Microstructure and Hydrogenation Behaviour of (Ti65Fe35)100-xVx Ternary Alloy AITranslate

Guangxi Key Laboratory of Information Materials,Guilin University of Electronic Technology,Guilin 541004,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Group 5B metals (Nb,V and Ta) and related alloys are considered as promising hydrogen permeation membranes to replace commercial Pd and its alloys. Vanadium-based alloys,as a new substitute for Pd membranes,not only have lower cost but also higher hydrogen permeability. Despite all this,huge challenges remain-especially the poor mechanical stability and high susceptibility to hydrogen embrittlement (HE) which is closely related to high absorbed hydrogen concentration of vanadium. Among group 5B alloys,hydrogenation (thermal-hydrogen treatment technology) has obvious advantages in improving the properties of V-based alloys.However,no relevant research has been carried out on V-TiFe alloys so far. Based on this,the hydrogenation behavior of (Ti65Fe35)100-xVx (x=0,2.5,5,10,15,25),x is the percentage of atoms of V) alloys with low cost and high hydrogen permeability were explored. In the solid state,two operating processes of static hydrogenation and dynamic hydrogenation were used,besides,the effects of hydrogen flow,hydrogenation time and hydrogenation temperature (350 and 450 ℃) on the hydrogenation behavior of the above alloys with different V content were systematically studied by the control variable method. The solidification path,microstructure evolution and mechanical properties of the alloy were analyzed by thermodynamic calculation software (Thermo-Calc),scanning electron microscope (SEM),energy spectrometer (EDS),X-ray diffraction meter (XRD),and Vickers hardness tester. First,the composition-temperature curve obtained from the thermodynamic solidification data of Thermo-Calc using the origin software found that: when 0<x<8,the primary phase was TiFe;when x=8,the alloy appeared fully eutectic;and when 8<x<25,the primary phase was body-centered cubic (bcc)-V.With the decrease of solidification temperature,binary and ternary eutectic reactions occurred successively until the end of solidification. Subsequently,the phase analysis of (Ti65Fe35)100-xVx cast alloys by XRD,SEM and EDS showed that: when 0<x<10,the alloy was composed of the primary TiFe phase and {bcc-(V,Ti)+TiFe} phase;when x=10,the alloy consisted of a divorced eutectic {β-Ti+TiFe};when x>10,the alloy consistd of a primary bcc-(V,Ti) solid solution phase and a small amount of TiFe phase. In addition,exploring the changes of hydrogenation amount of (Ti65Fe35)100-xVx alloys caused by the difference in hydrogen flow,hydrogenation time and hydrogenation temperature,it was found that: when V content was constant,the hydrogenation effect of alloys was proportional to the variable parameters under any single variable parameter such as hydrogen flow,hydrogenation time and hydrogenation temperature,in other words,when the hydrogenation temperature and hydrogen flow kept a constant,the hydrogenation amounts of the alloy grew with the increase of hydrogenation time. After the hydrogenation time reached a certain level,the hydrogenation amount reached the maximum and tends to be stable,the alloy composition also had a decisive influence on the hydrogenation amount of the alloy besides,that was to say,it would cause an increase in hydrogenation with the increase of V content. Finally,the mechanical properties of all alloys of the system were studied,and the hardness of the cast microstructure of (Ti65Fe35)100-xVx cast alloys and the hardness after hydrogenation at 350 and 450 ℃ were measured using Vickers hardness tester. The hardness of the alloy of the hydrogenated V-TiFe system was significantly enhanced compared with the alloy sample before hydrogenation,that was,Vickers hardness of (Ti65Fe35)85V15 alloy after hydrogenation at 450 ℃ was HV0.3 720.4,which was equivalent to 1.12 times before hydrogenation,and the hardness increased with the increase of hydrogenation temperature,which could be attributed to the solid solution strengthening of H atom inside the alloy and the precipitation of hydrides.

KeyWords AITranslate

V-Ti-Fe alloys hydrogenation microstructure Vickers hardness

[1]郭珲,赵刘会. 有色金属基纳米材料及复合材料的研究进展 [J]. 铜业工程,2023,(2): 74.

