daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Microstructure and Mechanical Properties of WE43A Rare Earth Magnesium Alloys with Loose Defects AITranslate

1.Beijing Institute of Aeronautical Materials,Air China Development,Beijing 100095,China
2.College of Materials Science and Engineering,Nanchang Hangkong University,Nanchang 330063,China
3.Beijing Key Laboratory of Aeronautical Materials Testing and Evaluation,Beijing 100095,China
4.Key Laboratory of Aeronautical Science and Technology for Material Testing and Evaluation,Beijing 100095,China
5.Key Laboratory of Material Testing and Evaluation,Aero Engine Corporation of China,Beijing 100095,China
6.School of Materials Science and Engineering,Nanchang Hangkong University,Nanchang 330063,China
7.Avic Harbin Dongan Engine Co.,Ltd.,Harbin 150066,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

WE43A rare earth magnesium alloy possesses advantages in terms of high specific strength,specific stiffness,and high temperature resistance,making it highly beneficial for lightweighting aerospace applications. It finds extensive use in aviation,aerospace,and related fields,such as helicopter frames,aircraft wings,and compressor casings. According to statistics,the majority of magnesium alloy components (90%) are produced through casting,which inevitably leads to the occurrence of porosity defects within the magnesium alloy. Even a small amount of porosity defects can cause a significant decrease in mechanical performance. This is due to the reduction in the effective load-bearing area of the castings caused by the presence of porosity defects,resulting in stress concentration and the initiation and propagation of fatigue cracks under cyclic loading conditions. As a result,the fatigue performance of critical load-bearing castings is compromised,leading to premature failure and severe consequences. In general,the generation of defects can be minimized by implementing techniques such as centrifugal casting and controlling the solidification temperature. Centrifugal casting promotes grain growth,thereby reducing defects associated with grain boundaries and producing a more uniform and dense material structure. Additionally,controlling the solidification temperature allows for the adjustment of the solidification rate,preventing defects caused by excessively high or low local temperatures and improving the overall quality of the material. However,there has been limited systematic investigation on the mechanical properties of materials with defects. Therefore,it is necessary to analyze and study the mechanical properties and changes of WE43A rare earth magnesium alloy containing porosity defects. In this study,WE43A rare earth magnesium alloy was selected as the research subject,and the samples were graded and screened to obtain specimens that meet the defect level requirements for subsequent mechanical property testing. This was achieved by increasing the probability of defect occurrence through process adjustments and directly selecting samples from a large number of production products to obtain specimens that conform to the defect level requirements. X-ray non-destructive testing was an efficient and accurate quality inspection method that played a crucial role in magnesium alloy castings. This technique provided internal structural imaging information of the samples,enabling comprehensive assessment of internal quality. According to the "Specification for Magnesium Alloy Castings",five defect levels (I to V) were defined to describe the severity of porosity defects. Sponge-like and dispersed forms were two typical types of porosity defects. Four-point bending fatigue tests were performed on specimens with dimensions of approximately (7.4±0.1) mm in thickness,(21.0±0.1) mm in width,and (82.2±0.1) mm in length. The fatigue specimens were plate-shaped,supported by rollers,with a roller diameter of 10 mm,and a pressure roller was used to apply an average stress of 100 MPa at a loading frequency of 20 Hz. Tensile tests were conducted on rod-shaped specimens with a diameter of approximately (5.00±0.02) mm and a length of (110±0.1) mm using an MTS electronic universal testing machine. The tensile tests were carried out in accordance with HB5143,with a strain rate of 0.00025 s−1. Metallographic analysis of the alloy was performed using an XJP-3Ad metallographic microscope (OM). Scanning electron microscopes (SEM),including S-3400N-type and SU1510-type,were utilized to observe the fracture morphology. The influence of different types and degrees of defects on the mechanical properties of rare earth magnesium alloys was systematically investigated,and the formation mechanism and control strategies of defects were discussed. This provided a theoretical basis for improving the casting quality and efficiency of rare earth magnesium alloys. The study of internal defects in alloys and further understanding of the destructive effects of defects had both theoretical and practical significance. The results indicated that the porosity defects mainly existed as irregular strip-like and elliptical voids at grain boundaries. With increasing defect levels,the area of porosity defects within the specimens continuously increased from 0.8% to 30%. The tensile strength,yield strength,and elongation of WE43A magnesium alloy exhibited a decreasing trend with increasing defect levels,with the decrease in elongation being slightly smaller than that in tensile strength. The average tensile strength of specimens with defect Level Ⅰ was approximately 260 MPa,which decreased to 80 MPa when the defect level reached Ⅴ. The yield strength decreased from 180 to 70 MPa. The reductions in tensile strength and yield strength were 70.71% and 62.22%,respectively,while the decrease in elongation was 41.56%. The average fatigue logarithmic life (lgN) of specimens with defect Level Ⅴ decreased by 28.17% compared to that of defect-free specimens. The average fatigue limit of specimens with defect Level Ⅴ decreased by 38.09% compared to that of defect-free specimens. The fatigue fracture exhibited cleavage feature;a small amount of porosity (defect Level Ⅰ) had a minor effect on the mechanical properties of the material. When the porosity content was low,there was little difference in tensile strength,yield strength,elastic modulus,and defect-free magnesium alloy. However,a noticeable decrease in mechanical performance occurred when the defect level reached Ⅱ. The excessive porosity defects significantly reduced the material's ductility.

