Effect of Ru on Microstructure and Properties of Ti(C,N)-based Cermets AITranslate
Abstract AITranslate
Ti(C5N5),Mo2C,Ru and Ni powders were mixed,and then Ti(C,N)-based cermets were prepared by powder metallurgy.The effects of Ru on microstructure and properties of Ti(C,N)-based cermets were studied as well as the mechanism.The results show that the Ti(C,N)-based cermets doped with Ru exhibit a core-ring structure.With the increase of Ru content,the main grains are refined,and the binder phase tends to be uniform.The change in Ru content has an effect on the concentration gradient of the binder phase in Ti(C,N)-based cermets.The thickness of the gradient layer increases at first and then decreases as the Ru content increases.Ti(C,N)-based cermet with 1.5% Ru has fracture toughness of 9.9 MPa·m1/2 and Vickers hardness of 1 500 HV10.Ru doping greatly improves the comprehensive mechanical properties of Ti(C,N)-based cermets,due to strengthening of the binder phase.
KeyWords AITranslate
1吕学鹏,郑勇,吴鹏.碳纳米管添加量对Ti(C,N)基金属陶瓷组织和力学性能的影响[J].中国有色金属学报,2011,21(1):145-151. 被引量:11
2刘爱军,刘宁.金属陶瓷颗粒尺寸与WC含量对双结构Ti(C,N)基金属陶瓷组织和性能的影响(英文)[J].稀有金属材料与工程,2019,48(2):375-384. 被引量:5
3姜佳庚,周书助,谭璟颢,田智豪,颜练武,彭英彪,伍小波.(Ti,La)(C,N)基金属陶瓷复合材料制备及性能研究[J].硬质合金,2019,36(2):109-115. 被引量:3
4刘爱军,刘宁,张宏亮,石俊.Ti(C,N)-xWC-Ni-Mo-C金属陶瓷组织的研究[J].稀有金属与硬质合金,2015,43(4):34-37 46. 被引量:1
5孙万昌,张佩,李攀,佘晓林,魏汉军,赵坤,张峰.烧结工艺和Y_2O_3添加量对Ti(C,N)基金属陶瓷显微组织和力学性能的影响[J].中国有色金属学报,2015,25(5):1277-1284. 被引量:6
6唐思文,刘德顺,李鹏南,唐文波,唐德.TiCN基梯度功能金属陶瓷的制备及其切削性能[J].功能材料,2014,45(13):13126-13130. 被引量:10
7刘宁,崔昆.Ti(C,N)基金属陶瓷的性能与发展[J].合肥工业大学学报:自然科学版,2000,23(1):1-5. 被引量:9
8时凯华,昝秀颀,杨新宇,董凯林,顾金宝,曾伟.含钌WC-Co硬质合金研究现状及展望[J].硬质合金,2018,35(5):315-323. 被引量:4
9朱刚,谢明,刘颖,陈家林,李再久,杨有才.Fe添加量对Ti(C,N)基金属陶瓷显微组织及力学性能的影响[J].稀有金属与硬质合金,2016,44(2):30-34. 被引量:7
1岳洋,杜勇,吕健,刘宜强,谭凯铭,李亚军,王忠华.Ti(C,N)-TaC-Ni金属陶瓷真空烧结过程的微观结构演变与性能的研究[J].硬质合金,2022,39(1):1-11.
