Preparation of RE Polishes From RE Chloride AITranslate
Abstract AITranslate
Study is made of the effects of roasting temperature, roasting time, fluoration and different intermediates on the properties of RE polishes from RE chloride. The properties of obtained RE polishes are indicated by particle analyzer, SEM,XRD. The results show that the following process is more for RE polishes (NH4)2SO4 precipitation followed by NaOH conversion,fluorating and 3 h roasting of the intermediate at 900 ℃
KeyWords AITranslate
1林河成.优良的研磨剂──稀土抛光粉[J].世界有色金属,1995,20(9):36-37. 被引量:4
1李学舜,谢兵,杨国胜,吴文远,涂赣峰.稀土抛光粉颜色的测定及影响因素[J].稀土,2007,28(1):34-37. 被引量:1
2谢兵,任慧平,李学舜.稀土抛光粉颜色的表征及影响因素研究[J].包钢科技,2007,33(3):14-16. 被引量:2
3黄绍东,李学舜.稀土抛光粉的应用及发展简介[J].稀土,2008,29(1):59-62. 被引量:15
4李永绣,周新木,辜子英,彭德院,胡平贵,周雪珍,焦晓燕,何小彬,魏坤,刘桂华.稀土抛光材料的生产、应用及其新进展[J].稀土,2002,23(5):71-74. 被引量:28
1弥宁,杨来东.氟化方式对含氟铈基稀土抛光粉性能的影响[J].稀有金属与硬质合金,2015,43(2):29-32. 被引量:1
2李永绣,陈伟凡,周雪珍,程昌明,辜子英,胡建东.氯化钠在球形纳米氧化铈形成过程中的作用[J].中国稀土学报,2004,22(5):636-640. 被引量:15
3周雪珍,李进,丁家文,辜子英,胡平贵,彭德院,李永绣.混合碳酸稀土两步煅烧法制备超细CeO_2[J].稀有金属,2004,28(5):820-824. 被引量:1
4郭瑞华,李梅.稀土抛光粉的发展现状及应用[J].稀土,2005,26(1):82-85. 被引量:12
5吴新根,陈琨,李常清,李才生.光学玻璃抛光材料前驱体的制备研究[J].江西冶金,2005,25(4):7-9.
6雷红,张鹏珍,卢海参.纳米氧化硅在玻璃基片表面亚纳米级抛光中的应用[J].润滑与密封,2006,31(1):31-34. 被引量:4
7周雪珍,程昌明,胡建东,辜子英,胡平贵,李永绣.以碳酸铈为前驱体制备超细氧化铈及其抛光性能[J].稀土,2006,27(1):1-3. 被引量:16
8周新木,李炳伟,李永绣,徐小丽.高铈抛光粉表面电性及悬浮液分散稳定性研究[J].稀土,2007,28(1):12-16. 被引量:10
9柴明霞,胡建东,冯晓平,周雪珍,罗军明,李永绣.SiO_2-CeO_2复合氧化物的制备及抛光性能[J].无机化学学报,2007,23(4):623-629. 被引量:15
10黄绍东,李学舜.稀土抛光粉的应用及发展简介[J].稀土,2008,29(1):59-62. 被引量:15
1陈玉勇,贾均,马顺龙,李庆春,杨剑秋.氯化稀土对ZL102合金变质作用及性能影响的研究[J].稀有金属,1989,13(6):472-479. 被引量:11
2宋晓虹.氯化稀土中氯化铵的快速分析[J].机械工程师,1991(4):17-17.
3陶小克,彭日升,孙永昌,刘杰.氯化稀土对热浸镀助镀剂性能的影响[J].金属热处理,2000,25(10):10-12. 被引量:3
4稀土在镁及镁合金中应用[J].中国稀土学报,1995,0(S1):524-524.
5陈玉勇,贾均,武鼎亨,王嘉奎,王秀元,马顺龙.氯化稀土变质剂在ZL107A合金中的实际应用[J].特种铸造及有色合金,1990(6):18-20. 被引量:1
6加快镧镨铈新型混合稀土金属(LPC)的应用[J].稀土信息,2005,11(11):23-23.
7潘雄.高性能稀土抛光粉及永磁材料项目将于7月开工建设[J].功能材料信息,2007,4(3):42-42.
8余丽萍,曾凡昌.蒸馏—容量法测定氯化稀土中的NH4^+[J].江西冶金,1995,15(2):41-41.
9谷志刚,席忠来.钢在A_1相变点之下的稀土硼氮共渗[J].热加工工艺,1999(2):26-28. 被引量:5
10徐招弟,周新木,李永绣,谭宏宇.水热法制备超细粉体及在抛光粉上应用前景[J].吉首大学学报:自然科学版,2004,25(2):21-24. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TB44[一般工业技术];TG175[金属学及工艺—金属表面处理]
Citation Information:
Study is made of the effects of roasting temperature, roasting time, fluoration and different intermediates on the properties of RE polishes from RE chloride. The properties of obtained RE polishes are indicated by particle analyzer, SEM,XRD. The results show that the following process is more for RE polishes (NH4)2SO4 precipitation followed by NaOH conversion,fluorating and 3 h roasting of the intermediate at 900 ℃
quote
| GB/T 7714-2015 | [1] CHENG Yao-geng, CHEN Jian-she, WEI Xu-jun. Preparation of RE Polishes From RE Chloride[J]. Rare Metals and Cemented Carbides, 1998(1): 9-13. |
| MLA | [1] CHENG Yao-geng, et al., "Preparation of RE Polishes From RE Chloride." Rare Metals and Cemented Carbides, no. 1, 1998, pp. 9-13. |
| APA | [1] CHENG Yao-geng, CHEN Jian-she, & WEI Xu-jun. (1998). Preparation of RE Polishes From RE Chloride. Rare Metals and Cemented Carbides(1), 9-13. |
| IEEE | [1] CHENG Yao-geng, CHEN Jian-she, and WEI Xu-jun, "Preparation of RE Polishes From RE Chloride," Rare Metals and Cemented Carbides, no. 1, pp. 9-13, 1998. keywords: {RE;CeO_2;polishes;preparation} |