KeyWords AITranslate

WE43A magnesium alloy defect morphology mechanical properties fatigue life prediction model

[1]卢立伟,康伟,黎小辉,罗骏,马旻,陈伟. 时效处理对Mg-Zn-Gd-Er稀土镁合金的组织和力学性能的影响 [J]. 稀有金属,2022,46(9): 1153.

L W Lu,W Kang,X H Li,J Luo,M Ma,W Chen. Effect of aging treatment on microstructure and mechanical properties of Mg-Zn-Gd-Er rare earth magnesium alloys [J]. Chinese Journal of Rare Metals,2022,46(9): 1153.

[2]唐昌平,张超,王雪兆,吴凯,陈旭,刘筱. 镁合金非对称变形研究进展 [J]. 稀有金属,2021,45(12): 1501.

C P Tang,C Zhang,X Z Wang,K Wu,X Chen,X Liu. Research progress on asymmetric deformation of Magnesium alloys [J]. Chinese Journal of Rare Metals,2021,45(12): 1501.

[3]Lei S Z,Xiang X,Hai L H,Shan S X,Zheng W H,Zhong H. Microstructure and properties of vacuum electron beam welded WE43 magnesium alloy joint [J]. SN Applied Sciences,2022,4(8): 207.1.

[4]关肖虎,王文,张婷,蔡军,王快社. 水下搅拌摩擦加工对 Mg-Gd-Y-Zn-Zr 合金微观组织和力学性能的影响 [J]. 塑性工程学报,2023,30(1): 191.

X H Guan,W Wang,T Zhang,J Cai,K S Wang. Influence of underwater friction stir processing on microstructure and me-chanical properties of Mg-Gd-Y-Zn-Zr alloy [J]. Journal of Plasticity Engineering,2023,30(1): 191.

[5]李星星,刘正,王越,魏子淇,王峰,王志. 铸态镁合金Mg-xZn-0.5Y-0.5Zr热裂缺陷研究 [J]. 稀有金属,2020,44(7): 697.

X X Li,Z Liu,Y Wang,Z Q Wei,F Wang,Z Wang. Study on thermal cracking defects of Mg-xZn-0.5Y-0.5Zr in as-cast magnesium alloys [J]. Chinese Journal of Rare Metals,2020,44(7): 697.

[6]Lovašiová P,Lovaši T,Kubásek J,Jablonská E,Msallamová Š,Michalcová A,Vojtěch D,Suchý J,Koutný D,Ghassan H A E. Biodegradable WE43 magnesium alloy produced by selective laser melting: mechanical properties,corrosion behavior,and in-vitro cytotoxicity [J]. Metals,2022,12(3): 469.

[7]吕刚,何建丽,赵卫东,何进. 挤压态WE43镁合金夹杂致裂的研究 [J]. 锻压技术,2022,47(2): 192.

G Lv,J L He,W D Zhao,J He. Study on inclusion cracking of extruded WE43 magnesium alloys [J]. Forging & Stamping Technology,2022,47(2): 192.

