Investigation on Low-concentration and Low-addition HCl Digestion of Scheelite Concentrate AITranslate
Abstract AITranslate
Investigation is made on the low-concentration, low-addition HCl digestion of scheelite concentrate. The results show that the average digestion rate can reach 97. 35% in 1. 5 hour at 95~10℃ with the addition of HCl (10% concentration ) .1. 5 times more than the theoretical value. Compared with the traditional acid digestion process, the said process can bring about large reduction of HCl consumption and concentration, resulting in large reduction of waste acid treatment cost and elimination of HCl gas volatization during acid digestion. In this way, the working conditions are improved and the cost for the control of HCl gas pollutant for environmental protection is also reduced. However, the said technology doesn't remove Mo and needs larger acid liquid volume (1. 5 times as much as that of the traditional technology).
KeyWords AITranslate
1成都科学技术大学,彭少方.钨冶金学[M]冶金工业出版社,1981.
1何贵香,何利华,曹才放,赵中伟,陈星宇,陈爱良,刘旭恒,贺跃辉.氢氧化钠分解白钨矿的热力学分析[J].粉末冶金材料科学与工程,2013,18(3):368-372. 被引量:9
2刘庆生,涂弢,郭浩,程华金,王学重.硫酸−草酸络合浸出白钨矿及含钨相的转化行为[J].中国有色金属学报:英文版,2021,31(10):3150-3161. 被引量:2
1刘飞飞,祝恩宇,徐鹏,龚亚忠,罗贤平,张宇舟.碱煮工艺过程的智能集成建模研究[J].有色金属:冶炼部分,2015(6):63-66. 被引量:2
2罗小燕,于孟,陈斌,蒙鹏宇.基于模糊自适应PID控制的反应釜系统的设计与仿真[J].有色金属科学与工程,2015,6(5):129-134. 被引量:6
3刘玉城,林如丹,梁勇,温葆林,刘元鑫,郭斗斗.氢氧化钠分解氟化钙的热力学分析[J].湿法冶金,2016,35(2):97-100. 被引量:3
4何鲁华,沈裕军,彭俊,刘强,周小舟.从低品位锡钨混合粗精矿中提取钨[J].矿冶工程,2016,36(3):87-90.
5李停停,钟祥熙,张威,张津,沈岩柏,魏德洲.白钨矿浸出工艺现状及发展趋势[J].金属矿山,2017,46(10):128-134. 被引量:8
6张建,琚成新,陈利革,王跃飞,聂小威,赵四方.白钨矿碳酸钠浸出工艺优化[J].中国钨业,2021,36(4):60-64. 被引量:2
7何秉轩,徐略渭,雷鑫,胡皓东,梁勇,刘德刚.磷酸钠低耗分解白钨矿的研究[J].稀有金属与硬质合金,2022,50(2):1-7.
8曾斌,曾祥荣,黄万抚.Na_(2)CO_(3)⁃CaO协同浸出钨冶炼除磷渣中钼和钨[J].矿冶工程,2022,42(5):106-110.
9彭伟,黄健,王振杰,刘安荣.钨冶炼渣中有价金属回收利用研究现状[J].化工进展,2022,41(12):6656-6663.
10吕世杰,李江涛,刘旭恒,陈星宇,何利华,孙丰龙,赵中伟.(Ca(OH)_(2)-)NaOH-Na_(2)WO_(4)-H2O和(Ca(OH)_(2)-)NaOH-Na_(3)PO_(4)-H_(2)O体系的热力学与应用[J].中南大学学报:英文版,2023,30(4):1132-1144.
1许菱,许孙曲,邱银兰.白钨精矿的酸浸及杂多钨酸盐的生产[J].中国钨业,2000,15(4):41-42.
2罗明润,程立,张凤美,曹子卿.用杂醇油代替正、异戊醇作萃取剂萃取磷酸的试验(一)[J].安徽师大学报,1989,12(4):56-61.
3天津石化100万吨/年乙烯及配套项目将投运[J].军民两用技术与产品,2010(1):29-29.
4喻新平,陈献桃.副产盐酸分解白云石制轻质氧化镁和氯化钙研究[J].河南化工,2001,20(5):14-15. 被引量:4
5宋谊君.爆炸危险性气体环境的区域划分及电气设计[J].山西化工,2013,33(6):30-32.
6贾方茹.窑尾漏料原因及处理[J].中国水泥,2011(12):74-75.
7肖惠玉.用碳酸钠熔融-盐酸分解-原子吸收光谱法测水泥中氧化镁[J].广东建材,2002,25(9).
8张娟.盐酸分解蛇纹石制取氧化镁工艺及设备[J].化学工程与装备,2012(3):34-35. 被引量:1
9郑冠山.石灰石CaO、MgO的连续测定[J].四川水泥,2003(2):43-44.
10热西旦.阿不力米提.火焰光度法测定熔料中的氧化锂[J].新疆有色金属,2012,35(6):56-56.
Basic Information:
DOI:
Chinese Library Classification Number:TQ136.13[化学工程—无机化工]
Citation Information:
Investigation is made on the low-concentration, low-addition HCl digestion of scheelite concentrate. The results show that the average digestion rate can reach 97. 35% in 1. 5 hour at 95~10℃ with the addition of HCl (10% concentration ) .1. 5 times more than the theoretical value. Compared with the traditional acid digestion process, the said process can bring about large reduction of HCl consumption and concentration, resulting in large reduction of waste acid treatment cost and elimination of HCl gas volatization during acid digestion. In this way, the working conditions are improved and the cost for the control of HCl gas pollutant for environmental protection is also reduced. However, the said technology doesn't remove Mo and needs larger acid liquid volume (1. 5 times as much as that of the traditional technology).
quote
| GB/T 7714-2015 | [1] LI Wei-qin. Investigation on Low-concentration and Low-addition HCl Digestion of Scheelite Concentrate[J]. Rare Metals and Cemented Carbides, 1998(1): 5-8. |
| MLA | [1] LI Wei-qin. "Investigation on Low-concentration and Low-addition HCl Digestion of Scheelite Concentrate." Rare Metals and Cemented Carbides, no. 1, 1998, pp. 5-8. |
| APA | [1] LI Wei-qin. (1998). Investigation on Low-concentration and Low-addition HCl Digestion of Scheelite Concentrate. Rare Metals and Cemented Carbides(1), 5-8. |
| IEEE | [1] LI Wei-qin, "Investigation on Low-concentration and Low-addition HCl Digestion of Scheelite Concentrate," Rare Metals and Cemented Carbides, no. 1, pp. 5-8, 1998. keywords: {low-concentration HCl;scheelite;digestion} |