Effect of Annealing Time on Structure and Gaseous Hydrogen Absorption and Desorption Properties of LaMgNi3.9Mn0.2 Alloy AITranslate

College of Quality and Technical Supervision;College of Quality and Technical Supervision;College of Quality and Technical Supervision;College of Quality and Technical Supervision;College of Quality and Technical Supervision;College of Quality and Technical Supervision
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In order to study the effect of annealing time on structure and gaseous hydrogen absorption and desorption properties of LaMgNi3.9Mn0.2 alloy,the phase and microstructure of the alloy were tested by XRD and SEM,and the hydrogen absorption and desorption kinetics plot was tested by semi-automatic Siever′s method.The experimental results show that with the increase of annealing time,the content of main phase LaMg(NiMn)4 decreases,while the content of(La,Mg)(NiMn)5 increases.The surface of as-cast and annealed alloys is mainly composed of columnar crystals with different sizes,which has obvious structural heredity.With the increase of annealing time,the content differences of La,Mg and Ni in the columnar crystal region of the alloy decrease,which makes the element distribution more uniform.Mn element disappears in the columnar crystal intergranular region of the alloy annealed for 15 h and 20 h.After the first hydrogen absorption of as-cast and annealed alloys,the corresponding maximum hydrogen absorption is reached.Therefore,the annealing time has no effect on the activation performance of the alloy,but has a significant effect on the maximum hydrogen absorption and the saturated hydrogen absorption and desorption of the alloy.With the increase of annealing time,the maximum hydrogen absorption and saturated hydrogen absorption and desorption of the alloy decrease,but the hydrogen absorption and desorption saturation increases firstly and then decreases,and that of the alloy annealed for 15 h is relatively high.

KeyWords AITranslate

annealing time LaMgNi4 alloy as-cast structure hydrogen absorption and desorption property

1Yiming Li,Zhuocheng Liu,Guofang Zhang,Yanghuan Zhang,Huiping Ren.Single phase A2B7-type La-Mg-Ni alloy with improved electrochemical properties prepared by melt-spinning and annealing[J].稀土学报:英文版,2019,37(12):1305-1311. 被引量:5

1纪铭悦,田晓,刘昕瑀,田璐,杨艳春,塔娜.新型La-Mg-Ni系储氢合金相结构及其制备工艺研究进展[J].材料导报,2022,36(15):87-96. 被引量:1

1李志强,郭正华,何玉汝.Zr/Mn元素替代及退火处理对汽车电池用储氢合金电化学性能的影响[J].无机盐工业,2023,55(6):78-84.

1汪亮兵,张国庆,杨倩,罗永春.高熵合金CrNbTiVZr的微观组织及其在模拟PEMFC环境中腐蚀行为研究[J].金属功能材料,2020,27(1):30-37. 被引量:5

2郑坤,罗永春,邓安强,杨洋,张海民.A2B7型La0.3Y0.7Ni3.4–xMnxAl0.1储氢合金微观结构和电化学性能研究[J].无机材料学报,2020,35(5):549-555. 被引量:2

3Ting-ting Zhai,Ze-ming Yuan,Feng Hu,Long Luo,Yong-zhi Li,Hao Sun,Dian-chen Feng,Yang-huan Zhang.Influence of melt spinning and annealing treatment on structures and hydrogen storage thermodynamic properties of La0.8Pr0.2MgNi3.6Co0.4 alloy[J].钢铁研究学报:英文版,2020,27(1):114-120. 被引量:1

4魏胜君,刘利杰.V-Ti-Ni-Al电池负极用钒基储氢合金的制备及性能研究[J].钢铁钒钛,2020,0(1):54-58.

