daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Leaching Behavior of Silver in Reduction Acid Leaching Process of Mn-Ag Paragenesis Ore AITranslate

1.Institute of Resources Utilization and Rare Earth Development,Guangdong Academy of Sciences,Guangzhou 510651,China
2.Yunnan Key Laboratory of Green Separation and Enrichment of Strategic Mineral Resources,Kunming University of Science and Technology,Kunming 650093,China
3.Southwest United Graduate School,Kunming 650092,China
4.State Key Laboratory of Rare Metal Separation and Comprehensive Utilization,Guangzhou 510651,China
5.Guangdong Provincial Key Laboratory of Development & Comprehensive Utilization of Mineral Resources,Guangzhou 510651,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Manganese-silver ore is an important precious metal strategic resource in China,it often associated with copper,gold,iron,and other minerals. Under the weathering and other environmental effects,Cu2+,Ag+,Pb2+,and other cations can enter the manganese minerals’ tunnel structure,which forming a multi-metal paragenesis ore with extremely complex mineralogical properties. Therefore,it is difficult to study mineralogy,beneficiation-metallurgy technology and engineering in the utilization of such resources. These situations had led to a low-level development and comprehensive utilization rate of multi-metals for a long time. The ore sample came from Fe-Mn-Ag polymetallic ore in Yunnan,China. Raw ore was prepared by crushing,grinding,and high gradient magnetic separation (HGMS),the research object was obtained. This article conducted chemical multi-element analysis,mineral liberation analyzer (MLA)mineral composition analysis,silver phase analysis,potential-pH (Eh-pH)relationship analysis,solution chemistry analysis,and scanning electron microscopy-energy dispersive spectrometer (SEM-EDS)analysis. The article systematically studied the main mineral types and contents in ores,the chemical phase composition of silver,the influence of acidic leaching pH on silver recovery,the leaching Eh-pH relationship of iron and manganese,the precipitation conditions of iron hydroxide,the mineral composition analysis of acid leaching residue,the particle size composition and metal distribution of silver in acid leaching residue,and the reaction relationship characterized between silver sulfate and iron colloids by SEM-EDS. The results showed that Ag content in the sample was 66.81×10−6,Mn content was 2.58%,and Fe content was 43.58%. The content of Mn and Ag were low relatively,and the main element was Fe. Most of the minerals in the sample were limonite,with a content of 70.18%,followed by manganese minerals with a content of 9.17%. The content of visible silver mineral was low,and the main gangue minerals were quartz and dolomite. The distribution rate of silver combined with manganese was 75.47%,while the distribution rate of silver combined with limonite was 6.78%. The content of native silver and silver sulfide were low. When pH of acid leaching was 3,the actual recovery rate of silver reached its highest value,and as pH further decreased,the silver recovery rate decreased significantly. Eh-pH relationship of Fe and Mn in this reaction system was calculated by hydrocarbon system calculator (HSC)chemistry software. Mn2+ in the acid leaching solution had a wide range solubility,even in alkaline environments,so it would not have a significant impact on the material composition of the acid leaching solution. Under conditions of insufficient acid dosage,Fe would form Fe(OH)SO4 and Fe(OH)3 colloids or precipitates. Under conditions of excessive acid,iron colloids would react with H+ and SO42−to form Fe2(SO4)3,which was soluble. At the same time,Fe2+ or Fe3+ would be hydrolyzed to form Fe(OH)2 and Fe(OH)3 precipitates. According to solution chemistry calculations,the theoretical pH at which Fe(OH)3 began to precipitate was about 1.48,and the theoretical pH at precipitated completely was about 2.82. Based on the above analysis,a principle model for the coagulation of silver sulfate by iron colloids had been designed. Through the study of acid leaching residue,it was found that FeOOH-colloid (colloidal hydroxide iron oxide)was a new substance in the acid leaching reaction,with a mineral content of 7.54%. Further analysis showed that the products were the final substance of the aging reaction of colloidal precipitates,such as Fe(OH)3. Ag distribution rate in acid leaching residue was mainly concentrated in the fine particle size of -0.020 mm,especially in -0.010 mm particle size,where Ag content was as high as 432×10−6. This phenomenon indicated a significant enrichment effect,and the particle size of newly formed silver sulfate was finer generally. In SEM images,a large amount of FeOOH-colloid could be observed in the acid leaching residue,which was dispersed by ultrasonic waves,but no silver was found. The overall particle size of FeOOH-colloid was extremely fine,even reaching the micro-nano scale. In the agglomerative state of the sample (without ultrasonic waves treated),EDS could detect the points with high silver content. Ag content was 4%~15% and sulfur trioxide content was 4%~11%,which proved the presence of silver sulfate. EDS surface scanning analysis revealed that Ag element was extremely dispersed in the iron colloid,with high brightness clusters appearing in some positions. The two-dimensional spatial scale of silver reached the nanometer level. At the same time,the results showed that the iron colloid can adsorb silver sulfate precipitation. These findings provided some theoretical supports for the efficient utilization of refractory manganese silver resources.

