Study on Compounding Process for a Steel-based As-cast Ceramal AITranslate

Hunan Provincial Institute of Metallurgical Materials;Hunan Provincial Institute of Metallurgical Materials;Hunan Provincial Institute of Metallurgical Materials;Hunan Provincial Institute of Metallurgical Materials;Hunan Provincial Institute of Metallurgical Materials;Hunan Provincial Institute of Metallurgical Materials;Hunan Provincial Institute of Metallurgical Materials
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper describes a study on the commercial possibility of compounding a steel-based as-cast ceramal. Factors of the compounding process has been analysed. This paper indicates that a key for producing the steel-based as-cast ceramal is to assure better liquidity of a melted steel entering prefabricated layer of the ceramal.The use of additives for this can give better result.Keyworks:steel-based; as-cast ceramal compounding process

KeyWords AITranslate

steel-based as-cast ceramal compounding process

1石功奇,丁培道,周守则.金属与陶瓷的浸渗复合[J].四川冶金,1991,13(2):68-72. 被引量:1

1张玉柱,郎建峰,李振国.含硼添加剂改善烧结矿质量机理及硼-镁复合添加剂的研究[J].矿产综合利用,2000(1):29-32. 被引量:6

2刘紫卉.将炉渣应用于国民经济中──生产低碳铬铁复合工艺的研究[J].铁合金,1994,25(5):53-55. 被引量:1

3王平,马廷温,李传薪,陈振南,易继松,王昌生.50吨EAF—60吨VAD生产的高清洁度轴承钢[J].钢铁,1992,27(5):17-19. 被引量:5

4P. Lemieux,Y. Thomas,P. E. Mongeon,S. Pelletier,S. St-Laurent,郭瑞金,韩凤麟(译).用静电模壁润滑—温压复合工艺增高粉末冶金零件生坯与烧结件性能[J].粉末冶金技术,2006,24(4):310-312. 被引量:1

5吕心刚.炼钢转炉尘泥球团应用研究[J].冶金设备,2011(2):67-70.

6吕心刚.炼钢转炉尘泥球团应用研究[J].河南冶金,2007,15(2):22-24. 被引量:1

7孙德勤,谢建新,吴春京.复合板的成形技术与发展趋势[J].金属成形工艺,2003,21(2):19-22. 被引量:30

8李英,李春玉,柴世昌,韩雅芳,夏洋,张跃,袁润章.Al/TiB_2复合工艺的铝含量研究[J].航空材料学报,1994,14(4):32-35.

9Lech Bulkowski,武成文.使用粉状脱硫剂在钢包内进行钢水脱硫[J].大型铸锻件,1985(1):86-91.

10张哲君.电炉技术的新发展[J].冶金丛刊,1996(4):8-14.

Basic Information:

DOI:

Chinese Library Classification Number:TG148[金属学及工艺—金属材料];TF125.31[冶金工程—粉末冶金]

Citation Information:

This paper describes a study on the commercial possibility of compounding a steel-based as-cast ceramal. Factors of the compounding process has been analysed. This paper indicates that a key for producing the steel-based as-cast ceramal is to assure better liquidity of a melted steel entering prefabricated layer of the ceramal.The use of additives for this can give better result.Keyworks:steel-based; as-cast ceramal compounding process

quote

GB/T 7714-2015 [1] HE Xu-chu, CHEN Guo-wei, DING Yun-yuan, et al. Study on Compounding Process for a Steel-based As-cast Ceramal[J]. Rare Metals and Cemented Carbides, 1998(1): 17-21.
MLA [1] HE Xu-chu, et al., "Study on Compounding Process for a Steel-based As-cast Ceramal." Rare Metals and Cemented Carbides, no. 1, 1998, pp. 17-21.
APA [1] HE Xu-chu, CHEN Guo-wei, DING Yun-yuan, TIAN Shu-sheng, TANG Yun-xing, WU Jin-feng, & CAO Xiang-rong. (1998). Study on Compounding Process for a Steel-based As-cast Ceramal. Rare Metals and Cemented Carbides(1), 17-21.
IEEE [1] HE Xu-chu, CHEN Guo-wei, DING Yun-yuan, TIAN Shu-sheng, TANG Yun-xing, WU Jin-feng, and CAO Xiang-rong, "Study on Compounding Process for a Steel-based As-cast Ceramal," Rare Metals and Cemented Carbides, no. 1, pp. 17-21, 1998. keywords: {steel-based,as-cast ceramal compounding process}