Effect of Doping on the Texture and Property of Tantalum Wire AITranslate
Abstract AITranslate
Effect of doping on microstructure and property of tantalum bar and wire is carefully investigated through observation of microstructure and SEM fractograph. The results show that with the increase of the dopant,the tantalum bar grain is refined,and the degree of grain refinement with dopant B is higher than that with dopant A. However,the increase of dopant B has resulted in a lower density of Ta bar. The increase of the dopant has resulted in tantalum wire having a higher recrystallization temperature and texture grain refinement degree, and the effect of the grain refinement with dopant B is more obvious than that with dopant A. Insufficient sintering and incomplete recrystallization at annealing are the main causes of burr and pit during the production of doped tantalum wire.
KeyWords AITranslate
1黄伯云.中国材料工程大典(第四卷)[M].北京:化学工业出版社,2005.247-250.
2何季麟.中国钽铌工业的进步与展望[J].中国工程科学,2003,5(5):40-46. 被引量:17
3何季麟.钽铌工业的进步与展望[J].稀有金属,2003,27(1):23-27. 被引量:41
4吴铭,邵志俊,孙有路,乔考德.钽铌冶金工艺学[M].北京:中国有色金属工业总公司,1995.309.
5泉知夫.TMS第125届年会论文[C].东京:昭和卡博特出版社,1996.
6Charles P. Controlling the texture of tantalum plate[J]. Journal of Metals, 1989,10:46-49.
1解永旭,马建政,韩鹏,姚俊武.冶金级钽粉微观结构对钽丝性能影响[J].金属制品,2017,43(4):16-19. 被引量:3
2解永旭,包玺芳,马建政,韩鹏.影响电容器级钽丝脆性因素的研究[J].金属制品,2017,43(6):26-30. 被引量:2
1王强,黄云红,牟东,陈飞.碳还原法生产冶金级钽粉的工艺研究[J].冶金管理,2019,0(17):35-36.
2刘闯.关于影响电容器级钽丝脆性因素的分析[J].科学与信息化,2020,0(1):107-107.
3李福成,柳金洲,包富贵,赵刚.钠还原电容器级FTW70K钽粉中Si的来源及其存在形态分析[J].宁夏大学学报:自然科学版,2020,41(4):388-392.
4马建政,解永旭,万庆峰,韩鹏.氢化钽粉烧结方式对钽丝加工过程及其性能的影响[J].云南冶金,2022,51(1):96-100.
1李国平,王建军,吴天海,温艳慧,李花兵,刘春明.2205双相不锈钢TIG焊接头组织及力学性能[J].材料研究学报,2016,30(12):897-902. 被引量:15
2赵晓萍,张国滨,张贵杰.高速线材的再结晶规律[J].河北理工大学学报:自然科学版,2008,30(4):45-49. 被引量:2
3刘小文,杨宁宁,穆耀钊,鄢君辉.紫铜-黄铜搅拌摩擦焊接头的组织与力学性能[J].中国有色金属学报,2005,15(5):700-704. 被引量:5
4王希靖,叶结和,孙丙岩,王丽.0Cr18Ni9不锈钢搅拌摩擦焊接头的微观组织和性能[J].热加工工艺,2006,35(23):36-38. 被引量:12
5张振亚,于化顺,王少卿,王海涛,闵光辉.快速凝固/粉末冶金法制备ZK60高强镁合金[J].材料工程,2010,38(5):72-77. 被引量:6
6余凌锋,梁宇,周磊.GH4169高温合金焊接接头的组织与性能[J].金属热处理,2014,39(4):88-91. 被引量:5
7张宇,葛昌纯,沈卫平,邱成杰.喷射成型FGH4095静态再结晶组织特征[J].物理学报,2012,61(20):508-515. 被引量:1
8钱红丽,周琦,陈俐,杨璟,何恩光.7A52铝合金光纤激光焊接头组织性能分析[J].焊接,2014(9):49-52. 被引量:10
9张洪梅,苏玉洁,黄桂杰,李丹.6061-T6铝合金棒材尾端中心大晶粒的研究[J].轻合金加工技术,2005,33(8):34-36. 被引量:5
10解永旭,万庆峰,马跃忠,韩鹏,刘云峰,张晓.钇掺杂钽丝拉拔断裂机理分析[J].有色金属工程,2014,4(1):24-26. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]
Citation Information:
Effect of doping on microstructure and property of tantalum bar and wire is carefully investigated through observation of microstructure and SEM fractograph. The results show that with the increase of the dopant,the tantalum bar grain is refined,and the degree of grain refinement with dopant B is higher than that with dopant A. However,the increase of dopant B has resulted in a lower density of Ta bar. The increase of the dopant has resulted in tantalum wire having a higher recrystallization temperature and texture grain refinement degree, and the effect of the grain refinement with dopant B is more obvious than that with dopant A. Insufficient sintering and incomplete recrystallization at annealing are the main causes of burr and pit during the production of doped tantalum wire.
quote
| GB/T 7714-2015 | [1] WAN Qing-feng, WANG De-zhi, ZHAO Bing, et al. Effect of Doping on the Texture and Property of Tantalum Wire[J]. Rare Metals and Cemented Carbides, 2008(3): 27-30. |
| MLA | [1] WAN Qing-feng, et al., "Effect of Doping on the Texture and Property of Tantalum Wire." Rare Metals and Cemented Carbides, no. 3, 2008, pp. 27-30. |
| APA | [1] WAN Qing-feng, WANG De-zhi, ZHAO Bing, CHEN Lin, & TIAN Miao. (2008). Effect of Doping on the Texture and Property of Tantalum Wire. Rare Metals and Cemented Carbides(3), 27-30. |
| IEEE | [1] WAN Qing-feng, WANG De-zhi, ZHAO Bing, CHEN Lin, and TIAN Miao, "Effect of Doping on the Texture and Property of Tantalum Wire," Rare Metals and Cemented Carbides, no. 3, pp. 27-30, 2008. keywords: {tantalum wire doping texture property;burr} |