daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of Rolling Process on Microstructure and Property of Warm Rolled Molybdenum Sheet for Down-stream Operation AITranslate

Western Metal Materials Co., Ltd.;Western Metal Materials Co., Ltd.;Western Metal Materials Co., Ltd.;Western Metal Materials Co., Ltd.;Western Metal Materials Co., Ltd.;Western Metal Materials Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effect of rolling process on microstructure and property of molybdenum sheet was investiga- ted by changing rolling capacity, rolling temperature and rolling process. The results show that the longitudinal and transverse microstructures and properties of molybdenum sheet are similar by high-rate blooming and low temperature alternative rolling process. Meanwhile, the sheet can be adapted to the downstream operation.

KeyWords AITranslate

molybdenum sheet down stream operation rolling process microstructure and property low temperature cross rolling

1钟培全.钼与钼合金的应用及其加工方法[J].中国钼业,2000,24(5):15-16. 被引量:28

2稀有金属材料加工手册编辑组.稀有金属材料加工手册[M].北京:冶金工业出版社,1984:400-470.

1杨松涛,李继文,魏世忠,徐流杰,彭光辉.纯钼及钼合金板材轧制加工工艺探讨[J].材料研究与应用,2010,4(1):60-64. 被引量:11

2杨松涛,李继文,魏世忠,徐流杰,彭光辉.纯钼及钼合金板材轧制加工工艺概述[J].中国钼业,2010,34(2):42-45. 被引量:7

3郭让民,淡新国,侯军涛.钼镧合金板材高温抗载荷弯曲性能研究[J].中国钼业,2013,37(3):47-49. 被引量:7

4李继文,杨松涛,魏世忠,张国赏,徐流杰,U.轧制方式和变形量对纯钼板坯微观组织和织构的影响[J].稀有金属,2014,38(3):348-353. 被引量:12

5王小康,陈艳芳,尤强周,陶诗伟,王壮,曾钦利,刘冰,罗银博.钼粉形貌对纯钼板坯组织和性能的影响[J].南方金属,2018(1):17-20. 被引量:4

6张二召,张灵杰,岳慎伟,彭光辉,李改改,杨雷雷,袁蔚.蓝宝石长晶炉用钼板终轧和预备热处理工艺研究[J].有色金属加工,2019,48(4):24-28. 被引量:2

1刘雨婷,郑洲顺,张帆,叶志坚,段柏华,杨栋林.基于DEFORM-3D的钼板多道次轧制仿真研究[J].中国体视学与图像分析,2020(2):157-165.

2傅蔡安,郝健,彭广盼,季坤.基于Deform的钼板轧制用轧辊辊形的研究[J].锻压技术,2011,36(3):50-54. 被引量:8

3郝健,傅蔡安.波纹廓形轧辊轧制钼基片坯的研究[J].机械设计与制造,2011(12):138-140.

4沈宏,邓宇锋,郝健.钼板材热轧工艺及质量控制的研究[J].稀有金属与硬质合金,2012,40(5):41-44.

5徐忠兰,郝健.钼板材轧制过程的数值模拟及其工艺参数的优化[J].稀有金属与硬质合金,2013,41(3):41-45. 被引量:1

6郭让民,淡新国,侯军涛.钼镧合金板材高温抗载荷弯曲性能研究[J].中国钼业,2013,37(3):47-49. 被引量:7

7黄江波,魏修宇,李光宗,张外平,夏艳成,常理,宋立强.热轧变形量及退火工艺对钼板材组织和性能的影响[J].硬质合金,2013,30(5):270-274. 被引量:8

8谭江飞,王快社,胡平,杨帆,于志涛,王华,何欢承,康轩齐.TZM合金高温性能研究现状[J].材料导报,2014,28(23):68-71. 被引量:5

9傅崇伟,魏修宇.粉末特性和加工工艺参数对钼板组织和性能影响的研究[J].硬质合金,2014,31(6):347-352. 被引量:3

10许晓静,陆文俊,蒋凌,卢予东,王子路,郭云飞.轧制驱动ECA大应变加工及后续热处理对5052铝合金力学性能与晶体取向的影响[J].稀有金属,2015,39(8):759-763. 被引量:5

1张蓉,钱书琨.轧制温度对交叉轧制AZ31镁合金板材显微组织和力学性能的影响[J].机械工程材料,2013,37(10):13-16.

2一种制备高性能引伸钼带的方法[J].中国钼业,2008,32(5):39-39.

3邓自南,赵娟,杨明杰.轧制工艺对深冲钼带组织和性能的影响[J].稀有金属快报,2008,27(4):18-21. 被引量:4

4刘劲松,竺晓华,张士宏,郑黎,宋广胜,王忠堂.AZ31镁合金轧制板材退火后的组织与力学性能[J].材料热处理学报,2010,31(2):104-107. 被引量:12

5张青来,李敏,韩寅奔,韩伟东,冯甜甜.交叉轧制钼带冷深冲性能及微观组织研究[J].稀有金属材料与工程,2012,41(12):2109-2112. 被引量:8

6刘劲松,竺晓华,郑黎,王忠堂,宋广胜,张士宏.AZ31镁合金交叉轧制塑性应变有限元模拟分析[J].轻合金加工技术,2009,37(2):18-20. 被引量:4

7史乃安,邹波,阎东宇,吴胜田.ASP小交叉轧制工艺研究[J].轧钢,2008,25(1):21-24. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]

Citation Information:

The effect of rolling process on microstructure and property of molybdenum sheet was investiga- ted by changing rolling capacity, rolling temperature and rolling process. The results show that the longitudinal and transverse microstructures and properties of molybdenum sheet are similar by high-rate blooming and low temperature alternative rolling process. Meanwhile, the sheet can be adapted to the downstream operation.

quote

GB/T 7714-2015 [1] DENG Zi-nan, GUO Lei, ZHAO Juan, et al. Effect of Rolling Process on Microstructure and Property of Warm Rolled Molybdenum Sheet for Down-stream Operation[J]. Rare Metals and Cemented Carbides, 2008(3): 24-26.
MLA [1] DENG Zi-nan, et al., "Effect of Rolling Process on Microstructure and Property of Warm Rolled Molybdenum Sheet for Down-stream Operation." Rare Metals and Cemented Carbides, no. 3, 2008, pp. 24-26.
APA [1] DENG Zi-nan, GUO Lei, ZHAO Juan, JIN Bo, HUANG Xian-ming, & YANG Ming-jie. (2008). Effect of Rolling Process on Microstructure and Property of Warm Rolled Molybdenum Sheet for Down-stream Operation. Rare Metals and Cemented Carbides(3), 24-26.
IEEE [1] DENG Zi-nan, GUO Lei, ZHAO Juan, JIN Bo, HUANG Xian-ming, and YANG Ming-jie, "Effect of Rolling Process on Microstructure and Property of Warm Rolled Molybdenum Sheet for Down-stream Operation," Rare Metals and Cemented Carbides, no. 3, pp. 24-26, 2008. keywords: {molybdenum sheet;down stream operation;rolling process;microstructure and property;low temperature cross rolling}