Preliminary Study of VB Doping for Improvement of Graphite Cathode Material AITranslate
Abstract AITranslate
VB is doped into graphite with solid-phase method. Study is made of the effect of VB dosage, roasting temperature and duration on the electrochemical property of the composite material. The following optimum technological parameters were developed as follows through orthogonal experiment: VB dosage 9%, the roasting temperature 1 200 ℃, roasting duration 3 h. The test results prove that the optimized synthesis technology is good for improvement of electrochemical property of lithium ion battery cathode material.
KeyWords AITranslate
1马军旗,胡成秋.提高锂离子电池炭负极材料性能的表面处理方法[J].炭素技术,2000,19(5):22-27. 被引量:17
2宋文生,胡成秋,尚尔超.锂离子二次电池炭负极材料[J].化学推进剂与高分子材料,2001(3):7-11. 被引量:1
3Hisayoshi Yoshida, Ogoori, Iehitaro Ogawa, et al. Silicon Carbide-boron Carbide Carbonaceous Body[P]. US Pat: 4518702,1985-05-21.
4尹鸽平,周德瑞,夏保佳,史鹏飞.掺磷碳材料的制备及其嵌锂行为[J].电池,2000,30(4):147-149. 被引量:12
5吴宇平,万春荣,姜长印,李建军.锂离子二次电池碳负极材料的改性[J].电化学,1998,4(3):286-292. 被引量:14
6Weibing Xing, Wilson A M, Zank G, et al. Pyrolysed pitch-polysilane blends for use as anode materials in lithium ion batteries[J]. Solid State Ionics,1997,93(3) :239-244.
7Tossic R, Berrettoni M, Rosolen M, et al. Electrochemistry of KC8 in lithium-containing electrolytes and its use in lithium-ion cells[J]. Electrochem Soc, 1997,144 (1) : 186-192.
8新田芳明.非水電解液二次電池[P].日本专利:特开平8-106898,1996-04-23.
9Wu Y P,Ju W G,Fang S B,etal. 6th international symposium on fine[J]. Chemistry & Functional Polymers (FCFP-VI), 1996:122 : 23-24.
10Wu Y P,Ju W G, Fang S B, et al. improving the electrochemical properties of carbon anodes in lithium secondary batteries[J]. Power Sources, 1998 , 70(1) : 114-117
1一种与打火机一样大小的燃料电池[J].现代材料动态,2003(3):26-26.
2邹邦坤,丁楚雄,陈春华.锂离子电池三元正极材料的研究进展[J].中国科学:化学,2014,44(7):1104-1115. 被引量:52
3柴永泉,唐永光.一硼化铌超导体电子结构研究[J].河北师范大学学报:自然科学版,2004,28(3):263-265.
4谭俐,曲群婷,张力,郑洪河.LiFePO_4/石墨电池容量衰退与抑制方法[J].化学通报,2013,76(10):888-896. 被引量:3
5程广玉,顾洪汇,高蕾,王可.电解液对LiNi_(0.8)Co_(0.15)Al_(0.05)O_2/石墨电池性能的影响[J].电池,2016,46(2):87-90. 被引量:3
6周国华,皮晓明,陈倪莉.锂离子电池石墨负极材料掺杂碳纳米管研究[J].电源技术,2015,39(6):1189-1190. 被引量:1
7刘云建,宋杨,魏洪兵,王彩娟,赵永,金挺,李新海,郭华军.锰酸锂电池储存后容量衰减机理[J].中国有色金属学报,2011,21(11):2812-2818. 被引量:10
8周德凤,李晓路,赵宝华,王荣顺.硼化酚醛树脂炭材料的制备及嵌锂性能[J].化学世界,2006,47(5):260-262.
9杜荣斌.尖晶石材料LiMn_2O_4的研究现状及展望[J].化工新型材料,2006,34(2):1-4. 被引量:4
10龚蓉,陈红雨.三元正极材料LiMn_(1/3)Ni_(1/3)Co_(1/3)O_2改性研究现状[J].电池工业,2014,19(1):47-52. 被引量:9
Basic Information:
DOI:
Chinese Library Classification Number:TM912.9[电气工程—电力电子与电力传动]
Citation Information:
VB is doped into graphite with solid-phase method. Study is made of the effect of VB dosage, roasting temperature and duration on the electrochemical property of the composite material. The following optimum technological parameters were developed as follows through orthogonal experiment: VB dosage 9%, the roasting temperature 1 200 ℃, roasting duration 3 h. The test results prove that the optimized synthesis technology is good for improvement of electrochemical property of lithium ion battery cathode material.
quote
| GB/T 7714-2015 | [1] ZHANG Xiao-kang, ZHONG Hui, DAI Yan-yang. Preliminary Study of VB Doping for Improvement of Graphite Cathode Material[J]. Rare Metals and Cemented Carbides, 2008(3): 31-34. |
| MLA | [1] ZHANG Xiao-kang, et al., "Preliminary Study of VB Doping for Improvement of Graphite Cathode Material." Rare Metals and Cemented Carbides, no. 3, 2008, pp. 31-34. |
| APA | [1] ZHANG Xiao-kang, ZHONG Hui, & DAI Yan-yang. (2008). Preliminary Study of VB Doping for Improvement of Graphite Cathode Material. Rare Metals and Cemented Carbides(3), 31-34. |
| IEEE | [1] ZHANG Xiao-kang, ZHONG Hui, and DAI Yan-yang, "Preliminary Study of VB Doping for Improvement of Graphite Cathode Material," Rare Metals and Cemented Carbides, no. 3, pp. 31-34, 2008. keywords: {lithium ion battery;cathode material;VB;doping;orthogonal test} |