering,2022(10):235-246. 被引量:1

1Lu Liu,Guobing Ying,Quanguo Jiang,Dong Wen,Peng Wang,Meng Wu,Ziying Ji,Yongting Zheng,Xiang Wang.Ultra-high-temperature application of MXene: Stabilization of 2D Ti_(3)C_(2)T_(x) for cross-scale strengthening and toughening of 3D TiC[J].Journal of Advanced Ceramics,2024,13(1):1-10.

2Lei Yang,Lijie Sun,Hongfei Huang,Rasoul Esmaeely Neisiany,Zhengwei You.An interfacial robust and entire self-healing ionogel-elastomer hybrid for elastic electronics enables discretionary assembly and reconfiguration[J].Science China Chemistry,2024,67(4):1316-1323.

3Jiajia Ma,Yichang Xia,Tienan Zhao,Wenfeng Hu,Weifeng Zhang,Qinfei Ke,Yi Zhao.Adaptable "bubble particles" prepared by green aqueous phase reshaping for completely removing odor[J].Nano Research,2024,17(3):2172-2180.

4Changhui Niu,Qing Zhang,Laifei Cheng,Fang Ye,Litong Zhang,Min Huang,Tao Yang.Enhanced thermal conductivity and mechanical properties of 2D C_(f)/SiC composites modified by in-situ grown carbon nanotubes[J].Journal of Advanced Ceramics,2024,13(1):19-33.

5乌云嘎,姚媛媛,潘春雨,岳新伟,李学华.泊松点距离约束下无人机辅助地面应急网络覆盖性能研究[J].电讯技术,2024,64(2):230-238.

6Z.Y.Xu,C.F.Fang,C.J.Li,R.Wang,X.P.Zhang,J.Tan,Y.M.Wang.GO/MgO/Mg interface mediated strengthening and electromagnetic interference shielding in AZ31 composite[J].Journal of Magnesium and Alloys,2023,11(10):3800-3814.

7易锦伟,习瑶瑶,李诵斌,丁思琪,李阁平,肖方闹.钨及钨合金强化方法和烧结工艺研究进展[J].铜业工程,2024(1):90-99.

8周卫新,娄朝刚.Fabrication of YAG:Ce^(3+) and YAG:Ce^(3+),Sc^(3+) Phosphors by Spark Plasma Sintering Technique[J].Journal of Wuhan University of Technology(Materials Science),2024,39(2):255-260.

9张雅玥,黄子音,陶晓悦,杨静,么焕开,李岩.莓叶委陵菜化学成分含量分析[J].广东化工,2024,51(1):127-129.

10X.Liu,L.Song,A.Stark,F.Pyczak,T.B.Zhang.In-situ synchrotron high energy X-ray diffraction study on the internal strain evolution of D019-α2 phase during high-temperature compression and subsequent annealing in a TiAl alloy[J].Journal of Materials Science & Technology,2023(32):212-222.

Basic Information:

DOI:

Chinese Library Classification Number:TB33[一般工业技术—材料科学与工程]

Citation Information:

The configuration and quality of reinforcements, as well as the robustness of interfacial bonding,holding a critical significance in determining the concurrence between electrical conductivity and mechanical strength in metal matrix composites. In this study, citric acid was employed as the precursor for synthesizing multiscale carbon nanomaterials(graphene quantum dots and graphene, abbreviated as GQDs and GN). The GQDs@GN/Cu composites were fabricated through a segmented ball milling process in conjunction with subsequent spark plasma sintering(SPS). The intragranular GQDs and intergranular GQDs@GN had synergistically reinforced Cu composites through Orowan strengthening, load transfer strengthening and refinement strengthening. Furthermore,the robust interface bonding between GQDs@GN and Cu effectively mitigated interfacial impedance stemming from electron-boundary scattering. The yield strength and ultimate tensile strength of the GQDs@GN/Cu composites were recorded as 270 and 314 MPa, respectively, representing an improvement of 92 and 28% over pure Cu, while maintaining electrical conductivity at a level comparable to that of pure Cu. This study advances the understanding of the possibility of realizing a synergistic compatibility between electrical conductivity and mechanical strength in Cu composites.

quote

GB/T 7714-2015 [1] Shuang-Yin Zhang, Liang Liu, Rui Bao, et al. Rare Metals, 2024(1): 366-379.
MLA [1] Shuang-Yin Zhang, et al., Rare Metals, no. 1, 2024, pp. 366-379.
APA [1] Shuang-Yin Zhang, Liang Liu, Rui Bao, Jian-Hong Yi, & Sheng-Da Guo. (2024). Rare Metals(1), 366-379.
IEEE [1] Shuang-Yin Zhang, Liang Liu, Rui Bao, Jian-Hong Yi, and Sheng-Da Guo, Rare Metals, no. 1, pp. 366-379, 2024.