KeyWords AITranslate

manganese and silver paragenesis ore reducing acid leaching leaching behavior agglomerate

[1]余丽秀,孙亚光,尚红卫. 中国含银锰矿资源分布及属性研究[J].中国锰业,2009,27(3):1.

L X Yu,Y G Sun,H W Shang. The study of resources distributing and characteristic of manganese ore of contain silver on China[J].China's Manganese Industry,2009,27(3):1.

[2]黄晓梅,李国斌,胡亮,苏毅. 银的提取研究进展及前景展望[J].稀有金属,2015,39(3):268.

X M Huang,G B Li,L Hu,Y Su. Research progress and prospect of extracting silver[J].Chinese Journal of Rare Metals,2015,39(3):268.

[3]杨洪英,巩恩普,范有静. 广西某锰银矿工艺矿物学及锰的赋存状态[J].东北大学学报(自然科学版),2006,27(2):199.

H Y Yang,E P Gong,Y J Fan. Technological mineralogy and manganese occurrence state of a manganese-silver deposit in Guangxi[J].Journal of Northeastern University (Natural Science),2006,27(2):199.

[4]Qing T,Hong Z,Shuai W,Jin Z L,Guang Y L. Reductive leaching of manganese oxide ores using waste tea as reductant in sulfuric acid solution[J].Transactions of Nonferrous Metals Society of China,2014,24(3):861.

[5]蒋英,邱显扬,梁冬云,李波,王成行. 云南北衙金铁氧化矿金银赋存状态与选冶回收研究[J].稀有金属,2019,43(9):974.

Y Jiang,X Y Qiu,D Y Liang,B Li,C H Wang. Au-Ag properties and benefucation of Beiya Au-Fe oxidized ore deposit in Yunnan Province,China[J].Chinese Journal of Rare Metals,2019,43(9):974.

[6]张斌,姜涛,杨永斌. 从锰银矿中一步法浸出锰和银的热力学基础与应用[J].中国有色金属学报,2007,17(11):1887.

B Zhang,T Jiang,Y B Yang. Fundamentals and applications of simultaneous leaching of manganese and silver from manganese-silver associated ore[J].The Chinese Journal of Nonferrous Metals,2007,17(11):1887.

[7]张斌,姜涛,陈启元,杨永斌. 锰银矿一步法浸出动力学探讨[J].矿产保护与利用,2001,(2):43.

B Zhang,T Jiang,Q Y Cheng,Y B Yang. Dynamics on simultaneous leaching of manganese and silver[J].Conservation and Utilization of Mineral Resources,2001,(2):43

[8]宋宝旭. 难选金银铁氧化矿粗磨-分类磁选-分组提取金银的选冶理论与工艺[D]. 昆明:昆明理工大学,2016. 15.

B X Song. The Beneficiation-Leaching Theory and Process of Coarse Grinding-Classified by Magnetic Separation-Leaching Separately to Comprehensive Utilize the Refractory Gold-Silver-Iron Oxidized Ore[D]. Kuming:Kuming University of Science and Technology,2016. 15.

[9]梁冬云,邱显扬,蒋英,李波,李美荣. 北衙金矿锰矿物类型与负载金属离子规律性[J].中国有色金属学报,2020,30(10):2444.

D Y Liang,X Y Qiu,Y Jiang,B Li,M R Li. Types of manganese minerals and regularity of loaded metal ions in Beiya gold deposit[J].The Chinese Journal of Nonferrous Metals,2020,30(10):2444.