[8]Huang Z Y,Liu C M,Jiang S N,Xiao H C,Chen X,Wan Y C,Zeng G. Achieving high-strength nanocrystalline WE43 Mg alloy by a combination of cold rotary swaging and aging treatment [J]. Vacuum,2022. doi:10.1016/j.vacuum.2021.110840.

[9]Barylski A,Aniołek K,Dercz G,Kowalewski P,Kaptacz S,Rak J,Kupka M. Investigation of micromechanical properties and tribological behavior of WE43 magnesium alloy after deep cryogenic treatment combined with precipitation hardening [J]. Materials,2021,14(23): 7343.

[10]Sun W T,Wu B,Fu H,Yang X S,Qiao X G,Zheng M Y,He Y,Lu J,Shi S Q. Combining gradient structure and supersaturated solid solution to achieve superior mechanical properties in WE43 magnesium alloy [J]. Journal of Materials Science & Technology,2022,99: 223.

[11]Pereira G S,Koga G Y,Avila J A,Bittencourt I M,Fernandez F,Miyazaki M H,Botta W J,Bose F W W. Corrosion resistance of WE43 Mg alloy in sodium chloride solution [J]. Materials Chemistry and Physics,2021,272: 124930.

[12]张玺,韩峰,赵柯,武冰冰,闫基森,解芳. 离焦量对ZK60镁合金激光表面熔凝组织及性能的影响 [J]. 有色金属工程,2023,13(8): 56.

X Zhang,F Han,K Zhao,B B Wu,J S Yan,F Xie. Effect of defocusing amount on microstructure and properties of laser surface melting of ZK60 magnesium alloy [J]. Nonferrous Metals Engineering,2023,13(8): 56.

[13]何维维,陈军洲,郝敏,戴圣龙. WE43镁合金的热变形行为及热加工图 [J]. 机械工程材料,2021,45(7): 69.

W W He,J Z Chen,M He,S L Dai. Hot deformation behavior and hot working diagram of WE43 magnesium alloy [J]. Materials for Mechanical Engineering,2021,45(7): 69.

[14]Kharitonov D S,Zimowska M,Ryl J,Zieliński A,Osipenko M A,Adamiec J,Wrzesińska A,Claesson P M,Kurilo I I. Aqueous molybdate provides effective corrosion inhibition of WE43 magnesium alloy in sodium chloride solutions [J]. Corrosion Science,2021,190: 109664.

[15]张涛,邹金超,黄志权,赵春江,王军朋. 轧制温度对AZ61镁合金耐腐蚀性的影响 [J]. 有色金属科学与工程,2023,14(4): 473.

T Zhang,J C Zou,Z Q Huang,C J Zhao,J P Wang. Effect of rolling temperature on the corrosion resistance of AZ61 magnesium alloy [J]. Nonferrous Metals Science and Engineering,2023,14(4): 473.

[16]耿纪龙,闫志峰,张红霞,董鹏. 超声表面滚压处理对AZ31B镁合金组织和性能的影响 [J]. 表面技术,2022,51(1): 368.

J L Geng,Z F Yan,H X Zhang,P Dong. Effect of ultrasonic surface rolling treatment on microstructure and properties of AZ31B magnesium alloy [J]. Surface Technology,2022,51(1): 368.

[17]张文玉,刘先兰,邓彬,何文鹏,吴朝曦,聂志诚. 轧制温度对AZ31镁合金板材组织和性能的影响 [J]. 锻压技术,2023,48(1): 158.

W Y Zhang,X L Liu,B Deng,W P He,Z X Wu,Z C Nie. Influence of rolling temperature on microstructure and properties of AZ31 magnesium alloy sheet [J]. Forging & Stamping Technology,2023,48(1): 158.

[18]张立杰,王浡婳. AZ91D镁合金表面Ni基激光熔覆涂层的组织和性能 [J]. 粉末冶金工业,2021,31(4): 77.

L J Zhang,B H Wang. Microstructure and properties of Ni-based laser cladding coating on AZ91D magnesium alloy surface [J]. Powder Metallurgy Industry,2021,31(4): 77.

