Effect of Refiner Addition on Particle Size and Electrical Properties of FTB-48 Capacitor Tantalum Powder AITranslate

Guangdong Rising Rare Metals-EO Materials Ltd.;Guangdong Rising Rare Metals-EO Materials Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of adding the refiner Na2SO4 in the stirring sodium reduction process during capacitor tantalum powder preparation on the particle size of the intermediate product washed powder and the particle size and electrical properties of the final product FTB-48 tantalum powder were studied.The experimental results indicate that the particle sizes of the washed powder and FTB-48 tantalum powder prepared by adding the refiner Na2SO4 were reduced,and the sintering shrinkage and weight specific capacitance of FTB-48 tantalum powder were improved to some extent.The intermediate product washed powder will agglomerate and sinter during the high-temperature heat treatment,which causes the particle size of FTB-48 tantalum powder product to increase.

KeyWords AITranslate

capacitor tantalum powder particle size electrical property refiner addition Na2SO4 sodium reduction

1胡小锋,许茜,吴艳.钽粉制备工艺研究进展[J].材料导报,2005,19(10):97-99. 被引量:11

2柴立元,钟海云.氟钽酸钾钠还原生产钽粉的工艺现状及展望[J].稀有金属与硬质合金,1994,22(4):30-33. 被引量:4

3包玺芳,马跃忠,王治道,李仲香.金属钽粉湿法提纯的水洗和酸洗方法研究[J].宁夏工程技术,2012,11(1):46-48. 被引量:7

4王东新,李军义,孙本双,任晓,何季麟.钽粉制备新工艺研究进展[J].湖南有色金属,2011,27(3):34-37. 被引量:19

1李承泽,尤俊华,白鹤山,张维维,刘苏杰.高熵合金的热处理综述[J].材料热处理学报,2020,41(5):1-12. 被引量:7

2马建政,解永旭,韩鹏,崔新民.钽粉物理性能对钽棒烧结效果的影响[J].中国金属通报,2020(4):91-92.

3夏小成.建筑工程结构检测的主要方法及质量控制[J].地产,2019,0(23):142-142. 被引量:1

4方力.花园生物:高利润率难持续[J].证券市场周刊,2020,0(9):34-35.

5杨磊,邓亚辉.湿法磷酸装置的改造及用材研究[J].神州,2020(16):231-231.

6张伟罡,龚希武.基于机器学习的工业炉智能控制与实现[J].工业炉,2020,42(3):45-49. 被引量:4

7高利军,白思林,梁苏岑,穆野,董强,胡超.ZIF衍生多孔碳纳米纤维用于高效电容去离子的研究[J].化工学报,2020,71(6):2760-2767. 被引量:3

8刘睿雯,徐舒,张川川.贸易开放、就业结构变迁与生产率增长[J].中国工业经济,2020,0(6):24-42. 被引量:18

9曹京华,潘红波,章静,张腾飞,李旭冬,刘伟明.Nb-Ti微碳深冲双相钢的连续冷却转变规律[J].钢铁研究学报,2020,32(4):329-334. 被引量:3

10陆慧,陈银莉,韦贺,刘泽盛.55SiCr弹簧钢中的残留奥氏体与碳化物[J].金属热处理,2020,45(5):103-110. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]

Citation Information:

The effects of adding the refiner Na2SO4 in the stirring sodium reduction process during capacitor tantalum powder preparation on the particle size of the intermediate product washed powder and the particle size and electrical properties of the final product FTB-48 tantalum powder were studied.The experimental results indicate that the particle sizes of the washed powder and FTB-48 tantalum powder prepared by adding the refiner Na2SO4 were reduced,and the sintering shrinkage and weight specific capacitance of FTB-48 tantalum powder were improved to some extent.The intermediate product washed powder will agglomerate and sinter during the high-temperature heat treatment,which causes the particle size of FTB-48 tantalum powder product to increase.

quote

GB/T 7714-2015 [1] YUE Ri-hui, ZHOU Li. Effect of Refiner Addition on Particle Size and Electrical Properties of FTB-48 Capacitor Tantalum Powder[J]. Rare Metals and Cemented Carbides, 2020(2): 18-21.
MLA [1] YUE Ri-hui, and ZHOU Li. "Effect of Refiner Addition on Particle Size and Electrical Properties of FTB-48 Capacitor Tantalum Powder." Rare Metals and Cemented Carbides, no. 2, 2020, pp. 18-21.
APA [1] YUE Ri-hui, & ZHOU Li. (2020). Effect of Refiner Addition on Particle Size and Electrical Properties of FTB-48 Capacitor Tantalum Powder. Rare Metals and Cemented Carbides(2), 18-21.
IEEE [1] YUE Ri-hui and ZHOU Li, "Effect of Refiner Addition on Particle Size and Electrical Properties of FTB-48 Capacitor Tantalum Powder," Rare Metals and Cemented Carbides, no. 2, pp. 18-21, 2020. keywords: {capacitor tantalum powder;particle size;electrical property;refiner addition;Na2SO4;sodium reduction}