Electrochemical and Kinetic Mechanism of Oxidizing Acid-Leaching Process of Niobium Tantalum Ore AITranslate

State Key Laboratory of Advanced Special Steels,Key Laboratory of Modern Metallurgy and Material Preparation,School of Material Science and Engineering,Shanghai University,Shanghai 200444,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In order to investigate the effects of oxidation conditions on the leaching rate of niobium tantalum ore,the cyclic voltammetry,Tafel polarization curve,impedance and open-circuit potential methods were used to study the effects of different oxidation potentials,different HF concentrations and different temperatures on the leaching rate of niobium tantalum ore. The cyclic voltammetry was used to investigate the oxidation reaction in the process of acid leaching of niobium tantalum ore. The cyclic voltammetry curve of niobium tantalum electrode had four oxidation peaks A1,A2,A3 and A4 of low valence Fe and Mn,and the oxidation peak potential values were -0.38,0.1,0.31 and 0.6 V,respectively. Among them,A1 and A2 were the oxidation peaks of MnO and Fe3O4 phases in niobium tantalum ore,corresponding to the oxidation of Mn2+ to Mn3+ and Fe2+ to Fe3+,respectively. A3 and A4 were the oxidation of (Fe,Mn)(Nb,Ta)2O6 mineral phase in niobium tantalum ore corresponding to the oxidation of Mn2+ to Mn3+ and Fe2+ to Fe3+ in (Fe,Mn)(Nb,Ta)2O6 mineral phase,respectively. The current density (Jcoor) of Tafel polarization curve increased with the increase of HF concentration in the electrolyte,and reached the maximum value of 849.68 µA·cm−2 at 10 mol·L−1 HF. The anode slope decreased with the increase of HF concentration and then tended to be stable,indicating that the oxidation leaching rate of total mineral phase at the ore/liquid interface on the surface of niobium tantalum electrode increased with the increase of HF concentration and then tended to be stable after reaching the maximum value at 10 mol·L−1 HF. At -0.38 and 0.1 V oxidation potential,AC impedance test of HF concentration on MnO and Fe3O4 mineral phases showed the charge transfer density (JRct) increased with increasing HF concentration. Mn charge transfer density JRct increased from 3.86 µA·cm−2 of 4 mol·L−1 HF to 68 µA·cm−2 of 10 mol·L−1 HF. Fe charge transfer density JRct increased from 1.11 µA·cm−2 of 4 mol·L−1 HF to 87.32 µA·cm−2 of 10 mol·L−1 HF. The leaching rates of Mn and Fe also accelerated with the increase of HF concentration in the electrolyte. Mn leaching rate reached the maximum of 29.4 mg·L−1·h−1 at 10 mol·L−1 HF and Fe leaching rate reached the maximum of 5.5 mg·L−1·h−1 at 10 mol·L−1 HF. The experimental results showed that the leaching rates of MnO and Fe3O4 mineral phase increased with the increase of HF concentration,and the leaching rates of Mn and Fe ions reached the maximum in 10 mol·L−1 HF electrolyte. At 0.31 and 0.6 V oxidation potential,AC impedance test of HF concentration on (Fe,Mn)(Nb,Ta)2O6 mineral phase showed that Fe and Mn charge transfer density JRct increased with the increase of HF concentration in the electrolyte. Fe charge transfer density JRct increased from 1.94 µA·cm−2 of 4 mol·L−1 HF to 143.7 µA·cm−2 of 11 mol·L−1 HF. Mn charge transfer density JRct increased from 13.06 µA·cm−2 of 4 mol·L−1 HF to 168.4 µA·cm−2 of 11 mol·L−1 HF. The leaching rates of Fe and Mn element from niobium tantalum was also accelerated with the increase of HF concentration in the electrolyte. The leaching rate of Fe reached the maximum of 2.56 mg·L−1·h−1 at 11 mol·L−1 HF and the leaching rate of Mn reached the maximum of 2.88 mg·L−1·h−1 at 11 mol·L−1 HF. The experimental results showed that the leaching rate of (Fe,Mn)(Nb,Ta)2O6 mineral phase increases with the increase of HF concentration,and the leaching rate of Nb ion reached the maximum at 11 mol·L−1 HF. Tafel results of niobium tantalum ore at different reaction temperatures showed that temperature had a significant effect on the oxidation leaching of niobium tantalum ore. With the increase of temperature,the oxidation leaching rate of niobium tantalum ore was accelerated,and the corrosion current density gradually increased. The corrosion current density tended to flatten out when it reached the maximum value of 959.20 µA·cm−2 at 80 ℃. The dominant activation energy of Nb ion in the oxidation leaching stage was 3.018 kJ·mol−1 based on Arrhenius formula. The results of AC impedance tests of (Fe,Mn)(Nb,Ta)2O6 mineral phase at different reaction temperatures and the determination of Nb ion leaching rate by inductively coupled plasma mass spectrometer (ICP) showed that with the increase of HF concentration,the oxidation current density also increased gradually,reaching the maximum 178.4 µA·cm−2 and 192.5 µA·cm−2 at 80 ℃. As determined by ICP,the oxidation leaching rate of Nb accelerated with the increase of temperature,reaching a maximum of 5.32 mg·L−1·h−1 at 80 ℃. The oxidation reaction rate of Nb ion was basically unchanged as the temperature continues to rise,which might be caused by the change of the double layer structure at the niobium tantalum/liquid interface with the increase of temperature. The results of impedance AC experiments at different temperatures showed that the current density increases with the increase of temperature,reaching the maximum values 192.5 µA·cm−2 at 80 ℃.