1汪志兵,张振玉.环状RNA在胃癌中的功能研究及潜在应用价值[J].胃肠病学和肝病学杂志,2020,29(5):481-484. 被引量:1
2罗婧.从团结型社会组织、行政型社会组织到治理型社会组织——1949年以来社会组织的变迁历史[J].清华大学学报:哲学社会科学版,2020,35(3):191-206. 被引量:12
3杨勇,冯和平,王琪,陈瑞润,郭景杰,丁宏升,苏彦庆.添加Fe元素改善TiAl-Nb合金的显微组织和力学性能[J].中国有色金属学报:英文版,2020,30(5):1315-1324. 被引量:3
4杨丽,赵岗,樊秀梅,吴玲玲,田淑卿.基于Nrf2/HO-1通路研究芹菜素改善妊娠期糖尿病大鼠氧化应激损伤[J].中国医药导报,2020,17(13):27-31. 被引量:14
5丁建,陆勇俊,曹鑫磊,尚帅朋,王霞,王峰会.连续梯度阳极功能层的引入对阳极支撑固体氧化物燃料电池的力学性能影响[J].陶瓷学报,2019,40(5):583-588.
6杨振,柳宁,樊湘芳,李勇,邱长军.2Cr12NiMoWV钢表面激光熔覆铁基合金组织及力学性能研究[J].应用激光,2020,40(1):22-28. 被引量:13
7陈巧旺,邓莹,姜山,姜中涛,敬小龙,陈慧,李力.表层富立方相WC-TiC-Co功能梯度硬质合金[J].粉末冶金技术,2020,38(1):36-41. 被引量:3
8范小明,陈希奎,汪子涵,曹帅,程凤如,杨则恒,张卫新.自牺牲模板法制备氮掺杂碳化钼/碳析氢电催化剂[J].化工学报,2020,71(6):2840-2849. 被引量:1
9梁金禄.一种天然气管道内防腐涂料的制备及性能研究[J].粘接,2020,42(4):1-4. 被引量:3
10叶小丹,林军,陈剑,苏林红,柳侠平,朱小区.基于HIF-1α/PPARγ研究荷叶颗粒对非酒精性脂肪肝大鼠脂代谢及SREBP-1c表达的影响[J].重庆医学,2020,49(10):1575-1579. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:TG148[金属学及工艺—金属材料]
Citation Information:
Ti(C5N5),Mo2C,Ru and Ni powders were mixed,and then Ti(C,N)-based cermets were prepared by powder metallurgy.The effects of Ru on microstructure and properties of Ti(C,N)-based cermets were studied as well as the mechanism.The results show that the Ti(C,N)-based cermets doped with Ru exhibit a core-ring structure.With the increase of Ru content,the main grains are refined,and the binder phase tends to be uniform.The change in Ru content has an effect on the concentration gradient of the binder phase in Ti(C,N)-based cermets.The thickness of the gradient layer increases at first and then decreases as the Ru content increases.Ti(C,N)-based cermet with 1.5% Ru has fracture toughness of 9.9 MPa·m1/2 and Vickers hardness of 1 500 HV10.Ru doping greatly improves the comprehensive mechanical properties of Ti(C,N)-based cermets,due to strengthening of the binder phase.
quote
| GB/T 7714-2015 | [1] TAN Kai-ming, DU Yong, LV Jian, et al. Effect of Ru on Microstructure and Properties of Ti(C,N)-based Cermets[J]. Rare Metals and Cemented Carbides, 2020(2): 53-56. |
| MLA | [1] TAN Kai-ming, et al., "Effect of Ru on Microstructure and Properties of Ti(C,N)-based Cermets." Rare Metals and Cemented Carbides, no. 2, 2020, pp. 53-56. |
| APA | [1] TAN Kai-ming, DU Yong, LV Jian, LIN Fu-ping, & YANG Yu-long. (2020). Effect of Ru on Microstructure and Properties of Ti(C,N)-based Cermets. Rare Metals and Cemented Carbides(2), 53-56. |
| IEEE | [1] TAN Kai-ming, DU Yong, LV Jian, LIN Fu-ping, and YANG Yu-long, "Effect of Ru on Microstructure and Properties of Ti(C,N)-based Cermets," Rare Metals and Cemented Carbides, no. 2, pp. 53-56, 2020. keywords: {Ti(C,N)-based cermet;ruthenium;toughening;solid solution strengthening;fracture toughness;Vickers hardness;concentration gradient} |