Study on Controllable Preparation of Porous Network TiO2 Flexible Electrode AITranslate
Abstract AITranslate
TiO2 flexible electrode materials were prepared by hydrothermal adjustment of NaOH concentration,hydrothermal reaction time and reaction temperature.The optimal conditions of hydrothermal synthesis are NaOH solution concentration of 0.5 mol/L,reaction temperature of 200 ℃,and reaction time of 16 h.TiO2 prepared under the conditions has a porous network structure,which can enhance the electrolyte infiltration,shorten the Li+ diffusion path,and accelerate the transport of lithium ions and electrons.Constant current charging performance test results show that TiO2 with porous network structure has good cycle stability.The reversible capacity is 112 mA·h/g and the capacity retention rate is 67.8% after 50 cycles at the current density of 800 mA/g.The TiO2 also has an excellent rate performance.When the current density is as high as 1 600 mA/g,the reversible capacity can still be maintained at 103.4 mA·h/g.
KeyWords AITranslate
1苏源,黄伟,耿嘉阳,徐磊.二氧化钛纳米材料的研究与应用[J].黑龙江科学,2019,10(2):42-43. 被引量:4
1吴凤燕.MOFs及其衍生物的制备及电化学性能研究进展[J].云南化工,2020,47(5):18-19.
2李靓晗,简现龙,张森,张明,孙玉平,王新昌.柔性、自支撑CNT/Si复合薄膜的制备及储能性能[J].化工学报,2020,71(6):2804-2810. 被引量:2
3吴亚梅.智能手环与手机是恒压或恒流充电吗[J].物理通报,2020,49(6):109-112.
4勾剑,王雨霄,张洪章,谭业强,于滢,曲超,阎景旺,张华民,李先锋.3D金属绣花电极:下一代柔性、个性化的储能设备的理想电极[J].科学通报:英文版,2020,65(11):917-925. 被引量:1
5张鸣,王国志,沙卫华,刘波,陈立义.α-ω全氟聚醚二元醇的制备研究[J].现代涂料与涂装,2020,23(5):15-17.
6王赫,秦楠,郭鑫,郑俊生,赵基钢.锂离子电容器硬碳负极材料的表面改性及其电化学性能研究[J].化工学报,2020,71(6):2735-2742. 被引量:3
7韩丹丹,申烨,潘怡帆,赵远,魏金鹤.棉布的功能化及在柔性电极中的应用[J].化学研究与应用,2020,32(5):725-731. 被引量:1
8马香钰,夏广波,邱琳琳,董丽卡,丁明乐,杜平凡.纤维及织物基柔性可穿戴器件研究进展[J].材料导报,2020,34(S01):490-497. 被引量:4
9安玉良,任玉杰,闫杭亮,马腾飞,袁霞.四氧化三铁/石墨烯复合锂离子电池负极材料制备及性能研究[J].化学与粘合,2020,42(3):159-161. 被引量:2
10肖利娜,张乐平,刘小娜,果岩,牛小利,白丹阳.一种新型多酸超分子化合物的水热合成与结构表征[J].郑州师范教育,2019,0(6):18-21.
Basic Information:
DOI:
Chinese Library Classification Number:TM914.42[电气工程—电力电子与电力传动]
Citation Information:
TiO2 flexible electrode materials were prepared by hydrothermal adjustment of NaOH concentration,hydrothermal reaction time and reaction temperature.The optimal conditions of hydrothermal synthesis are NaOH solution concentration of 0.5 mol/L,reaction temperature of 200 ℃,and reaction time of 16 h.TiO2 prepared under the conditions has a porous network structure,which can enhance the electrolyte infiltration,shorten the Li+ diffusion path,and accelerate the transport of lithium ions and electrons.Constant current charging performance test results show that TiO2 with porous network structure has good cycle stability.The reversible capacity is 112 mA·h/g and the capacity retention rate is 67.8% after 50 cycles at the current density of 800 mA/g.The TiO2 also has an excellent rate performance.When the current density is as high as 1 600 mA/g,the reversible capacity can still be maintained at 103.4 mA·h/g.
quote
| GB/T 7714-2015 | [1] FENG Qian, DONG Peng, ZHANG Ying-jie, et al. Study on Controllable Preparation of Porous Network TiO2 Flexible Electrode[J]. Rare Metals and Cemented Carbides, 2020(2): 47-52. |
| MLA | [1] FENG Qian, et al., "Study on Controllable Preparation of Porous Network TiO2 Flexible Electrode." Rare Metals and Cemented Carbides, no. 2, 2020, pp. 47-52. |
| APA | [1] FENG Qian, DONG Peng, ZHANG Ying-jie, & LI Xue. (2020). Study on Controllable Preparation of Porous Network TiO2 Flexible Electrode. Rare Metals and Cemented Carbides(2), 47-52. |
| IEEE | [1] FENG Qian, DONG Peng, ZHANG Ying-jie, and LI Xue, "Study on Controllable Preparation of Porous Network TiO2 Flexible Electrode," Rare Metals and Cemented Carbides, no. 2, pp. 47-52, 2020. keywords: {porous network structure;TiO2;Li-ion battery;hydrothermal method;electrochemical property} |