A Novel Artificial Biomass Polymer SEI Film for Highly Stable Zn Anode AITranslate

School of Environment and Resources,Chongqing Technology and Business University,Chongqing 400067,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The overuse of fossil fuels has caused serious harm to the environment and undermined the overall sustainable development of mankind. Therefore,the development and application of renewable clean energy has become a hot research field,and the use of stable charge and discharge electrochemical energy storage devices to store and collect dispersed clean energy has also attracted great attention from academia and industry around the world. Lithium-ion batteries (LIBs)have significant theoretical capacity,excellent performance in secondary battery systems,and have been effectively applied in mobile phones,notebook computers,and other products,maintaining a dominant position in the commercial field. However,LIBs carry specific safety risks,including the use of flammable and explosive organic electrolytes. In addition,with increasing challenges such as depletion of lithium reserves and soaring costs,it is imperative to develop and successfully commercialize a very safe,economically viable,and environmentally sustainable battery storage system. Among the many options,aqueous-based zinc-ion batteries (AZIBs)with high safety and stable charge-discharge performance are widely considered to be one of the most promising. AZIBs have the following advantages:1)the natural abundance of zinc metal is high,2)the electrolyte used in the battery is water,which is environmentally friendly and safe compared to the flammable organic electrolyte of lithium-ion batteries,3)the theoretical specific capacity is high (820 mAh·g−1),and 4)the redox potential is low (compared to the standard hydrogen electrode:–0.762 V). However,the zinc anode of aqueous zinc-ion batteries encounters significant challenges,including hydrogen evolution,corrosion passivation,and pronounced zinc dendrite growth,resulting in diminished battery capacity,inferior cycling stability,and reduced coulombic efficiency,thereby constraining the advancement and utilization of aqueous zinc-ion batteries. Among many strategies,the artificial solid electrolyte interphase (SEI)membrane is considered to be one of the simple and efficient strategies,as it can completely inhibit the interaction between the zinc anode and the electrolyte,while regulating the diffusion kinetics of Zn2+ cations. In this study,furfuryl alcohol/aspartic acid (FA/ASP)artificial SEI film was constructed on the surface of zinc anode by esterification using the cheap and easily obtained furfuryl alcohol biomass and aspartic acid as raw materials. FA/ASP artificial SEI film had many polar groups containing oxygen and nitrogen,which enhanced the zincophile of the zinc anode,promoted the uniform deposition of Zn2+,and hindered the growth of zinc dendrites. FA/ASP artificial SEI film also hindered the direct contact between aqueous electrolyte and zinc anode,reduced the reactivity of hydrogen evolution reaction,inhibited the occurrence of hydrogen evolution reaction,and improved the corrosion resistance of zinc anode. Therefore,Zn||Zn-symmetric battery assembled based on FA/ASP@Zn could work stably for 950 h at 1 mA·cm−2 and 1 mAh·cm−2,with an average Coulomb efficiency (CE)of about 98%. And FA/ASP@Zn||Cu asymmetric cell could stably cycle for 270 h,which was almost three times more than the bare Zn||Cu asymmetric cell. Meanwhile,FA/ASP@Zn||V2O5 full battery also showed an enhanced reversible capacity of 157 mAh·g−1 at 1 A·g−1 and CE could reach up to 100%. The significant improvement in cycle stability and coulomb efficiency illustrated the great potential of artificial solid electrolyte interface films based on this biomass for stabilizing zinc-ion battery anodes.

KeyWords AITranslate

aqueous zinc ion batteries (AZIBs) Zn anode solid electrolyte interphase (SEI)film zinc dendrite corrosion

[1]徐杰,阮挺婷,马全新,孙蓉,路胜利. 水系锌离子电池负极改性策略研究进展[J].有色金属科学与工程,2024,15(4):513.

J Xu,T T Ruan,Q X Ma,R Sun,S L Lu. Advances in anode modification strategies for aqueous zinc ion batteries[J].Nonferrous Metals Science and Engineering,2024,15(4):513.