[10]朱佳俊,谢铿,黄凯,郭学益. 葡萄皮选择性吸附黄金的机制研究[J].稀有金属,2024,48(10):1436.

J J Zhu,K Xie,K Huang,X Y Guo. Selective adsorption mechanism of gold by grape peel[J].Chinese Journal of Rare Metals,2024,48(10):1436.

[11]李波,邱显扬,梁冬云,蒋英,李美荣. 天然载银隐钾锰矿分子级孔道结构与银离子占位替代研究[J].稀有金属,2020,44(12):1308.

B Li,X Y Qiu,D Y Liang,Y Jiang,M R Li. Tunnel structure of molecular dimensions and substitution of silver ions in natural silver bearing cryptomelane[J].Chinese Journal of Rare Metals,2020,44(12):1308.

[12]黄清源,刘志强,李伟. 锰银矿还原浸出工艺现状[J].材料研究与应用,2015,9(2):69.

Q Y Huang,Z Q Liu,W Li. State of art of manganese-silver ore reduction leaching process[J].Materials Research and Application,2015,9(2):69.

[13]苏成德,赵礼兵,安雪梅. 从难选锰银矿尾矿中回收银的研究[J].中国矿业,2008,17(1):89.

C D Su,L B Zhao,X M An. A research for silver recovery from silver-manganese ore[J].China Mining Magazine,2008,17(1):89.

[14]郭嘉诚,金永丽,赵增武. 微波场中铌、 铁选择性还原行为研究[J].稀有金属,2024,48(1):68.

J C Guo,Y L Jin,Z W Zhao. Selective reduction of niobium and iron in microwave field[J].Chinese Journal of Rare Metals,2024,48(1):68.

[15]秦兵,张伟东,李淑贤. 磁性表面分子印迹聚合物的制备及对梓醇的选择性吸附[J].分析试验室,2024,43(3):394.

B Qin,W D Zhang,S X Li. Preparation of magnetic surface molecular imprinted polymer and its selective adsorption for catalpol[J].Chinese Journal of Analysis Laboratory,2024,43(3):394.

[16]赵成东,王宁,顾汉念,温汉捷,田元江. 云南某锰银矿特征及湿法分离实验研究[J].矿冶工程,2015,35(2):111.

C D Zhao,N Wang,H N Gu,H J Wen,Y J Tian. Characteristics and hydrometallurgical processing of manganese-silver ore from Yunnan[J].Mining and metallurgical Engineering,2015,35(2):111.

[17]郎淳慧,张鸣昕,崔商哲,王法春,任洪胜,刘新艳,韩治纬. 硫精矿浮选-焙烧综合利用硫酸烧渣中铁试验研究[J].黄金,2023,44(3):48.

C H Lang,M X Zhang,S Z Cui,F C Wang,H S Ren,X Y Liu,Z W Han. Experimental study on the comprehensive utilization of iron in the sulfuric acid slag by sulfur concentrate flotation-roasting[J].Gold,2023,44(3):48.

[18]Zhang C,Wang S,Cao Z F,Zhong H. Two-stage leaching of manganese and silver from manganese-silver ores by reduction with calcium sulfide and oxidation with copper(Ⅱ)[J].Hydrometallurgy,2018,175:240.

[19]Manish K S,Walter P. Reducing agents in the leaching of manganese ores:a comprehensive review[J].Hydrometallurgy,2019,187:168.

[20]徐本军,丁先胜,黄彩娟. 某锰银矿富银浸出渣的硫脲浸出研究[J].矿冶工程,2013,33(4):88.

B J Xu,X S Ding,C J Huang. Thiourea leaching of silver-rich leach residue of some manganese-silver ore[J].Mining and Metallurgical Engineering,2013,33(4):88.

[21]Li Q,Rao X F,Xu B,Yang Y B,Liu T,Jiang T,Hu L. Extraction of manganese and zinc from their compound ore by reductive acid leaching[J].Transactions of Nonferrous Metals Society of China,2017,27(5):1172.

[22]Zhao Q,Sun L,Wang G X,Luo C H,Shun Y,Yan K P. Novel reduction roasting and leaching method for manganese dioxide ore using Fe-P slag as the reductant[J].Hydrometallurgy,2019,189:105.

[23]Xiong S F,Li X,Liu P L,Hao S H,Hao F,Yin Z L,Liu J X. Recovery of manganese from low-grade pyrolusite ore by reductively acid leaching process using lignin as a low cost reductant[J].Minerals Engineering,2018,125:126.

