Study on the Poly(N-Isopropylacrylamide-co-Styrene) Microgel Interaction with Samarium(Ⅲ) AITranslate

Wuxi Jiajian Medical Equipment Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The complex of N-isopropylacrylamide and styrene copolymeric microgel P(NIPAM-co-St) with Sm was prepared by soapless emulsion polymerization. The complex was characterized by transmission electron micrography (TEM), dynamic light scattering (DLS), Zeta potential, UV spectrum, IR spectrum and fluorescence spectrum. The results showed that the mierogel particle size and surface morphology had no remarkable change after the Samarium addition and samarium interacted with microgel mainly by electrostatic action. Effective energy transfer failed due to unmatched energy level between microgel and Sm (Ⅲ).

KeyWords AITranslate

Poly(N-isopropylacry.lamide) styrene microgel Sm (Ⅲ) fluorescence spectrum

1Hoffmann S. Applications of thermally reversible polymers and hydrogels in therapeutics and Diagnostics[J]. Control Release,1987, 69(1) :297-305.

2Yoshioka H, Mikami M, Nakai T, et al. Preparation of poly (N-isopropylacrylamide)-grafted silica gel and its temperature-dependent interaction with proteins[J].Polymers for Advanced Technologies, 1994, 6 (6) : 418- 420.

3Kondo A, Kaneko T, Higashitani K. Development and application of thermo-sensitive immunmicrospheres for antibody purification[J]. Biotechnology and Bioengineering, 1994,44(1) : 1-6 .

4Shibayama M, Tanaka T. Volume phase-transition and related phenomena of polymer gels [J]. Advances in Polymer Science, 1993,109:1-62.

5Wu X Y, Lee P I. Preparation and characterization of thermal and pH-sensitive nanospheres[J]. Pharmaceutical Research, 1993,10(10): 1 544-1 547.

6Chaaya R G, Anna G, Liu F, et al. Polymer molecular weight alters properties of pH-/temperature-sensitive polymeric beads[J]. Pharmaceutical Research, 1999,16 (6):819-827.

7肖雨亭,陈明清,陆天虹,MITSURU Akashi,黄晓华.聚N-异丙基丙烯酰胺-丙烯酸共聚微凝胶与Tb(Ⅲ)相互作用的研究[J].高分子学报,2005(3):458-462. 被引量:10

8肖雨亭,陈明清,陆天虹,Mitsuru Akashi,黄晓华.聚N-异丙基丙烯酰胺-丙烯酸共聚微凝胶与Eu(Ⅲ)的相互作用[J].江南大学学报:自然科学版,2005,4(5):531-535. 被引量:1

9Yin W Q,Chen M Q, Lu TH ,et al. Study on interaction between Tb (Ⅲ) and poly(N-isopropylacrylamide)[J]. European Polymer Journal, 2006,42(6) : 1 305-1 312.

10Banks E,Okamoto Y. Rare earth metal containing polymer(Ⅰ) [J]. Journal of Applied Polymer Science, 1980, 25(2) :359-368.

1陈栋栋,王林,孙俊奇.表面活性剂胶束实现疏水分子在聚合物微凝胶层层组装膜中的高效负载[J].化学学报,2012,70(17):1779-1784. 被引量:4

2吴俊涛,于成芬,陈守明,赵晓燕,吴其晔.核壳型St/BVA/BA微凝胶的制备及性能测试[J].高分子材料科学与工程,2001,17(3):48-51. 被引量:6

3刘峰,王旭,叶开其,裘令瑛,沈家骢.塑料表面载银微凝胶层层组装膜的制备及抗菌活性[J].高等学校化学学报,2011,32(4):990-994. 被引量:10

4Zhang, Ying Liu, Huijin Fang, Yu.Preparation of CuS-P(NIPAM-co-MAA) Hybrid Microgels with Controlled Surface Structures[J].中国化学:英文版,2011,29(1):33-40.

5王尊志,张健夫,陈栋栋.导尿管表面具有抗菌功能的层层组装微凝胶膜[J].应用化学,2014,31(10):1149-1155. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:O613.24[理学—无机化学];O614.33[理学—无机化学]

Citation Information:

The complex of N-isopropylacrylamide and styrene copolymeric microgel P(NIPAM-co-St) with Sm was prepared by soapless emulsion polymerization. The complex was characterized by transmission electron micrography (TEM), dynamic light scattering (DLS), Zeta potential, UV spectrum, IR spectrum and fluorescence spectrum. The results showed that the mierogel particle size and surface morphology had no remarkable change after the Samarium addition and samarium interacted with microgel mainly by electrostatic action. Effective energy transfer failed due to unmatched energy level between microgel and Sm (Ⅲ).

quote

GB/T 7714-2015 [1] XIAO Yu-ting. Study on the Poly(N-Isopropylacrylamide-co-Styrene) Microgel Interaction with Samarium(Ⅲ)[J]. Rare Metals and Cemented Carbides, 2008(3): 15-18.
MLA [1] XIAO Yu-ting. "Study on the Poly(N-Isopropylacrylamide-co-Styrene) Microgel Interaction with Samarium(Ⅲ)." Rare Metals and Cemented Carbides, no. 3, 2008, pp. 15-18.
APA [1] XIAO Yu-ting. (2008). Study on the Poly(N-Isopropylacrylamide-co-Styrene) Microgel Interaction with Samarium(Ⅲ). Rare Metals and Cemented Carbides(3), 15-18.
IEEE [1] XIAO Yu-ting, "Study on the Poly(N-Isopropylacrylamide-co-Styrene) Microgel Interaction with Samarium(Ⅲ)," Rare Metals and Cemented Carbides, no. 3, pp. 15-18, 2008. keywords: {Poly(N-isopropylacry.lamide);styrene;microgel;Sm (Ⅲ);fluorescence spectrum}