[19]魏振伟,陈皓晖,沈佳萌,刘昌奎,周伟. WE43A镁合金补焊组织及性能研究 [J]. 失效分析与预防,2022,17(5): 328.

Z W Wei,H H Chen,J M Shen,C K Liu,W Zhou. Study on the microstructure and properties of repair welding joints in WE43A magnesium alloys [J]. Failure Analysis and Prevention,2022,17(5): 328.

[20]何树先,王俊,孙宝德. 热等静压对高温合金薄壁铸件疏松缺陷及性能的影响 [J]. 热加工工艺,2014,43(21): 88.

S X He,J Wang,B D Sun. Influence of hot isostatic pressing on loose defects and properties of thin-wall superalloy castings [J]. Hot Working Technology,2014,43(21): 88.

[21]赵朋飞,王育红,张新运,李宏民. 含疏松缺陷的ZL205A合金力学性能研究 [J]. 装备环境工程,2017,14(8): 88.

P F Zhao,Y H Wang,X Y Zhang,H M Li. Mechanical properties of ZL205A alloy with loose defects [J]. Equipment Environmental Engineering,2017,14(8): 88.

[22]Carroll J D,Brewer L N,Battaile C C,Boyce B L,Emery J M. The effect of grain size on local deformation near a void-like stress concentration [J]. International Journal of Plasticity,2012,39: 46.

[23]康丽霞,曹义华,宁向荣. 直升机传动系统疲劳定寿技术 [J].航空动力学报,2011,26(6): 1431.

L X Kang,Y H Cao,X R Ning. Fatigue life determination technology of helicopter transmission system [J]. Journal of Aerospace Power,2011,26(6): 1431.

[24]宁向荣,陈伟,蔡显新,廖学军,米栋. 四参数疲劳定寿方法 [J]. 航空动力学报,2012,27(8): 1746.

X R Ning,W Chen,X X Cai,X J Liao,D Mi. Four-parameter fatigue life determination method [J]. Journal of Aerodynamics,2012,27(8): 1746.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY23090022

Chinese Library Classification Number:TG146.2

Citation Information:

WE43A rare earth magnesium alloy possesses advantages in terms of high specific strength,specific stiffness,and high temperature resistance,making it highly beneficial for lightweighting aerospace applications. It finds extensive use in aviation,aerospace,and related fields,such as helicopter frames,aircraft wings,and compressor casings. According to statistics,the majority of magnesium alloy components (90%) are produced through casting,which inevitably leads to the occurrence of porosity defects within the magnesium alloy. Even a small amount of porosity defects can cause a significant decrease in mechanical performance. This is due to the reduction in the effective load-bearing area of the castings caused by the presence of porosity defects,resulting in stress concentration and the initiation and propagation of fatigue cracks under cyclic loading conditions. As a result,the fatigue performance of critical load-bearing castings is compromised,leading to premature failure and severe consequences. In general,the generation of defects can be minimized by implementing techniques such as centrifugal casting and controlling the solidification temperature. Centrifugal casting promotes grain growth,thereby reducing defects associated with grain boundaries and producing a more uniform and dense material structure. Additionally,controlling the solidification temperature allows for the adjustment of the solidification rate,preventing defects caused by excessively high or low local temperatures and improving the overall quality of the material. However,there has been limited systematic investigation on the mechanical properties of materials with defects. Therefore,it is necessary to analyze and study the mechanical properties and changes of WE43A rare earth magnesium alloy containing porosity defects. In this study,WE43A rare earth magnesium alloy was selected as the research subject,and the samples were graded and screened to obtain specimens that meet the defect level requirements for subsequent mechanical property testing. This was achieved by increasing the probability of defect occurrence through process adjustments and directly selecting samples from a large number of production products to obtain specimens that conform to the defect level requirements. X-ray non-destructive testing was an efficient and accurate quality inspection method that played a crucial role in magnesium alloy castings. This technique provided internal structural imaging information of the samples,enabling comprehensive assessment of internal quality. According to the "Specification for Magnesium Alloy Castings",five defect levels (I to V) were defined to describe the severity of porosity defects. Sponge-like and dispersed forms were two typical types of porosity defects. Four-point bending fatigue tests were performed on specimens with dimensions of approximately (7.4±0.1) mm in thickness,(21.0±0.1) mm in width,and (82.2±0.1) mm in length. The fatigue specimens were plate-shaped,supported by rollers,with a roller diameter of 10 mm,and a pressure roller was used to apply an average stress of 100 MPa at a loading frequency of 20 Hz. Tensile tests were conducted on rod-shaped specimens with a diameter of approximately (5.00±0.02) mm and a length of (110±0.1) mm using an MTS electronic universal testing machine. The tensile tests were carried out in accordance with HB5143,with a strain rate of 0.00025 s−1. Metallographic analysis of the alloy was performed using an XJP-3Ad metallographic microscope (OM). Scanning electron microscopes (SEM),including S-3400N-type and SU1510-type,were utilized to observe the fracture morphology. The influence of different types and degrees of defects on the mechanical properties of rare earth magnesium alloys was systematically investigated,and the formation mechanism and control strategies of defects were discussed. This provided a theoretical basis for improving the casting quality and efficiency of rare earth magnesium alloys. The study of internal defects in alloys and further understanding of the destructive effects of defects had both theoretical and practical significance. The results indicated that the porosity defects mainly existed as irregular strip-like and elliptical voids at grain boundaries. With increasing defect levels,the area of porosity defects within the specimens continuously increased from 0.8% to 30%. The tensile strength,yield strength,and elongation of WE43A magnesium alloy exhibited a decreasing trend with increasing defect levels,with the decrease in elongation being slightly smaller than that in tensile strength. The average tensile strength of specimens with defect Level Ⅰ was approximately 260 MPa,which decreased to 80 MPa when the defect level reached Ⅴ. The yield strength decreased from 180 to 70 MPa. The reductions in tensile strength and yield strength were 70.71% and 62.22%,respectively,while the decrease in elongation was 41.56%. The average fatigue logarithmic life (lgN) of specimens with defect Level Ⅴ decreased by 28.17% compared to that of defect-free specimens. The average fatigue limit of specimens with defect Level Ⅴ decreased by 38.09% compared to that of defect-free specimens. The fatigue fracture exhibited cleavage feature;a small amount of porosity (defect Level Ⅰ) had a minor effect on the mechanical properties of the material. When the porosity content was low,there was little difference in tensile strength,yield strength,elastic modulus,and defect-free magnesium alloy. However,a noticeable decrease in mechanical performance occurred when the defect level reached Ⅱ. The excessive porosity defects significantly reduced the material's ductility.

quote

GB/T 7714-2015 [1] Zhenwei Wei, Zifeng Wang, Aihua Zou, et al. Microstructure and Mechanical Properties of WE43A Rare Earth Magnesium Alloys with Loose Defects[J]. Chinese Journal of Rare Metals, 2025, 49(2): 153-162. DOI:10.13373/j.cnki.cjrm.XY23090022.
MLA [1] Zhenwei Wei, et al., "Microstructure and Mechanical Properties of WE43A Rare Earth Magnesium Alloys with Loose Defects." Chinese Journal of Rare Metals, vol. 49, no. 2, 2025, pp. 153-162, https://doi.org/10.13373/j.cnki.cjrm.XY23090022.
APA [1] Zhenwei Wei, Zifeng Wang, Aihua Zou, Zhipeng Li, Heng Wang, Wei Zhao, Guangshan Yang, & Changkui Liu. (2025). Microstructure and Mechanical Properties of WE43A Rare Earth Magnesium Alloys with Loose Defects. Chinese Journal of Rare Metals, 49(2), 153-162. https://doi.org/10.13373/j.cnki.cjrm.XY23090022
IEEE [1] Zhenwei Wei, Zifeng Wang, Aihua Zou, Zhipeng Li, Heng Wang, Wei Zhao, Guangshan Yang, and Changkui Liu, "Microstructure and Mechanical Properties of WE43A Rare Earth Magnesium Alloys with Loose Defects," Chinese Journal of Rare Metals, vol. 49, no. 2, pp. 153-162, 2025, doi: 10.13373/j.cnki.cjrm.XY23090022. keywords: {WE43A magnesium alloy;defect morphology;mechanical properties;fatigue life prediction model}