[24]于元进. 从锰银矿湿法提银的尾矿中回收银的研究[J].中国锰业,2015,33(1):28.

Y J Yu. Recovery of silver from the tailings produced by treating silver-manganese ore[J].China's Manganese Industry,2015,33(1):28.

[25]贺跃,李明东,杨攀,王松,王海峰,王家伟. 电解锰阳极渣吸附硫酸锰溶液中钼的行为研究[J].有色金属科学与工程,2022,13(6):1.

Y He,M D Li,P Yang,S Wang,H F Wang,J W Wang. Study on the adsorption behavior of molybdenum in manganese sulfate solution by electrolytic manganese anode slag[J].Nonferrous Metals Science and Engineering,2022,13(6):1.

[26]Li W,Liu Z Q,Huang Q Y,Tang Y L,Qiu X Y. Extraction of low-grade silver from a refractory Au-Ag ore in cyanidation by pretreatment with reductive alkaline leaching[J].Hydrometallurgy,2016,164:257.

[27]杨明学,罗庆教,楚立军,尹延西. 锌冶炼过程中浸渣加压还原酸浸除铁工艺优化[J].铜业工程,2023,(4):159.

M X Yang,Q J Luo,L J Chu,Y X Yin. Process optimization of iron removal by pressure reduction acid leaching of residue in hydrometallurgical zinc[J].Copper Engineering,2023,(4):159.

[28]孙亚光,余丽秀. 过氧化氢湿法处理锰银矿工艺[J].中国锰业,2003,21(2):13.

Y G Sun,L X Yu. Study on technique of reduction of Mn-Ag ore with hydrogen peroxide[J].China's Manganese Industry,2003,21(2):13.

[29]Erik P,Etipurwaningsih W. Selective-reductive leaching of manganese from low-grade manganese ore using tannic acid as reductant[J].Mining,Metallurgy & Exploration,2019,71(12):50.

[30]刘祁. 云南某锰银矿选冶联合工艺选矿部分设计研究[J].矿业工程,2017,15(2):22.

Q Liu. Study on beneficiation design for a manganese-silver ore in Yunnan[J].Mining Engineering,2017,15(2):22.

[31]Tian Y,Shu J C,Chen M J,Wang J Y,Wang Y,Luo Z G,Wang R,Yang F H,Xiu F R,Sun Z. Manganese and ammonia nitrogen recovery from electrolytic manganese residue by electric field enhanced leaching[J].Journal of Cleaner Production,2019,236:117.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY24090016

Chinese Library Classification Number:TD865

Citation Information:

Manganese-silver ore is an important precious metal strategic resource in China,it often associated with copper,gold,iron,and other minerals. Under the weathering and other environmental effects,Cu2+,Ag+,Pb2+,and other cations can enter the manganese minerals’ tunnel structure,which forming a multi-metal paragenesis ore with extremely complex mineralogical properties. Therefore,it is difficult to study mineralogy,beneficiation-metallurgy technology and engineering in the utilization of such resources. These situations had led to a low-level development and comprehensive utilization rate of multi-metals for a long time. The ore sample came from Fe-Mn-Ag polymetallic ore in Yunnan,China. Raw ore was prepared by crushing,grinding,and high gradient magnetic separation (HGMS),the research object was obtained. This article conducted chemical multi-element analysis,mineral liberation analyzer (MLA)mineral composition analysis,silver phase analysis,potential-pH (Eh-pH)relationship analysis,solution chemistry analysis,and scanning electron microscopy-energy dispersive spectrometer (SEM-EDS)analysis. The article systematically studied the main mineral types and contents in ores,the chemical phase composition of silver,the influence of acidic leaching pH on silver recovery,the leaching Eh-pH relationship of iron and manganese,the precipitation conditions of iron hydroxide,the mineral composition analysis of acid leaching residue,the particle size composition and metal distribution of silver in acid leaching residue,and the reaction relationship characterized between silver sulfate and iron colloids by SEM-EDS. The results showed that Ag content in the sample was 66.81×10−6,Mn content was 2.58%,and Fe content was 43.58%. The content of Mn and Ag were low relatively,and the main element was Fe. Most of the minerals in the sample were limonite,with a content of 70.18%,followed by manganese minerals with a content of 9.17%. The content of visible silver mineral was low,and the main gangue minerals were quartz and dolomite. The distribution rate of silver combined with manganese was 75.47%,while the distribution rate of silver combined with limonite was 6.78%. The content of native silver and silver sulfide were low. When pH of acid leaching was 3,the actual recovery rate of silver reached its highest value,and as pH further decreased,the silver recovery rate decreased significantly. Eh-pH relationship of Fe and Mn in this reaction system was calculated by hydrocarbon system calculator (HSC)chemistry software. Mn2+ in the acid leaching solution had a wide range solubility,even in alkaline environments,so it would not have a significant impact on the material composition of the acid leaching solution. Under conditions of insufficient acid dosage,Fe would form Fe(OH)SO4 and Fe(OH)3 colloids or precipitates. Under conditions of excessive acid,iron colloids would react with H+ and SO42−to form Fe2(SO4)3,which was soluble. At the same time,Fe2+ or Fe3+ would be hydrolyzed to form Fe(OH)2 and Fe(OH)3 precipitates. According to solution chemistry calculations,the theoretical pH at which Fe(OH)3 began to precipitate was about 1.48,and the theoretical pH at precipitated completely was about 2.82. Based on the above analysis,a principle model for the coagulation of silver sulfate by iron colloids had been designed. Through the study of acid leaching residue,it was found that FeOOH-colloid (colloidal hydroxide iron oxide)was a new substance in the acid leaching reaction,with a mineral content of 7.54%. Further analysis showed that the products were the final substance of the aging reaction of colloidal precipitates,such as Fe(OH)3. Ag distribution rate in acid leaching residue was mainly concentrated in the fine particle size of -0.020 mm,especially in -0.010 mm particle size,where Ag content was as high as 432×10−6. This phenomenon indicated a significant enrichment effect,and the particle size of newly formed silver sulfate was finer generally. In SEM images,a large amount of FeOOH-colloid could be observed in the acid leaching residue,which was dispersed by ultrasonic waves,but no silver was found. The overall particle size of FeOOH-colloid was extremely fine,even reaching the micro-nano scale. In the agglomerative state of the sample (without ultrasonic waves treated),EDS could detect the points with high silver content. Ag content was 4%~15% and sulfur trioxide content was 4%~11%,which proved the presence of silver sulfate. EDS surface scanning analysis revealed that Ag element was extremely dispersed in the iron colloid,with high brightness clusters appearing in some positions. The two-dimensional spatial scale of silver reached the nanometer level. At the same time,the results showed that the iron colloid can adsorb silver sulfate precipitation. These findings provided some theoretical supports for the efficient utilization of refractory manganese silver resources.

quote

GB/T 7714-2015 [1] Peilun Li, Xianyang Qiu, Dianwen Liu, et al. Leaching Behavior of Silver in Reduction Acid Leaching Process of Mn-Ag Paragenesis Ore[J]. Chinese Journal of Rare Metals, 2025, 49(5): 737-747. DOI:10.13373/j.cnki.cjrm.XY24090016.
MLA [1] Peilun Li, et al., "Leaching Behavior of Silver in Reduction Acid Leaching Process of Mn-Ag Paragenesis Ore." Chinese Journal of Rare Metals, vol. 49, no. 5, 2025, pp. 737-747, https://doi.org/10.13373/j.cnki.cjrm.XY24090016.
APA [1] Peilun Li, Xianyang Qiu, Dianwen Liu, Kaizhi Yang, & Peilun Shen. (2025). Leaching Behavior of Silver in Reduction Acid Leaching Process of Mn-Ag Paragenesis Ore. Chinese Journal of Rare Metals, 49(5), 737-747. https://doi.org/10.13373/j.cnki.cjrm.XY24090016
IEEE [1] Peilun Li, Xianyang Qiu, Dianwen Liu, Kaizhi Yang, and Peilun Shen, "Leaching Behavior of Silver in Reduction Acid Leaching Process of Mn-Ag Paragenesis Ore," Chinese Journal of Rare Metals, vol. 49, no. 5, pp. 737-747, 2025, doi: 10.13373/j.cnki.cjrm.XY24090016. keywords: {manganese and silver;paragenesis ore;reducing acid leaching;leaching behavior;agglomerate}