H Guo,L H Zhao. Research progress of non-ferrous metal-based nanomaterials and composites [J]. Copper Engineering,2023,(2): 74.

[2]吴岱丰,李睿,陈鹏允,周庆,唐仁衡,肖方明. Ti-Mn基高容量固态低压储氢合金研究 [J]. 稀有金属,2023,47(3): 35.

D F Wu,R Li,P Y Chen,Q Zhou,R H Tang,F M Xiao. Properties and structure of Ti-Mn based high-capacity solid low pressure hydrogen storage alloys [J]. Chinese Journal of Rare Metals,2023,47(3): 357.

[3]王舟欣,李帅,蒋利军,米菁,郝雷,林阳. Pd基二元合金膜应用研究进展 [J]. 稀有金属,2023,47(11): 1545.

Z X Wang,S Li,L J Jiang,J Mi,L Hao,Y Lin. Progress of pd-based binary alloy membranes [J]. Chinese Journal of Rare Metals,2023,47(11): 1545.

[4]Merve N D,Ziya E,Kemal D,Evren T,Berkay G,Arcan F D. Microstructural and texture evolution during thermo-hydrogen processing of Ti6Al4V alloys produced by electron beam melting [J]. Materials Characterization,2020,168: 110549.

[5]Froes F H,Senkov O N,Qazi J I. Hydrogen as a temporary alloying element in titanium alloys: thermohydrogen processing [J]. International Materials Reviews,2004,49(3–4): 227.

[6]Huang S,Agyenim-Boateng E,Sheng J,Yuan G,Dai F Z,Ma D H,Zhao J X,Zhou J Z. Effects of laser peening with different laser power densities on the mechanical properties of hydrogenated TC4 titanium alloy [J]. International Journal of Hydrogen Energy,2019,44(31): 17114.

[7]Wu L H,Jia C L,Han S C,Li N,Ni D R,Xiao B L,Ma Z Y,Fu M J,Wang Y Q,Zeng Y S. Superplastic deformation behavior of lamellar microstructure in a hydrogenated friction stir welded Ti-6Al-4V joint [J]. Journal of Alloys and Compounds,2019,787: 1320.

[8]常筠袖,杨帆,张靖晨,杜广煜,王佳聪,姜文全. 温度对TiAl涂层微裂纹扩展影响的分子动力学研究 [J]. 塑性工程学报,2023,30(2): 197.

J X Chang,F Yang,J C Zhang,G Y Du,J C Wang,W Q Jiang. Molecular dynamics study on effect of temperature on micro-crack propagation of TiAl coating [J]. Journal of Plasticity Engineering,2023,30(2): 197.

[9]雷豹,肖平安,周威,范安平,张小虎. 热氢处理对MIMTi-6Al-4V组织及性能的影响 [J]. 稀有金属材料与工程,2013,42(5): 1057.

B Lei,P A Xiao,W Zhou,A P Fan,X H Zhang. Effect of thermal hydrogen treatment on microstructure and properties of MIMTi-6Al-4V [J]. Rare Metal Materials and Engineering,2013,42(5): 1057.

[10]冯欣欣,衣晓洋,王海振,张尚洲,高智勇,孟祥龙. Ti-V-Al轻质记忆合金的研究进展 [J]. 有色金属科学与工程,2021,2(6): 72.

X X Feng,X Y Yi,H Z Wang,S Z Zhang,Z Y Gao,X L Meng. Research progress of Ti-V-Al lightweight shape memory alloys [J]. Nonferrous Metals Science and Engineering,2021,12(6): 72.

[11]张少卿. 氢在钛合金热加工中的作用 [J]. 材料工程,1992,(2): 24.

S Q Zhang. The role of hydrogen in the thermal processing of titanium alloys [J]. Journal of Materials Engineering,1992,(2): 24.

[12]唐敏,陈莉君,王轩,栾佰峰,刘庆. 置氢处理对铸态TiZrAlV合金高温变形行为及显微组织的影响 [J]. 稀有金属材料与工程,2021,50(2): 7.