KeyWords AITranslate

niobium tantalum ore electrochemistry ore/liquid interface oxidation leaching rate surface oxidation mechanism

[1]Gao W C,Wen J K,Wu B,Shang H. Extraction of niobium yttrium and cerium from a low-grade niobium-bearing ore by roasting (NH4)2SO4-Na2SO4-H2SO4 system [J]. Rare Metals,2014,33(6): 754.

[2]Wöhlecke M,Corradi G,Betzler K. Optical methods to characterise the composition and homogeneity of lithium niobate single crystals [J]. Applied Physics B,1996,63(4): 323.

[3]El-Hussaini O M,Mahdy M A. Sulfuric acid leaching of Kab Amiri niobium-tantalum bearing minerals,Central Eastern Desert,Egypt [J]. Hydrometallurgy,2002,64(3): 219.

[4]高文成,温建康,武彪,尚鹤. 处理铌钽矿的冶金技术进展概况 [J]. 稀有金属,2016,40(1): 77.

W C Gao,J K Wen,B Wu,H Shang. Progress in metallurgical technology for treating niobium tantalum ore [J]. Chinese Journal of Rare Metals,2016,40(1): 77.

[5]周宏明,郑诗礼,张懿. 钽铌湿法冶金技术概况及发展趋势探讨 [J]. 现代化工,2005,25(4): 16.

H M Zhou,S L Zheng,Y Zhang. Tantalum niobium hydrometallurgy technology overview and development trend [J]. Modern Chemical Industry,2005,25(4): 16.

[6]任卿,张锦柱,赵春红. 钽、 铌资源现状及其分离方法研究进展 [J]. 湿法冶金,2006,25(2): 65.

Q Ren,J Z Zhang,C H Zhao. Progress of tantalum and niobium resources and their separation methods [J]. Hydrometallurgy,2006,25(2): 65.

[7]Wang D,Li Q J,Guo X,Zou X L. Study on dissolution mechanism of mineral/liquid interface during HF acid leaching niobium-tantalum ore [J]. Minerals Engineering,2022,188: 107835.

[8]Yang F X,Li Q J,Wang D,Zhou C,Zheng S B. Interfacial structure change and selective dissolution of columbite-(Fe) mineral during HF acid leaching [J]. Minerals,2021,11(2): 146.

[9]周宏明,郑诗礼,张懿. 难分解铌钽矿高浓氢氧化钾浸出机理研究 [J].高校化学工程学报,2005,19(2): 148.

H M Zhou,S L Zheng,Y Zhang. Study on leaching mechanism of high concentration potassium hydroxide from refractory niobium tantalum ore [J]. Journal of Chemical Engineering in Universities,2005,19(2): 148.

[10]Rodriguez M H,Gustavo D R,Eliana G P,Daniela S S. Extraction of niobium and tantalum from ferrocolumbite by hydrofluoric acid pressure leaching [J]. Hydrometallurgy,2015,156: 17.

[11]Rodriguez M H,Quiroga O,Ruiz M D. Kinetic study of ferrocolumbite dissolution in hydrofluoric acid medium [J]. Hydrometallurgy,2007,85(2): 87.