[2]Xiong Y,Dai J H,Kuang L Y,Li X D,Gu X X. Advancements in the exploration of gel electrolytes for aqueous zinc ion batteries[J].Bulletin of Chemical Reaction Engineering & Catalysis,2023,18(3):442.

[3]乔亚峰,万小涵,马文会,李绍元,席风硕. 热等离子法制备锂离子电池硅碳负极材料[J].有色金属工程,2023,13(8):28.

Y F Qiao,X H Wan,W H Ma,S Y Li,F S Xi. Preparation of silicon/carbon matieral by thermal plasma method for lithium-ion battery application[J].Nonferrous Metals Engineering,2023,13(8):28.

[4]Gu X X,Qiao S,Ren X L,Liu X Y,He Y Z,Liu X T,Liu T F. Multi-core-shell-structured LiFePO4@Na3V2(PO4)3@C composite for enhanced low-temperature performance of lithium-ion batteries[J].Rare Metals,2021,40(4):828.

[5]Gu X X,Kuang L Y,Lin J,Qiao S,Ma S,Li Y,Wang Q,Dai J H,Zhou X and Zhou H Y. Highly porous nitrogen-doped biochar nanosheets for high-performance Li-Se batteries [J].Rare Metals,2023,42(3):822.

[6]甘億,王聪,李敬迎,郑俊杰,万厚钊,王浩. 水系锌离子电池的稳定性优化策略[J].稀有金属,2022,46(6):753.

Y Gan,C Wang,J Y Li,J J Zheng,H Z Wan,H Wang. Stability optimization strategy of aqueous zinc ion batteries[J].Chinese Journal of Rare Metals,2022,46(6):753.

[7]欧镇滔,罗刚,冯小勇,郭子依,李建伟,秦伟. 碳包覆硒化锌用作高性能锂离子电池负极材料[J].铜业工程,2024,(1):81.

Z T Ou,G Luo,X Y Feng,Z Y Guo,J W Li,W Qin. Carbon-coated ZnSe nanoparticles for high-performance lithium-ions battery anode[J].Copper Engineering,2024,(1):81.

[8]Han L S,Guo Y M,Ning F H,Liu X Y,Jin Y,Luo Q,Qu B H,Yue J L,Lu Y F,Li Q. Lotus effect inspired hydrophobic strategy for stable Zn metal anodes[J].Advanced Materials,2024,36(11):2308086.

[9]Duan F X,Yin X X,Ba J J,Li J P,Yu Y,Wang C Y,Wei Y J,Wang Y Z. A hydrophobic and zincophilic interfacial nanofilm as a protective layer for stable Zn anodes[J].Advanced Functional Materials,2024,34(10):2310342.

[10]匡玲瑶,乔双,王倩,王星敏,代金航,古兴兴. 原位构筑聚糠醇SEI膜用于稳定锌负极的机制研究[J].稀有金属,2024,48(7):965.

L Y Kuang,S Qiao,Q Wang,X M Wang,J H Dai,X X Gu. In-situ construction of polyfurfuryl alcohol SEI film for stabilizing zinc anode[J].Chinese Journal of Rare Metals,2024,48(7):965

[11]Guigo N,Mija A,Vincent L,Sbirrazzuoli N. Chemorheological analysis and model-free kinetics of acid catalysed furfuryl alcohol polymerization[J].Physical Chemistry Chemical Physics,2007,9(39):5359.

[12]Wu S X,Yang Y J,Liu C B,Liu T F,Zhang Y P,Zhang B K,Luo D,Pan F,Zhang L. In-situ polymerized binder:a three-in-one design strategy for all-integrated SiOx anode with high mass loading in lithium ion batteries[J].ACS Energy Letters,2020,6(1):290.

[13]Răcuciu M,Barbu-Tudoran L,Oancea S,Drăghici O,Morosanu C,Grigoras M,Brînză F,Creangă D E. Aspartic acid stabilized iron oxide nanoparticles for biomedical applications[J].Nanomaterials,2022,12(7):1151.

