Experimental Study on Feasibility of Catalytic Denitrification by Rare Earth Tailings AITranslate

School of Environment&Energy,Inner Mongolia University of Science&Technology;School of Environment&Energy,Inner Mongolia University of Science&Technology;School of Environment&Energy,Inner Mongolia University of Science&Technology;School of Environment&Energy,Inner Mongolia University of Science&Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

X-ray fluorescence spectrometer(XRF),X-ray diffractometer(XRD) and scanning electron microscopy(SEM) were used to characterize the rare earth tailings.It is found that there are many elements in the tailings,and the relationship among minerals is complex.According to the characteristics of rare earth tailings,the catalytic denitrification performance of rare earth tailings was tested in a vertical tube furnace.The results show that NO conversion rate increases with the increase of reaction temperature and gas residence time,and NO conversion rate in fixed bed reactor is higher than that in bubbling bed reactor.When the reaction temperature is 800 ℃,NO conversion rate reaches 98.7%.The denitration catalyst was prepared by grinding and roasting with pseudo-boehmite and rare earth tailings as raw materials.When the total amount of rare earth tailings remains unchanged,the NO conversion rate increases with the increase of pseudo-boehmite mass.When the reaction temperature is 600 ℃,the NO conversion rate of the catalyst with the mass ratio of pseudo-boehmite to rare earth tailings of 1∶2 is 15% higher than that of the pure rare earth tailings.The thermodynamic calculation proves that the rare earth tailings with high iron content is feasible for CO reduction denitrification.

KeyWords AITranslate

catalytic denitration rare earth tailing CO pseudo-boehmite NO conversion rate thermodynamic calculation

1张悦,林海,董颖博,许晓芳,王鑫,高月娇.白云鄂博地区尾矿中铁、铌、稀土、萤石综合回收研究[J].稀有金属,2017,41(7):799-809. 被引量:27

2郭伟,付瑞英,赵仁鑫,赵文静,郭江源,张君.内蒙古包头白云鄂博矿区及尾矿区周围土壤稀土污染现状和分布特征[J].环境科学,2013,34(5):1895-1900. 被引量:70

3郭财胜,李梅,柳召刚,张栋梁,高凯.白云鄂博稀土、铌资源综合利用现状及新思路[J].稀土,2014,35(1):96-100. 被引量:53

4张鉴.白云鄂博共生矿铁选矿技术现状与展望[J].包钢科技,2004,30(3):1-5. 被引量:5

5龚志军,赵蕾,李保卫,武文斐.稀土尾矿对半焦燃烧NO_x产生量的影响研究[J].稀土,2018,39(5):144-150. 被引量:2

6胡辉,王书霞,张晓玲,赵全中,李劲.Study on Simultaneous Catalytic Reduction of Sulfur Dioxide and Nitric Oxide on Rare Earth Mixed Compounds[J].稀土学报:英文版,2006,24(6):695-698. 被引量:13

7顾卫荣,周明吉,马薇,王玉丽.选择性催化还原脱硝催化剂的研究进展[J].化工进展,2012,31(7):1493-1500. 被引量:53

8王坤,龚志军,武文斐.水热法制备稀土基催化剂及其NH_3-SCR脱硝性能研究[J].稀有金属与硬质合金,2018,46(5):37-42. 被引量:2

1李雪礼,袁程远,王启飞,张琰图.抗铁污染催化裂化催化剂的制备及性能评价[J].石油炼制与化工,2020,51(6):42-46. 被引量:3

2梁晓彤,李博.煤热解产物分布影响因素研究[J].科技风,2020,0(1):156-156.

3李晓明,张红,智丽飞.碱金属K对无烟煤灰熔融性的影响规律[J].热科学与技术,2019,18(6):483-489.

4胡雯雯.SCR脱硝催化剂在生物质电厂的应用[J].电子乐园,2019,0(33):0462-0462.

5刘海岩,李冬,苗雪,朱元元,刘小峰,吕莹,李杰,吴萍霞,彭悦,陈建军,李俊华.CuO-WO3/TiO2催化剂制备方法对NH3-SCR脱硝性能的影响[J].环境工程,2020,38(5):89-95. 被引量:3

6高秀平.紫砂壶泥料与造型简介[J].陶瓷科学与艺术,2020,54(4):96-96.

7毛书磊,李云霞,张秋月,徐良龙,朱承驻.介质阻挡放电协同Bi2WO6/天然赤铁矿降解乙酸乙酯[J].环境科学研究,2020,33(2):333-340. 被引量:3

8王杰,崔荣基,杨秉川,孙淑君,马素霞.采用底渣灰碱-磁改性催化H2O2脱除NO[J].煤炭学报,2019,44(11):3571-3577. 被引量:1

9吕长海,李晶,吴国平,闫威,闫晨,戴雨翔.转炉生产低碳低磷钢炉衬侵蚀机理研究[J].江西冶金,2019,39(6):1-8. 被引量:4

10思积勇,李领贵,张子龙.西藏多才玛铅锌矿石工艺矿物学研究[J].矿产保护与利用,2020,40(1):105-109. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TQ426.83[化学工程]

Citation Information:

X-ray fluorescence spectrometer(XRF),X-ray diffractometer(XRD) and scanning electron microscopy(SEM) were used to characterize the rare earth tailings.It is found that there are many elements in the tailings,and the relationship among minerals is complex.According to the characteristics of rare earth tailings,the catalytic denitrification performance of rare earth tailings was tested in a vertical tube furnace.The results show that NO conversion rate increases with the increase of reaction temperature and gas residence time,and NO conversion rate in fixed bed reactor is higher than that in bubbling bed reactor.When the reaction temperature is 800 ℃,NO conversion rate reaches 98.7%.The denitration catalyst was prepared by grinding and roasting with pseudo-boehmite and rare earth tailings as raw materials.When the total amount of rare earth tailings remains unchanged,the NO conversion rate increases with the increase of pseudo-boehmite mass.When the reaction temperature is 600 ℃,the NO conversion rate of the catalyst with the mass ratio of pseudo-boehmite to rare earth tailings of 1∶2 is 15% higher than that of the pure rare earth tailings.The thermodynamic calculation proves that the rare earth tailings with high iron content is feasible for CO reduction denitrification.

quote

GB/T 7714-2015 [1] WANG Jian, GONG Zhi-jun, XU Guo-dong, et al. Experimental Study on Feasibility of Catalytic Denitrification by Rare Earth Tailings[J]. Rare Metals and Cemented Carbides, 2020(2): 22-27.
MLA [1] WANG Jian, et al., "Experimental Study on Feasibility of Catalytic Denitrification by Rare Earth Tailings." Rare Metals and Cemented Carbides, no. 2, 2020, pp. 22-27.
APA [1] WANG Jian, GONG Zhi-jun, XU Guo-dong, & WU Wen-fei. (2020). Experimental Study on Feasibility of Catalytic Denitrification by Rare Earth Tailings. Rare Metals and Cemented Carbides(2), 22-27.
IEEE [1] WANG Jian, GONG Zhi-jun, XU Guo-dong, and WU Wen-fei, "Experimental Study on Feasibility of Catalytic Denitrification by Rare Earth Tailings," Rare Metals and Cemented Carbides, no. 2, pp. 22-27, 2020. keywords: {catalytic denitration;rare earth tailing;CO;pseudo-boehmite;NO conversion rate;thermodynamic calculation}