[12]Candon P B. Proeess for Recovering Colubium and Tantalum from Ore Concentrates Containing Same[P]. USA: 2058825,1962.

[13]刘云. 黄铁矿氧化机理及表面钝化行为的电化学研究[D].广州: 华南理工大学,2011. 1.

Y Liu. Electrochemical Study on the Oxidation Mechanism and Surface Passivation Behavior of Pyrite[D].Guangzhou: South China University of Technology,2011.1.

[14]帅阿敏,缪清清,王晨,庄凰龙. DPV法测定食量茶中的芦丁 [J].化学工程与装备,2021,(11): 213.

A M Shuai,Q Q Miu,C Wang,Y Lin,H L Zhuang. Determination of rutin in edible tea by DPV method [J]. Chemical Engineering and Equipment,2021,(11): 213.

[15]闵定伟,陈功,文棠根,石忠宁,黄义鹏,杨少华. NaCl-KCl-MgCl2-Cu2S熔体中铜电沉积的电化学机理 [J]. 有色金属科学与工程,2023,14(2): 182.

D W Min,G Chen,T G Wen,Z N Shi,Y P Huang,S H Yang. Electrochemical mechanism of copper electrodeposition in NaCl-KCl-MgCl2-Cu2S melts [J]. Nonferrous Metals Science and Engineering,2023,14(2): 182.

[16]刘虹灵,别传玉,宋华伟,张宇平,李晨威,高标. 基于等效电路模型RBF网络的电池容量快速预测 [J]. 稀有金属,2023,47(6): 915.

H L Liu,C Y Bie,H W Song,Y Y Zhang,C W Li,B Gao. Fast prediction of battery capacity based on equivalent circuit model and RBF network [J]. Chinese Journal of Rare Metals,2023,47(6): 915.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY23030038

Chinese Library Classification Number:TF841.6

Citation Information:

In order to investigate the effects of oxidation conditions on the leaching rate of niobium tantalum ore,the cyclic voltammetry,Tafel polarization curve,impedance and open-circuit potential methods were used to study the effects of different oxidation potentials,different HF concentrations and different temperatures on the leaching rate of niobium tantalum ore. The cyclic voltammetry was used to investigate the oxidation reaction in the process of acid leaching of niobium tantalum ore. The cyclic voltammetry curve of niobium tantalum electrode had four oxidation peaks A1,A2,A3 and A4 of low valence Fe and Mn,and the oxidation peak potential values were -0.38,0.1,0.31 and 0.6 V,respectively. Among them,A1 and A2 were the oxidation peaks of MnO and Fe3O4 phases in niobium tantalum ore,corresponding to the oxidation of Mn2+ to Mn3+ and Fe2+ to Fe3+,respectively. A3 and A4 were the oxidation of (Fe,Mn)(Nb,Ta)2O6 mineral phase in niobium tantalum ore corresponding to the oxidation of Mn2+ to Mn3+ and Fe2+ to Fe3+ in (Fe,Mn)(Nb,Ta)2O6 mineral phase,respectively. The current density (Jcoor) of Tafel polarization curve increased with the increase of HF concentration in the electrolyte,and reached the maximum value of 849.68 µA·cm−2 at 10 mol·L−1 HF. The anode slope decreased with the increase of HF concentration and then tended to be stable,indicating that the oxidation leaching rate of total mineral phase at the ore/liquid interface on the surface of niobium tantalum electrode increased with the increase of HF concentration and then tended to be stable after reaching the maximum value at 10 mol·L−1 HF. At -0.38 and 0.1 V oxidation potential,AC impedance test of HF concentration on MnO and Fe3O4 mineral phases showed the charge transfer density (JRct) increased with increasing HF concentration. Mn charge transfer density JRct increased from 3.86 µA·cm−2 of 4 mol·L−1 HF to 68 µA·cm−2 of 10 mol·L−1 HF. Fe charge transfer density JRct increased from 1.11 µA·cm−2 of 4 mol·L−1 HF to 87.32 µA·cm−2 of 10 mol·L−1 HF. The leaching rates of Mn and Fe also accelerated with the increase of HF concentration in the electrolyte. Mn leaching rate reached the maximum of 29.4 mg·L−1·h−1 at 10 mol·L−1 HF and Fe leaching rate reached the maximum of 5.5 mg·L−1·h−1 at 10 mol·L−1 HF. The experimental results showed that the leaching rates of MnO and Fe3O4 mineral phase increased with the increase of HF concentration,and the leaching rates of Mn and Fe ions reached the maximum in 10 mol·L−1 HF electrolyte. At 0.31 and 0.6 V oxidation potential,AC impedance test of HF concentration on (Fe,Mn)(Nb,Ta)2O6 mineral phase showed that Fe and Mn charge transfer density JRct increased with the increase of HF concentration in the electrolyte. Fe charge transfer density JRct increased from 1.94 µA·cm−2 of 4 mol·L−1 HF to 143.7 µA·cm−2 of 11 mol·L−1 HF. Mn charge transfer density JRct increased from 13.06 µA·cm−2 of 4 mol·L−1 HF to 168.4 µA·cm−2 of 11 mol·L−1 HF. The leaching rates of Fe and Mn element from niobium tantalum was also accelerated with the increase of HF concentration in the electrolyte. The leaching rate of Fe reached the maximum of 2.56 mg·L−1·h−1 at 11 mol·L−1 HF and the leaching rate of Mn reached the maximum of 2.88 mg·L−1·h−1 at 11 mol·L−1 HF. The experimental results showed that the leaching rate of (Fe,Mn)(Nb,Ta)2O6 mineral phase increases with the increase of HF concentration,and the leaching rate of Nb ion reached the maximum at 11 mol·L−1 HF. Tafel results of niobium tantalum ore at different reaction temperatures showed that temperature had a significant effect on the oxidation leaching of niobium tantalum ore. With the increase of temperature,the oxidation leaching rate of niobium tantalum ore was accelerated,and the corrosion current density gradually increased. The corrosion current density tended to flatten out when it reached the maximum value of 959.20 µA·cm−2 at 80 ℃. The dominant activation energy of Nb ion in the oxidation leaching stage was 3.018 kJ·mol−1 based on Arrhenius formula. The results of AC impedance tests of (Fe,Mn)(Nb,Ta)2O6 mineral phase at different reaction temperatures and the determination of Nb ion leaching rate by inductively coupled plasma mass spectrometer (ICP) showed that with the increase of HF concentration,the oxidation current density also increased gradually,reaching the maximum 178.4 µA·cm−2 and 192.5 µA·cm−2 at 80 ℃. As determined by ICP,the oxidation leaching rate of Nb accelerated with the increase of temperature,reaching a maximum of 5.32 mg·L−1·h−1 at 80 ℃. The oxidation reaction rate of Nb ion was basically unchanged as the temperature continues to rise,which might be caused by the change of the double layer structure at the niobium tantalum/liquid interface with the increase of temperature. The results of impedance AC experiments at different temperatures showed that the current density increases with the increase of temperature,reaching the maximum values 192.5 µA·cm−2 at 80 ℃.

quote

GB/T 7714-2015 [1] Xiao Guo, Cong Liang, Qiuju Li, et al. Electrochemical and Kinetic Mechanism of Oxidizing Acid-Leaching Process of Niobium Tantalum Ore[J]. Chinese Journal of Rare Metals, 2025, 49(2): 203-211. DOI:10.13373/j.cnki.cjrm.XY23030038.
MLA [1] Xiao Guo, et al., "Electrochemical and Kinetic Mechanism of Oxidizing Acid-Leaching Process of Niobium Tantalum Ore." Chinese Journal of Rare Metals, vol. 49, no. 2, 2025, pp. 203-211, https://doi.org/10.13373/j.cnki.cjrm.XY23030038.
APA [1] Xiao Guo, Cong Liang, Qiuju Li, & Bowen Han. (2025). Electrochemical and Kinetic Mechanism of Oxidizing Acid-Leaching Process of Niobium Tantalum Ore. Chinese Journal of Rare Metals, 49(2), 203-211. https://doi.org/10.13373/j.cnki.cjrm.XY23030038
IEEE [1] Xiao Guo, Cong Liang, Qiuju Li, and Bowen Han, "Electrochemical and Kinetic Mechanism of Oxidizing Acid-Leaching Process of Niobium Tantalum Ore," Chinese Journal of Rare Metals, vol. 49, no. 2, pp. 203-211, 2025, doi: 10.13373/j.cnki.cjrm.XY23030038. keywords: {niobium tantalum ore;electrochemistry;ore/liquid interface;oxidation leaching rate;surface oxidation mechanism}