Synthesis of LiFePO_4/C Anode Material for Lithium-ion Battery AITranslate

School of Materials Science and Engineering, Chang'an University;School of Materials Science and Engineering, Chang'an University;School of Materials Science and Engineering, Chang'an University;School of Materials Science and Engineering, Chang'an University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The LiFePO4/C anode material for lithium-ion batteries was synthesized by solid-phase synthesis. The crystalline structure,grain morphology and electrochemical performance of the product were investiga-ted. The results show that the resultant LiFePO4/C has simple pure olive-type structure with uniform distribution of the gain sizes. The initial specific charge and discharge capacity of LiFePO4/C is the highestwith 115 mAh/g at the rate of 0.1C and the retained capacity is 97% after 20 cycles .

KeyWords AITranslate

lithium-ion battery anode material LiFePO4/C synthesis

1Wakihara M, Yamaoto O. Lithium Ion Battery-Fundamentals and Performance[M]. New York: Wiley-Vch, 1998.

2陈杨,周振君,童昀,朱海霞,张丽军.锂离子电池正极材料的研究进展与展望[J].稀有金属与硬质合金,2007,35(3):54-57. 被引量:1

3Anderson A S. The source of first-cycle capacity loss in LiFeO4 [J]. J Power Sources, 2001,97-98 : 498-501.

1白立朋,李秋红,陈立宝,陈杰,王太宏.形貌对LiFePO_4性能影响的研究进展[J].微纳电子技术,2010,47(3):152-156. 被引量:2

1郑波,郎雷鸣.丙三醇辅助水热法合成纳米棒状LiFePO_4[J].化学研究与应用,2011,23(10):1401-1404. 被引量:1

2蒋阳梅,刘全兵,罗传喜,廖世军.具有特殊形貌的纳米级磷酸铁锂正极材料的合成及研究进展[J].现代化工,2012,32(1):23-29. 被引量:4

1王守伟,苏雪花,夏德强.碳包覆对正极材料LiFePO_4结构的影响[J].山东化工,2016,45(21):32-33.

2李涛,魏明坤,王雪飞,吴静,罗田,王灏.埋炭条件下制备LiFePO_4材料的性能研究[J].广东化工,2010,37(12):5-6. 被引量:1

3徐文飞,范供齐,施丰华,王海波.硅酸盐橙红色荧光粉的制备与发光性能研究[J].中国照明电器,2012(5):7-10. 被引量:1

4杨志萍,杜海燕,孙家跃.上转换发光材料的合成与应用[J].化工新型材料,2009,37(2):6-8. 被引量:5

5黄小文.锂离子电池正极材料LiFePO_4/C的制备及电化学性能研究[J].广州化工,2014,42(24):70-71.

6刘鸣,李宝骏,张宝刚,周萌,刘晓伟,李颖,付丽.Ca_xSr_(1-x)Al_2O_4∶Eu^(2+)磷光体的制备及性能研究[J].辽宁化工,2005,34(1):14-16. 被引量:2

7李强,周启立,宋晓莉.硼酸镁晶须的制备及应用[J].无机盐工业,2004,36(2):13-14. 被引量:17

8彭能,黄奇书,雷一锋,张四奇,郑爱勤.葡萄糖添加量对LiFePO_4/C性能影响的研究[J].材料研究与应用,2011,5(4):263-266.

9姚耀春,戴永年,任海伦,李伟宏,崔萌佳.合成温度与时间对尖晶石LiMn_2O_4性能的影响[J].有色金属,2005,57(2):32-34. 被引量:5

10王守伟,苏雪花,夏德强.合成温度对磷酸亚铁锂电化学性能的影响[J].兰州石化职业技术学院学报,2013,13(4):28-30. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动];TQ132.2[化学工程—无机化工]

Citation Information:

The LiFePO4/C anode material for lithium-ion batteries was synthesized by solid-phase synthesis. The crystalline structure,grain morphology and electrochemical performance of the product were investiga-ted. The results show that the resultant LiFePO4/C has simple pure olive-type structure with uniform distribution of the gain sizes. The initial specific charge and discharge capacity of LiFePO4/C is the highestwith 115 mAh/g at the rate of 0.1C and the retained capacity is 97% after 20 cycles .

quote

GB/T 7714-2015 [1] CHEN Yang, ZHOU Zhen-jun, TONG Yun, et al. Synthesis of LiFePO_4/C Anode Material for Lithium-ion Battery[J]. Rare Metals and Cemented Carbides, 2008(3): 35-37.
MLA [1] CHEN Yang, et al., "Synthesis of LiFePO_4/C Anode Material for Lithium-ion Battery." Rare Metals and Cemented Carbides, no. 3, 2008, pp. 35-37.
APA [1] CHEN Yang, ZHOU Zhen-jun, TONG Yun, & ZHU Hai-xia. (2008). Synthesis of LiFePO_4/C Anode Material for Lithium-ion Battery. Rare Metals and Cemented Carbides(3), 35-37.
IEEE [1] CHEN Yang, ZHOU Zhen-jun, TONG Yun, and ZHU Hai-xia, "Synthesis of LiFePO_4/C Anode Material for Lithium-ion Battery," Rare Metals and Cemented Carbides, no. 3, pp. 35-37, 2008. keywords: {lithium-ion battery anode material LiFePO4/C synthesis}