Study of Forge Deformation and Microstructure on Steel-Bonded Cemented Carbides AITranslate
Abstract AITranslate
In this paper, the effects of forge deformation on the microstructres and properties of steel-bonded cemented carbides have been studied. The results show that the use of die forging is suitable for processing the steel-bonded cemented carbides. The use of die forging can not only refine the structure, but also make up for the defects in the process of free forge. It improves forge efficiency and proportion of finished products.
KeyWords AITranslate
1张志恒,张军.高强韧钢结硬质合金及其碳化物球化[J].粉末冶金工业,2008,18(5):30-35. 被引量:5
1周书助,兰登飞,鄢玲利,尹绍峰.钢结硬质合金的研究进展[J].粉末冶金材料科学与工程,2015,20(5):661-669. 被引量:3
2肖逸锋,周年丰,吴靓,许艳飞,钱锦文,李浪浪,贺跃辉.Cr含量对WC钢结硬质合金组织及力学性能的影响[J].金属热处理,2017,42(4):22-26. 被引量:4
3王蕾,刘辛,谢焕文,邹黎明,蔡一湘.不同方法制备的球形铸造碳化钨粉末的性能研究[J].粉末冶金工业,2017,27(4):7-11. 被引量:2
4李金普,施瑜蕾,柳学全,姜丽娟,李彪.低压烧结温度对WC-6Ni无磁硬质合金性能的影响[J].粉末冶金工业,2021,31(1):46-50. 被引量:4
5范兴平,王本菊,马兰,范维,李俊翰.烧结温度对30TiC-0.5%C-Fe钢结硬质合金性能的影响[J].粉末冶金工业,2021,31(2):63-67. 被引量:1
1王安家,李金山,周中波,李建峰,胡锐,王建国.A357合金低压铸造过程及性能研究[J].热加工工艺,2007,36(13):59-60. 被引量:11
2王克杰,薛瑞,董天真,刘海英,骆春民.控冷工艺对82B盘条相变行为影响的研究[J].天津冶金,2010(4):13-15. 被引量:3
3杨博.退火对TW40钢结硬质合金组织及锻造性能的影响[J].稀有金属,2001,25(1):36-38. 被引量:1
4林一坚,罗光敏,史海生,章靖国.一种具有优化组织和优异性能的超高碳钢[J].钢铁,2005,40(11):57-61. 被引量:11
5戴品强,何则荣.优化组织球铁的力学性能及其微观断裂行为[J].机械强度,2004,26(z1):150-153. 被引量:3
6汪凌云,黄光杰,陈林,黄光胜,李伟,潘复生.镁合金板材轧制工艺及组织性能分析[J].稀有金属材料与工程,2007,36(5):910-914. 被引量:41
7何则荣,纪松,林国雄,周虹.灰口铸铁组织的优化与性能[J].福州大学学报:自然科学版,1998,26(4):57-61.
8戴品强,何则荣.球墨铸铁强韧化的组织设计及其热处理工艺[J].热处理,2007,22(4):32-36. 被引量:4
9陈鼎欣,李晓谦,黎正华,蒋日鹏.超声铸造7050铝合金的微观组织和宏观偏析规律[J].北京科技大学学报,2012,34(6):666-670. 被引量:7
10王正军,司乃潮.Al-Ti-B-RE中间合金第二相的形态及分布对工业纯铝细化效果的影响[J].稀有金属材料与工程,2015,44(6):1494-1498. 被引量:17
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
In this paper, the effects of forge deformation on the microstructres and properties of steel-bonded cemented carbides have been studied. The results show that the use of die forging is suitable for processing the steel-bonded cemented carbides. The use of die forging can not only refine the structure, but also make up for the defects in the process of free forge. It improves forge efficiency and proportion of finished products.
quote
| GB/T 7714-2015 | [1] WANG Che, YANG Bo, ZHOU Mei-ling. Study of Forge Deformation and Microstructure on Steel-Bonded Cemented Carbides[J]. Rare Metals and Cemented Carbides, 1998(1): 13-17. |
| MLA | [1] WANG Che, et al., "Study of Forge Deformation and Microstructure on Steel-Bonded Cemented Carbides." Rare Metals and Cemented Carbides, no. 1, 1998, pp. 13-17. |
| APA | [1] WANG Che, YANG Bo, & ZHOU Mei-ling. (1998). Study of Forge Deformation and Microstructure on Steel-Bonded Cemented Carbides. Rare Metals and Cemented Carbides(1), 13-17. |
| IEEE | [1] WANG Che, YANG Bo, and ZHOU Mei-ling, "Study of Forge Deformation and Microstructure on Steel-Bonded Cemented Carbides," Rare Metals and Cemented Carbides, no. 1, pp. 13-17, 1998. keywords: {Steel-bonded cemented carbide;forging;microstructure;deformation} |