Study on Separation of Al-V-Mo from Alkali System AITranslate
Abstract AITranslate
Study is made on V and Mo precipitation efficiency from the V-H2O/Mo-H2O system, Al-V- H2O)/Al-Mo-H2O system and Al-V-Mo-H2O system with CaO,CaCl2 ,MgSO47H2O,Fe2O3 ,CDJ as the precipitators. The results show that in V-H2O/Mo-H2O system,V and Mo precipitation efficiency with CaO and CaCl2 are better than that in Al-V-H2O/Al-Mo-H2O system. Thermodynamics calculation indicates that reason is that Ca^2+ reacts with Al in solution to form various calcium aluminate. The CDJ is very effective for V and Mo fractional precipitation from alkali solution in Al-V-Mo-H2O system under controlled test conditions and with controlled dosage of CDJ.
KeyWords AITranslate
1管永诗,张云.我国铝土矿资源及氧化铝工业的现状[J].矿产保护与利用,1998(6):42-44. 被引量:10
2国土资源部矿产开发管理司.中国矿产资源主要矿种开发利用水平与政策建议[R],2002.
3施友富,王海北.废催化剂中钼和钒的分离[J].中国钼业,2004,28(2):39-41. 被引量:22
4陈云,冯其明,张国范,欧乐明,卢毅屏.废铝基催化剂综合回收现状与发展前景[J].金属矿山,2005(7):55-58. 被引量:9
5赵骧.废催化剂回收技术与现状[J].中氮肥,1989(1):1-16. 被引量:7
6Keiji Toyage, Kenji Kirishima, Haruo Shibayama,et al. Process for recovering valuable metal from waste catalyst[P]. US Pat:5431892,1995-07-11.
7户田正作.资源の素材.资源素材学会志,1989,(3):265-269.
8Sebenik, Roger F, Lavalle, Pablo P, et al. Recovery of metal values from spent hydrodesulfurization catalysts. US Pat :4495157,1985-01-22.
9蔡昭铃 王玉春 栾美琅.从钠化钒渣浸取液中分离钒的研究.钢铁钒钛,1987,(1):33-37.
10李国良.钒的沉淀工艺及其发展.国外钒钛,1982,(2):51-60.
1陈肖虎,陈颖,甘蔓,徐开鑫.沉淀法从拜耳法铝酸钠溶液中分离钒[J].过程工程学报,2010,10(S1):142-145. 被引量:6
2张文朴.加强钼资源综合利用与再生研发 促进我国生态钼业建设[J].中国钼业,2010,34(2):13-18. 被引量:3
3丁瑞锋,刘桂华.溶液中钒分离富集技术的研究进展[J].湖南有色金属,2011,27(3):15-19. 被引量:8
4赵东峰,田侣,丁瑞锋,刘桂华,周秋生,李小斌,彭志宏.铬酸钠碱性液中加石灰除钒[J].中国有色金属学报,2011,21(12):3162-3168. 被引量:11
5李贺,刘旭恒,何利华.钙盐沉钒的热力学研究[J].稀有金属与硬质合金,2014,42(1):15-19. 被引量:3
6谭佳文,王嘉华,宋盈盈,刘志壮,刘美,凌江华,安会勇.化学沉淀法分离回收碱性溶液中V、Mo、Al的研究[J].石油化工高等学校学报,2020,33(6):13-18. 被引量:1
1王克勤,李生虎.氧化铝赤泥盐酸浸出回收钒的试验研究[J].稀有金属与硬质合金,2012,40(6):5-8. 被引量:11
2李贺,刘旭恒,何利华.钙盐沉钒的热力学研究[J].稀有金属与硬质合金,2014,42(1):15-19. 被引量:3
3侯明,路畅,王立华.聚乙烯醇-海藻酸钠-钙-铁凝胶球对钒(Ⅴ)的吸附特性研究和应用[J].分析科学学报,2014,30(3):337-341.
