Study on Experimental Parameters of Induction Smelting of Sm-Fe Alloy AITranslate
Abstract AITranslate
Sm-Fe alloy was prepared by induction smelting.The effects of smelting pressure and times on Sm volatilization during smelting and the Sm content,phase composition and microstructure evolution of Sm-Fe alloy at smelting end were studied by XRD,SEM and XRF.The optimum raw material state and Sm compensation amount were determined.The results show that the phase distribution of Sm-Fe alloy is more uniform and stable after multiple smelting.However,Sm-Fe alloy should not be smelted for too many times to avoid excessive volatilization of Sm,and three smelting times are enough.The higher the smelting pressure,the lower the Sm volatilization.Higher melting pressure can also inhibit the growth of the internal structure of the alloy.Using uniform and stable Sm-Fe alloy as the raw material of smelting is more conducive to suppressing the evaporation of Sm in the smelting process.Excessive Sm compensation cannot stabilize the Sm content of Sm-Fe alloy at smelting end.Generally,4% pure samarium compensation amount can be selected for induction smelting.
KeyWords AITranslate
1李大勇,段焕强.钐铁氮稀土永磁材料产业化进展[J].中国新技术新产品,2012(20):146-148. 被引量:17
2叶金文,刘颖,朱国丽,高升吉,涂铭旌.Zr元素对Sm_2Fe_(17)合金结构的影响[J].稀有金属材料与工程,2006,35(5):746-748. 被引量:7
3袁亮亮,高爱民,王书桓,王黎光.熔炼条件对钐铁合金成分的影响[J].有色金属工程,2018,8(5):11-14. 被引量:1
4启明.高性能稀土磁体的开发[J].金属功能材料,2007,14(1):41-42. 被引量:9
5叶金文,刘颖,张然,陈梅,朱国丽,高升吉,涂铭旌.各向同性Sm_2Fe_(17)N_x磁粉及其粘结磁体的制备[J].稀有金属材料与工程,2007,36(2):329-331. 被引量:5
6薛平,郭学益.Sm_2Fe_(17)N_x稀土永磁材料的研究现状及进展[J].稀有金属与硬质合金,2007,35(2):53-57. 被引量:8
7罗阳.SmFe_7金属间化合物——新一代磁体的希望[J].粉末冶金工业,2000,10(5):26-31. 被引量:7
1单亚玲.完成“大任务” 学习活动这样“走”[J].教育革新,2020,0(4):26-26.
2M.P.KUZ′MIN,M.Yu.KUZ′MINA,P.B.KUZ′MIN.利用无定形微硅粉生产不同硅含量硅铝合金的可能性与前景[J].中国有色金属学报:英文版,2020,30(5):1406-1418.
3赵竑.泛在电力物联网中安全信息实时调度方法研究[J].电子乐园,2019,0(33):0019-0019.
4孙鸿滨.企业税务风险管理控制的研究[J].现代国企研究,2019,0(12):27-27.
5李鑫,谢辉,杨宾,李双明.Mg2(Si,Sn)基热电材料研究进展[J].材料导报,2020,34(S01):43-47. 被引量:2
6王力.论抗战内迁对昆明文学生态演变的影响[J].南京师大学报:社会科学版,2020(3):151-160.
7李仪,陶宇.大数据技术下消费者个人信用信息共享的治理机制[J].中国信用,2020,0(2):126-126. 被引量:2
8杨勇,冯和平,王琪,陈瑞润,郭景杰,丁宏升,苏彦庆.添加Fe元素改善TiAl-Nb合金的显微组织和力学性能[J].中国有色金属学报:英文版,2020,30(5):1315-1324. 被引量:3
9邓佳诚,王赫男,李昊宸.Sc对Al-3Cu-1Li合金酸性条件下腐蚀行为的影响[J].沈阳航空航天大学学报,2020,37(2):35-42. 被引量:1
10李根,兰鹏,张家泉.基于Ce变质处理的TWIP钢凝固组织细化[J].金属学报,2020,56(5):704-714. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TG146.45[金属学及工艺—金属材料]
Citation Information:
Sm-Fe alloy was prepared by induction smelting.The effects of smelting pressure and times on Sm volatilization during smelting and the Sm content,phase composition and microstructure evolution of Sm-Fe alloy at smelting end were studied by XRD,SEM and XRF.The optimum raw material state and Sm compensation amount were determined.The results show that the phase distribution of Sm-Fe alloy is more uniform and stable after multiple smelting.However,Sm-Fe alloy should not be smelted for too many times to avoid excessive volatilization of Sm,and three smelting times are enough.The higher the smelting pressure,the lower the Sm volatilization.Higher melting pressure can also inhibit the growth of the internal structure of the alloy.Using uniform and stable Sm-Fe alloy as the raw material of smelting is more conducive to suppressing the evaporation of Sm in the smelting process.Excessive Sm compensation cannot stabilize the Sm content of Sm-Fe alloy at smelting end.Generally,4% pure samarium compensation amount can be selected for induction smelting.
quote
| GB/T 7714-2015 | [1] LIU Kun, WANG Shu-huan, ZHANG Yi-kun, et al. Study on Experimental Parameters of Induction Smelting of Sm-Fe Alloy[J]. Rare Metals and Cemented Carbides, 2020(2): 35-40. |
| MLA | [1] LIU Kun, et al., "Study on Experimental Parameters of Induction Smelting of Sm-Fe Alloy." Rare Metals and Cemented Carbides, no. 2, 2020, pp. 35-40. |
| APA | [1] LIU Kun, WANG Shu-huan, ZHANG Yi-kun, & LI Bo-hai. (2020). Study on Experimental Parameters of Induction Smelting of Sm-Fe Alloy. Rare Metals and Cemented Carbides(2), 35-40. |
| IEEE | [1] LIU Kun, WANG Shu-huan, ZHANG Yi-kun, and LI Bo-hai, "Study on Experimental Parameters of Induction Smelting of Sm-Fe Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 35-40, 2020. keywords: {Sm-Fe alloy;induction smelting;smelting pressure;smelting time;Sm volatilization;Sm content;microstructure} |