M Tang,L J Chen,X Wang,B F Luan,Q Liu. Effect of hydrogen placement on high temperature deformation behavior and microstructure of cast TiZrAlV alloy [J]. Rare Metal Materials and Engineering,2021,50(2): 7.

[13]张伟福,李淼泉,林莺莺. 置氢Ti-6Al-4V 钛合金的热压缩变形行为研究 [J]. 塑性工程学报,2008,15(6): 107.

W F Zhang,M Q Li,Y Y Lin. Study on thermocompression deformation behavior of hydrogen Ti-6Al-4V titanium alloy [J]. Chinese Journal of Plastic Engineering,2008,15(6): 107.

[14]侯红亮,黄重国,王耀奇. 置氢Ti-6Al-4V合金组织演变与超塑性能 [J]. 北京科技大学学报,2008,30(11): 1270.

H L Hou,C G Huang,Y Q Wang. Microstructure evolution and superplastic properties of hydrogen Ti-6Al-4V alloy [J]. Journal of University of Science and Technology Beijing,2008,30(11): 1270.

[15]李晓华,牛勇,侯红亮,李志强. 置氢 Ti-6Al-4V 合金显微组织演变与高温变形行为 [J]. 中国有色金属学报,2008,18(8): 1414.

X H Li,Y Niu,H L Hou,Z Q Li. Microstructure evolution and high temperature deformation behavior of hydrogen Ti-6Al-4V alloy [J]. Chinese Journal of Nonferrous Metals,2008,18(8): 1414.

[16]Xiong W,Luo J F,Wang B,Li X F,Chen J. High temperature creep behavior of hydrogenated Ti-6Al-4V alloy [J]. International Journal of Lightweight Materials and Manufacture,2020,3(3): 298.

[17]Hashi K,Ishikawa K,Matsuda T,Aoki K. Hydrogen permeation characteristics of (V,Ta)-Ti-Ni alloys [J]. Journal of Alloys and Compounds,2005,404: 273.

[18]Song G,Dolan M D,Kellam M E,Ling D,Zambelli S. V-Ni-Ti multiphase alloy membranes for hydrogen purification [J]. Journal of alloys and compounds,2011,509(38): 9322.

[19]Niu J,Guo Y,Li K,Liu W,Dan Z,Sun Z,Chang H,Zhou L,Improved mechanical,bio-corrosion properties and in vitro cell responses of Ti-Fe alloys as candidate dental implants [J]. Materials Science and Engineering: C,2021,122: 111917.

[20]Suzuki A,Yukawa H,Ijiri S,Nambu T,Matsumoto Y,Murata Y. Alloying effects on hydrogen solubility and hydrogen permeability for V-based alloy membranes [J]. Materials Transactions,2015,56(10): 1688.

[21]Yan E H,Sun L X,Xu F,Xu D M,Qiu S J,Xiang C L,Zhang H Z,Sun Y X. Changes in microstructure,solidification path and hydrogen permeability of Nb-Hf-Co alloy by adjusting Hf/Co ratio [J]. International Journal of Hydrogen Energy,2016,41(3): 1391.

[22]Yan E H,Li X Z,Rettenmayr M,Liu D M,Su Y Q,Guo J J,Xu D M,Fu H Z. Design of hydrogen permeable Nb-Ni-Ti alloys by correlating the microstructures,solidification paths and hydrogen permeability [J]. International Journal of Hydrogen Energy,2014,39(7): 3505.

[23]Kostov A,Živković D. Thermodynamic analysis of alloys Ti-Al,Ti-V,Al-V and Ti-Al-V [J]. Journal of Alloys and Compounds,2008,460(1-2): 164.

[24]Huang F F,Li X Z,Shan X R,Guo J J,Gallucci F,Annaland M,Liu D M.hydrogen transport through the V-Cr-Al alloys: hydrogen solution,permeation and thermal-stability [J]. Separation and Purification Technology,2020,240: 116654.

[25]Jiang P,Huang H C,Sun B,Song G S,Wu W P,Wang Z Z,Zhang Y. Microstructure,mechanical properties and hydrogen permeability of multiphase V-Ti-Ni alloy membranes [J]. Materials Today Communications,2020,24: 101112.