4吕振福,冯安生.几种矿产资源综合利用率计算方法的探讨[J].矿产保护与利用,2014,34(2):6-8. 被引量:12
5朱茂兰,黄中省,衷水平,陈杭,胡志彪.镓精矿中镓的提取工艺[J].中国有色金属学报,2018,28(11):2351-2357. 被引量:2
6竹斌耀,吴刘曦,周骏,柳建设.含钼废催化剂中钼的回收技术现状[J].广州化工,2014,42(13):39-41. 被引量:2
7蒋霖.钒铬溶液中钒铬提取及分离工艺研究进展[J].钢铁钒钛,2014,35(6):52-59. 被引量:10
8赵斌,张玉龙,张少峰,王德武,邱亚娟.连续式密实移动床逆流操作下轴向解吸K^+特性[J].过程工程学报,2015,15(1):100-105. 被引量:1
9郑川立,张红玲,张炳烛,李平,徐红彬,张懿.工业含钒废水处理工艺的研究进展[J].化工环保,2015,35(3):247-252. 被引量:11
10徐乐,王建平,余德彪,陈洪,孙长波,刘彬,张方方.我国钼资源产业现状及可持续开发建议[J].资源与产业,2015,17(3):32-38. 被引量:16
1王敏.利用盐泥制取七水硫酸镁[J].苏盐科技,2003(2):1-1. 被引量:8
2杨春霞,张京.泡沫铝用可溶性石膏材料的制备[J].无机盐工业,2011,43(10):60-61.
3硼化物文摘[J].无机盐技术,2007(6):42-42.
4鲁利梅,赵斌,郭宏飞,曹吉林.硫酸镁与氨水水热反应合成碱式硫酸镁晶须[J].人工晶体学报,2015,44(8):2171-2177. 被引量:4
5马俊林,杨红琳,胡菊,刘平,邓斌.纳米氧化镍的制备及工艺条件选优[J].十堰职业技术学院学报,2004,17(2):68-70.
6曾翎.制备条件对Bi-Mo复合氧化物的物性影响的考察[J].平顶山学院学报,1998,15(2):37-40.
7吴华,缪根,陈剑.二氧化硅水溶液的沉淀效果[J].现代传输,2014(2):52-53.
8张玉明,张福元,熊领领.浸铅液有价元素综合回收实验研究[J].无机盐工业,2014,46(10):62-64.
9李国栋,毕万利,孙恩禹,李晶,李宇,杨学奇.改性硫氧镁水泥的配制及性能研究[J].耐火材料,2016,50(6):469-472. 被引量:6
10梁希,李建明,陈志,卢铭,贾江宁,刘东杰,曹蕾.γ-Al_2O_3多孔膜的分离性能[J].膜科学与技术,2008,28(3):45-49. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TQ028.3[化学工程]
Citation Information:
Study is made on V and Mo precipitation efficiency from the V-H2O/Mo-H2O system, Al-V- H2O)/Al-Mo-H2O system and Al-V-Mo-H2O system with CaO,CaCl2 ,MgSO47H2O,Fe2O3 ,CDJ as the precipitators. The results show that in V-H2O/Mo-H2O system,V and Mo precipitation efficiency with CaO and CaCl2 are better than that in Al-V-H2O/Al-Mo-H2O system. Thermodynamics calculation indicates that reason is that Ca^2+ reacts with Al in solution to form various calcium aluminate. The CDJ is very effective for V and Mo fractional precipitation from alkali solution in Al-V-Mo-H2O system under controlled test conditions and with controlled dosage of CDJ.
quote
| GB/T 7714-2015 | [1] SUN Jian-cheng, FENG Qi-ming, CHEN Yun. Study on Separation of Al-V-Mo from Alkali System[J]. Rare Metals and Cemented Carbides, 2008(3): 19-23. |
| MLA | [1] SUN Jian-cheng, et al., "Study on Separation of Al-V-Mo from Alkali System." Rare Metals and Cemented Carbides, no. 3, 2008, pp. 19-23. |
| APA | [1] SUN Jian-cheng, FENG Qi-ming, & CHEN Yun. (2008). Study on Separation of Al-V-Mo from Alkali System. Rare Metals and Cemented Carbides(3), 19-23. |
| IEEE | [1] SUN Jian-cheng, FENG Qi-ming, and CHEN Yun, "Study on Separation of Al-V-Mo from Alkali System," Rare Metals and Cemented Carbides, no. 3, pp. 19-23, 2008. keywords: {vanadium;molybdenum;precipitator;chemical precipitation method;alkali system} |