Research Status and Prospect of Sm2Fe17N3 Permanent Magnetic Material AITranslate
Abstract AITranslate
Lattice structure and intrinsic magnetic property principle of Sm2Fe17N3 interstitial compound are briefly analyzed.The current preparation methods of Sm2Fe17N3 permanent magnetic material and the influence of element addition on its magnetic properties are mainly introduced.Besides,the preparation status of Sm2Fe17N3/α-Fe dual-phase nanocomposites is reviewed.Finally,the existing problems in preparation process and development tendency of Sm2Fe17N3 permanent magnetic material are summarized and prospected.
KeyWords AITranslate
1李芳,刘颖,杨锦,李军,高升吉,涂铭旌.HDDR法制备各向同性SmFeN永磁体的研究[J].稀土,2005,26(2):22-25. 被引量:2
2倪建森,徐晖,朱明原,李强,周邦新,董远达.双相纳米晶永磁体的研究[J].中国稀土学报,2002,20(3):215-218. 被引量:16
3Guiyong Wu,Hongwei Li,Dunbo Yu,Kuoshe Li,Wenlong Yan,Chao Yuan,Liang Sun,Yang Luo,Kun Zhang.Effect of niobium substitution on microstructures and thermal stability of TbCu7-type Sm-Fe-N magnets[J].稀土学报:英文版,2018,36(3):281-286. 被引量:2
4林国标,王显荣,于一公,尹有祥,于申军,周寿增.低温氢处理对制取Sm_2Fe_(17)N_x的作用[J].有色金属:冶炼部分,1996(1):48-48. 被引量:4
5郝延明,安立群,谭明,谈清华,王玲玲,严达利.Sm2Fe17化合物的差热-热重分析[J].稀有金属,2009(1):76-79. 被引量:5
6叶金文,刘颖,张然,陈梅,朱国丽,高升吉,涂铭旌.各向同性Sm_2Fe_(17)N_x磁粉及其粘结磁体的制备[J].稀有金属材料与工程,2007,36(2):329-331. 被引量:5
7徐送宁,孙树滋,史维东,马腾才.Sm─FeCo─N合金薄膜的磁性与微观结构[J].东北大学学报:自然科学版,1996,17(5):538-540. 被引量:1
8金延,晓敏.磁性薄膜[J].金属功能材料,2003,10(5):46-47. 被引量:3
9邓庚凤,何桂荣,邓华军,黄崛起.还原扩散法制备钐铁氮磁性材料的组织结构与性能研究[J].中国稀土学报,2010,28(6):676-679. 被引量:5
10金延.磁记录材料的发展[J].金属功能材料,2002,9(3):40-41. 被引量:3
1李青华,刘冬,胡国辉,贾立颖,王倩,李志宏,刘荣明,李炳山.Sm_(2)Fe_(17)N_(x)永磁材料矫顽力机理探究及影响因素分析[J].矿冶,2022,31(1):85-90.
2李迎畅,俞能君,泮敏翔,杨杭福,吴琼,颜冲,葛洪良.SmFe_(12)基永磁合金研究进展[J].磁性材料及器件,2022,53(6):111-117.
1周春隆.酞菁颜料结晶形态与调整技术(续)[J].染料与染色,2020,57(2):1-9.
2王兴悦,张辉,阮子林,郝振亮,杨孝天,蔡金明,卢建臣.超高真空条件下分子束外延生长的单层二维原子晶体材料的研究进展[J].物理学报,2020,69(11):284-307. 被引量:4
3云璐,郝新.Ti对Fe-B-C-Ti系堆焊层组织及耐磨性的影响[J].焊接技术,2020,49(4):5-8. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.45[金属学及工艺—金属材料]
Citation Information:
Lattice structure and intrinsic magnetic property principle of Sm2Fe17N3 interstitial compound are briefly analyzed.The current preparation methods of Sm2Fe17N3 permanent magnetic material and the influence of element addition on its magnetic properties are mainly introduced.Besides,the preparation status of Sm2Fe17N3/α-Fe dual-phase nanocomposites is reviewed.Finally,the existing problems in preparation process and development tendency of Sm2Fe17N3 permanent magnetic material are summarized and prospected.
quote
| GB/T 7714-2015 | [1] ZHANG Yi-kun, WANG Shu-huan, FENG Yun-li, et al. Research Status and Prospect of Sm2Fe17N3 Permanent Magnetic Material[J]. Rare Metals and Cemented Carbides, 2020(2): 41-46. |
| MLA | [1] ZHANG Yi-kun, et al., "Research Status and Prospect of Sm2Fe17N3 Permanent Magnetic Material." Rare Metals and Cemented Carbides, no. 2, 2020, pp. 41-46. |
| APA | [1] ZHANG Yi-kun, WANG Shu-huan, FENG Yun-li, & LIU Kun. (2020). Research Status and Prospect of Sm2Fe17N3 Permanent Magnetic Material. Rare Metals and Cemented Carbides(2), 41-46. |
| IEEE | [1] ZHANG Yi-kun, WANG Shu-huan, FENG Yun-li, and LIU Kun, "Research Status and Prospect of Sm2Fe17N3 Permanent Magnetic Material," Rare Metals and Cemented Carbides, no. 2, pp. 41-46, 2020. keywords: {permanent magnetic material;Sm2Fe17N3;preparation method;element addition;research status;development tendency} |