[26]Vinit K,Punit K,Keisuke T,Pratibha. Hydrogen adsorption studies of TiFe surfaces via 3-d transition metal substitution [J]. International Journal of Hydrogen Energy,2022,47(36): 16156.

[27]Hamasaki Y,Miyajima Y,Ishikawa K. Microstructural changes and hydrogen permeability of rolled and annealed Nb30Ti35Co35 alloys [J]. Materials Transactions,2022,63(7): 981.

[28]王静. Fe-(Ti,V)C复合材料耐磨性研究 [J]. 热加工工艺,2013,42(14): 83.

J Wang. Study on wear resistance of Fe-(Ti,V)C composites [J]. Hot Working Technology,2013,42(14): 83.

[29]Galina P G,Ekaterina N S,Ilya V R,I.P M,Olga V Z. Effect of hydrogen on the development of superplastic deformation in the submicrocrystalline Ti-6Al-4V alloy [J]. Materials Science Forum,2016,4248(838-839): 344.

[30]Ma T F,Chen R R,Zheng D S,Guo J J,Ding H S,Su Y Q,Fu H Z. Hydrogen enhanced the room-temperature compressive properties of Ti44Al6Nb alloy [J]. Materials Letters,2018,213: 170.

[31]肖宏伟,赵敬伟,赵文娟,宋丹,杜刚,丁桦,王耀奇. 置氢对 Ti6Al4V 合金微观组织和硬度的影响 [J]. 稀有金属材料与工程,2008,37(10): 1795.

H W Xiao,J W Zhao,W J Zhao,D Song,G Du,H Ding,Y Q Wang. Effect of hydrogen on microscopic microstructure and hardness of Ti6Al4V alloy [J]. Rare Metal Materials and Engineering,2008,37(10): 1795.

[32]Zhang Y H,Li C,Yuan Z M,Qi Y,Guo S H,Zhao D L. Research progress of TiFe-based hydrogen storage alloys [J]. Journal of Iron and Steel Research International,2022,29(4): 537.

[33]Sujan G K,Pan Z X,Li H J,Liang D,Alam N. An overview on TiFe intermetallic for solid-state hydrogen storage: microstructure,hydrogenation and fabrication processes [J]. Critical Reviews in Solid State and Materials Sciences,2020,45(5): 410.

[34]Zadorozhnyy V Y,Milovzorov G S,Klyamkin S N,Zadorozhnyy M Y,Strugova D V,Gorshenkov M V,Kaloshkin S D. Preparation and hydrogen storage properties of nanocrystalline TiFe synthesized by mechanical alloying [J]. Progress in Natural Science: Materials International,2017,27(1): 149.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY22120020

Chinese Library Classification Number:TG146

Citation Information:

Group 5B metals (Nb,V and Ta) and related alloys are considered as promising hydrogen permeation membranes to replace commercial Pd and its alloys. Vanadium-based alloys,as a new substitute for Pd membranes,not only have lower cost but also higher hydrogen permeability. Despite all this,huge challenges remain-especially the poor mechanical stability and high susceptibility to hydrogen embrittlement (HE) which is closely related to high absorbed hydrogen concentration of vanadium. Among group 5B alloys,hydrogenation (thermal-hydrogen treatment technology) has obvious advantages in improving the properties of V-based alloys.However,no relevant research has been carried out on V-TiFe alloys so far. Based on this,the hydrogenation behavior of (Ti65Fe35)100-xVx (x=0,2.5,5,10,15,25),x is the percentage of atoms of V) alloys with low cost and high hydrogen permeability were explored. In the solid state,two operating processes of static hydrogenation and dynamic hydrogenation were used,besides,the effects of hydrogen flow,hydrogenation time and hydrogenation temperature (350 and 450 ℃) on the hydrogenation behavior of the above alloys with different V content were systematically studied by the control variable method. The solidification path,microstructure evolution and mechanical properties of the alloy were analyzed by thermodynamic calculation software (Thermo-Calc),scanning electron microscope (SEM),energy spectrometer (EDS),X-ray diffraction meter (XRD),and Vickers hardness tester. First,the composition-temperature curve obtained from the thermodynamic solidification data of Thermo-Calc using the origin software found that: when 0<x<8,the primary phase was TiFe;when x=8,the alloy appeared fully eutectic;and when 8<x<25,the primary phase was body-centered cubic (bcc)-V.With the decrease of solidification temperature,binary and ternary eutectic reactions occurred successively until the end of solidification. Subsequently,the phase analysis of (Ti65Fe35)100-xVx cast alloys by XRD,SEM and EDS showed that: when 0<x<10,the alloy was composed of the primary TiFe phase and {bcc-(V,Ti)+TiFe} phase;when x=10,the alloy consisted of a divorced eutectic {β-Ti+TiFe};when x>10,the alloy consistd of a primary bcc-(V,Ti) solid solution phase and a small amount of TiFe phase. In addition,exploring the changes of hydrogenation amount of (Ti65Fe35)100-xVx alloys caused by the difference in hydrogen flow,hydrogenation time and hydrogenation temperature,it was found that: when V content was constant,the hydrogenation effect of alloys was proportional to the variable parameters under any single variable parameter such as hydrogen flow,hydrogenation time and hydrogenation temperature,in other words,when the hydrogenation temperature and hydrogen flow kept a constant,the hydrogenation amounts of the alloy grew with the increase of hydrogenation time. After the hydrogenation time reached a certain level,the hydrogenation amount reached the maximum and tends to be stable,the alloy composition also had a decisive influence on the hydrogenation amount of the alloy besides,that was to say,it would cause an increase in hydrogenation with the increase of V content. Finally,the mechanical properties of all alloys of the system were studied,and the hardness of the cast microstructure of (Ti65Fe35)100-xVx cast alloys and the hardness after hydrogenation at 350 and 450 ℃ were measured using Vickers hardness tester. The hardness of the alloy of the hydrogenated V-TiFe system was significantly enhanced compared with the alloy sample before hydrogenation,that was,Vickers hardness of (Ti65Fe35)85V15 alloy after hydrogenation at 450 ℃ was HV0.3 720.4,which was equivalent to 1.12 times before hydrogenation,and the hardness increased with the increase of hydrogenation temperature,which could be attributed to the solid solution strengthening of H atom inside the alloy and the precipitation of hydrides.

quote

GB/T 7714-2015 [1] Jinwang Bai, Erhu Yan, Dongshuai Ma, et al. Microstructure and Hydrogenation Behaviour of (Ti65Fe35)100-xVx Ternary Alloy[J]. Chinese Journal of Rare Metals, 2025, 49(2): 163-173. DOI:10.13373/j.cnki.cjrm.XY22120020.
MLA [1] Jinwang Bai, et al., "Microstructure and Hydrogenation Behaviour of (Ti65Fe35)100-xVx Ternary Alloy." Chinese Journal of Rare Metals, vol. 49, no. 2, 2025, pp. 163-173, https://doi.org/10.13373/j.cnki.cjrm.XY22120020.
APA [1] Jinwang Bai, Erhu Yan, Dongshuai Ma, Hao Wang, Yongjin Zou, Hailiang Chu, & Lixian Sun. (2025). Microstructure and Hydrogenation Behaviour of (Ti65Fe35)100-xVx Ternary Alloy. Chinese Journal of Rare Metals, 49(2), 163-173. https://doi.org/10.13373/j.cnki.cjrm.XY22120020
IEEE [1] Jinwang Bai, Erhu Yan, Dongshuai Ma, Hao Wang, Yongjin Zou, Hailiang Chu, and Lixian Sun, "Microstructure and Hydrogenation Behaviour of (Ti65Fe35)100-xVx Ternary Alloy," Chinese Journal of Rare Metals, vol. 49, no. 2, pp. 163-173, 2025, doi: 10.13373/j.cnki.cjrm.XY22120020. keywords: {V-Ti-Fe alloys;hydrogenation;microstructure;Vickers hardness}