5Yang-Huan Zhang,Gang Huang,Ze-Ming Yuan,Shi-Hai Guo,Yan Qi,Dong-Liang Zhao.Electrochemical hydrogen storage behaviors of as-cast and spun RE-Mg-Ni-Co-Al-based AB2-type alloys applied to Ni-MH battery[J].稀有金属:英文版,2020,0(2):181-192. 被引量:1

6邵成伟,王俊涛,赵晓丽,惠卫军.两相区退火处理含铝中锰钢的组织和力学性能[J].钢铁,2020,55(5):87-93. 被引量:12

7潘美玲,马琰,刘飞,杜赵新.轧程中间退火工艺对高强β钛合金组织及性能的影响[J].塑性工程学报,2020,27(2):108-113. 被引量:8

8贾云刚,张铁珍,孙发民,吴显军,王甫村.凝析油加氢处理催化剂CoMoNi/Al2O3-ZrO2的研制及性能评价[J].精细石油化工进展,2019,20(6):40-42.

9郑坤,杨倩,杨洋,罗永春.La0.7Y0.3Ni3.4-xMnxAl0.1(Х=0~0.5)储氢合金微观结构和电化学性能[J].金属功能材料,2020,27(1):16-23. 被引量:6

10吕芳琳,张金秋,沈锡田.黄绿色磷灰石热处理改色工艺探究[J].宝石和宝石学杂志,2020,22(2):29-37. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG138.1[一般工业技术—材料科学与工程]

Citation Information:

In order to study the effect of annealing time on structure and gaseous hydrogen absorption and desorption properties of LaMgNi3.9Mn0.2 alloy,the phase and microstructure of the alloy were tested by XRD and SEM,and the hydrogen absorption and desorption kinetics plot was tested by semi-automatic Siever′s method.The experimental results show that with the increase of annealing time,the content of main phase LaMg(NiMn)4 decreases,while the content of(La,Mg)(NiMn)5 increases.The surface of as-cast and annealed alloys is mainly composed of columnar crystals with different sizes,which has obvious structural heredity.With the increase of annealing time,the content differences of La,Mg and Ni in the columnar crystal region of the alloy decrease,which makes the element distribution more uniform.Mn element disappears in the columnar crystal intergranular region of the alloy annealed for 15 h and 20 h.After the first hydrogen absorption of as-cast and annealed alloys,the corresponding maximum hydrogen absorption is reached.Therefore,the annealing time has no effect on the activation performance of the alloy,but has a significant effect on the maximum hydrogen absorption and the saturated hydrogen absorption and desorption of the alloy.With the increase of annealing time,the maximum hydrogen absorption and saturated hydrogen absorption and desorption of the alloy decrease,but the hydrogen absorption and desorption saturation increases firstly and then decreases,and that of the alloy annealed for 15 h is relatively high.

quote

GB/T 7714-2015 [1] CHEN Ya-fang, DONG Xiao-ping, MA Yu-rui, et al. Effect of Annealing Time on Structure and Gaseous Hydrogen Absorption and Desorption Properties of LaMgNi3.9Mn0.2 Alloy[J]. Rare Metals and Cemented Carbides, 2020(2): 28-34.
MLA [1] CHEN Ya-fang, et al., "Effect of Annealing Time on Structure and Gaseous Hydrogen Absorption and Desorption Properties of LaMgNi3.9Mn0.2 Alloy." Rare Metals and Cemented Carbides, no. 2, 2020, pp. 28-34.
APA [1] CHEN Ya-fang, DONG Xiao-ping, MA Yu-rui, LI Xu, GAO Teng-yuan, & SU Jian-wen. (2020). Effect of Annealing Time on Structure and Gaseous Hydrogen Absorption and Desorption Properties of LaMgNi3.9Mn0.2 Alloy. Rare Metals and Cemented Carbides(2), 28-34.
IEEE [1] CHEN Ya-fang, DONG Xiao-ping, MA Yu-rui, LI Xu, GAO Teng-yuan, and SU Jian-wen, "Effect of Annealing Time on Structure and Gaseous Hydrogen Absorption and Desorption Properties of LaMgNi3.9Mn0.2 Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 28-34, 2020. keywords: {annealing time;LaMgNi4 alloy;as-cast;structure;hydrogen absorption and desorption property}