[14]Krishnamurthy R,Rajasekaran R,Samuel B S. Growth and characterization of KDP crystals doped with l-aspartic acid[J].Spectrochimica Acta Part A:Molecular and Biomolecular Spectroscopy,2013,104:310.

[15]Liu X,Han Q G,Ma Q X,Wang Y H,Liu C G. Cellulose-acetate coating by integrating ester group with zinc salt for dendrite-free Zn metal anodes[J].Small,2022,18(39):2203327.

[16]Gu X X,Du Y X,Ren X L,Ma F C,Zhang X F,Li M,Wang Q H,Zhang L,Lai C,Zhang S Q. Shielding-anchoring double protection tactics of imidazo [1,2-b] pyridazine additive for ultrastable zinc anode[J].Advanced Functional Materials,2024,34:2316541.

[17]Guan K L,Li T,Yang R,Zhang H N,Wang N Z,Wan H Z,Cui J,Zhang J,Wang H B,Wang H. Anti-corrosion for reversible zinc anode via a hydrophobic interface in aqueous zinc batteries[J].Advanced Energy Materials,2022,12(9):2103557.

[18]Shi Z H,Yang M,Ren Y F,Wang Y Z,Guo J H,Yin J,Lai F L,Zhang W L,Chen S L,Alshareef H N. Highly reversible Zn anodes achieved by enhancing ion-transport kinetics and modulating Zn (002)deposition[J].ACS Nano,2023,17(21):21893.

[19]Zhou X,Chen R P,Cui E H,Liu Q,Zhang H,Deng J H,Zhang N N,Xie C,Xu L,Mai L Q. A novel hydrophobic-zincophilic bifunctional layer for stable Zn metal anodes[J].Energy Storage Materials,2023,55:538.

[20]Huang C,Zhao X,Hao Y S,Yang Y J,Qian Y,Chang G,Zhang Y,Tang Q L,Hu A P,Chen X H. Self‐healing SeO2 additives enable zinc metal reversibility in aqueous ZnSO4 electrolytes[J].Advanced Functional Materials,2022,32(18):2112091.

[21]Feng T,Feng K J,Liu Y,Ren J Z,Xiong Y,Li C B,Ren F Z. Suppressing interfacial side reactions of zinc metal anode via isolation effect toward high-performance aqueous zinc-ion batteries[J].Nano Research,2023,16(5):6789.

[22]Zhao Z M,Zhao J W,Hu Z L,Li J D,Li J J,Zhang Y J,Wang C,Cui G L. Long-life and deeply rechargeable aqueous Zn anodes enabled by a multifunctional brightener-inspired interphase[J].Energy & Environmental Science,2019,12(6):1938.

[23]Quan Z,Zhuang Y L,Liu C F,Kang Q L,Wu Y Z,Zhang J J,Wang J Y,Tao D W,Zhang Q L,Cao G Z. Dual effects of metal and organic ions co-intercalation boosting the kinetics and stability of hydrated vanadate cathodes for aqueous zinc-ion batteries[J].Advanced Energy Materials,2023,13(31):2301480.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY24110020

Chinese Library Classification Number:TQ151.1

Citation Information:

The overuse of fossil fuels has caused serious harm to the environment and undermined the overall sustainable development of mankind. Therefore,the development and application of renewable clean energy has become a hot research field,and the use of stable charge and discharge electrochemical energy storage devices to store and collect dispersed clean energy has also attracted great attention from academia and industry around the world. Lithium-ion batteries (LIBs)have significant theoretical capacity,excellent performance in secondary battery systems,and have been effectively applied in mobile phones,notebook computers,and other products,maintaining a dominant position in the commercial field. However,LIBs carry specific safety risks,including the use of flammable and explosive organic electrolytes. In addition,with increasing challenges such as depletion of lithium reserves and soaring costs,it is imperative to develop and successfully commercialize a very safe,economically viable,and environmentally sustainable battery storage system. Among the many options,aqueous-based zinc-ion batteries (AZIBs)with high safety and stable charge-discharge performance are widely considered to be one of the most promising. AZIBs have the following advantages:1)the natural abundance of zinc metal is high,2)the electrolyte used in the battery is water,which is environmentally friendly and safe compared to the flammable organic electrolyte of lithium-ion batteries,3)the theoretical specific capacity is high (820 mAh·g−1),and 4)the redox potential is low (compared to the standard hydrogen electrode:–0.762 V). However,the zinc anode of aqueous zinc-ion batteries encounters significant challenges,including hydrogen evolution,corrosion passivation,and pronounced zinc dendrite growth,resulting in diminished battery capacity,inferior cycling stability,and reduced coulombic efficiency,thereby constraining the advancement and utilization of aqueous zinc-ion batteries. Among many strategies,the artificial solid electrolyte interphase (SEI)membrane is considered to be one of the simple and efficient strategies,as it can completely inhibit the interaction between the zinc anode and the electrolyte,while regulating the diffusion kinetics of Zn2+ cations. In this study,furfuryl alcohol/aspartic acid (FA/ASP)artificial SEI film was constructed on the surface of zinc anode by esterification using the cheap and easily obtained furfuryl alcohol biomass and aspartic acid as raw materials. FA/ASP artificial SEI film had many polar groups containing oxygen and nitrogen,which enhanced the zincophile of the zinc anode,promoted the uniform deposition of Zn2+,and hindered the growth of zinc dendrites. FA/ASP artificial SEI film also hindered the direct contact between aqueous electrolyte and zinc anode,reduced the reactivity of hydrogen evolution reaction,inhibited the occurrence of hydrogen evolution reaction,and improved the corrosion resistance of zinc anode. Therefore,Zn||Zn-symmetric battery assembled based on FA/ASP@Zn could work stably for 950 h at 1 mA·cm−2 and 1 mAh·cm−2,with an average Coulomb efficiency (CE)of about 98%. And FA/ASP@Zn||Cu asymmetric cell could stably cycle for 270 h,which was almost three times more than the bare Zn||Cu asymmetric cell. Meanwhile,FA/ASP@Zn||V2O5 full battery also showed an enhanced reversible capacity of 157 mAh·g−1 at 1 A·g−1 and CE could reach up to 100%. The significant improvement in cycle stability and coulomb efficiency illustrated the great potential of artificial solid electrolyte interface films based on this biomass for stabilizing zinc-ion battery anodes.

quote

GB/T 7714-2015 [1] Hanyu Xu, Long Huang, Lingyao Kuang, et al. A Novel Artificial Biomass Polymer SEI Film for Highly Stable Zn Anode[J]. Chinese Journal of Rare Metals, 2025, 49(5): 695-703. DOI:10.13373/j.cnki.cjrm.XY24110020.
MLA [1] Hanyu Xu, et al., "A Novel Artificial Biomass Polymer SEI Film for Highly Stable Zn Anode." Chinese Journal of Rare Metals, vol. 49, no. 5, 2025, pp. 695-703, https://doi.org/10.13373/j.cnki.cjrm.XY24110020.
APA [1] Hanyu Xu, Long Huang, Lingyao Kuang, & Xingxing Gu. (2025). A Novel Artificial Biomass Polymer SEI Film for Highly Stable Zn Anode. Chinese Journal of Rare Metals, 49(5), 695-703. https://doi.org/10.13373/j.cnki.cjrm.XY24110020
IEEE [1] Hanyu Xu, Long Huang, Lingyao Kuang, and Xingxing Gu, "A Novel Artificial Biomass Polymer SEI Film for Highly Stable Zn Anode," Chinese Journal of Rare Metals, vol. 49, no. 5, pp. 695-703, 2025, doi: 10.13373/j.cnki.cjrm.XY24110020. keywords: {aqueous zinc ion batteries (AZIBs);Zn anode;solid electrolyte interphase (SEI)film;zinc dendrite;corrosion}