daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Status and Prospect of Toughening Methods of Ti(C,N)-based Cermets AITranslate

College of Mechanical Engineering,Sichuan University of Science and Engineering;College of Mechanical Engineering,Sichuan University of Science and Engineering;College of Mechanical Engineering,Sichuan University of Science and Engineering;College of Mechanical Engineering,Sichuan University of Science and Engineering;College of Mechanical Engineering,Sichuan University of Science and Engineering
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The recent research progress of the methods such as self-toughening,particle toughening and whisker toughening adopted to improve the toughness of Ti(C,N)-based cermets and their comprehensive properties is reviewed.The related toughening mechanism is expounded,and the problems existing in toughening technologies of cermet materials and their future development directions are briefly described.

KeyWords AITranslate

Ti(C N)-based cermet fracture toughness toughening method toughening mechanism research progress

1潘传增,赵忠民,张龙,张靖.超重力场反应加工自增韧(Ti,W)C-TiB_2凝固陶瓷刀具材料研究[J].稀有金属材料与工程,2013,42(S1):358-362. 被引量:2

2倪秀英,赵军,孙加林,李洪江,侯冠明,田源.梯度结构Al_2O_3-(W,Ti)C-TiN-Mo-Ni纳米金属陶瓷刀具材料的设计及制备[J].材料工程,2018,46(2):50-56. 被引量:4

3孟祥龙,肖光春,王兴海,许崇海.热压工艺对Ti(C,N)基纳米复合金属陶瓷模具材料力学性能与微观结构的影响[J].人工晶体学报,2015,44(6):1668-1674. 被引量:5

4周曦亚,方培育.自增韧陶瓷复合材料的研究[J].中国陶瓷,2003,39(6):30-32. 被引量:15

5谭锦颢,周书助,朱磊,胡倞,罗成.NbC含量对Ti(C,N)基金属陶瓷组织和力学性能的影响[J].硬质合金,2010,27(2):78-82. 被引量:10

6刘爱军,刘宁.金属陶瓷颗粒尺寸与WC含量对双结构Ti(C,N)基金属陶瓷组织和性能的影响(英文)[J].稀有金属材料与工程,2019,48(2):375-384. 被引量:5

7邓建新,李兆前,艾兴.晶须增韧陶瓷基复合材料的进展[J].材料导报,1994(5):72-75. 被引量:13

8瞿峻,熊惟皓,刘文俊,叶大萌.SiC晶须改性金属陶瓷断裂韧性及增韧机理[J].华中科技大学学报:自然科学版,2010,38(3):25-28. 被引量:11

9胡巍巍,李冠晓,刘宁,徐伟,汪金文.球磨工艺对Ti(C,N)基金属陶瓷组织和性能的影响[J].硬质合金,2010,27(6):358-364. 被引量:4

10王守文,郑勇,丁伟民,邵想,张梦迪,朱杏根.Ti(C,N)固溶体的N/C原子比对Ti(C,N)基金属陶瓷组织及力学性能的影响[J].硬质合金,2018,35(2):79-85. 被引量:7

1黄梓键,罗展鹏,张展,张岩,郭伟明,林华泰.Ni-Mo黏结剂含量对放电等离子烧结TiC_(0.7)N_(0.3)基金属陶瓷力学性能的影响[J].机械工程材料,2022,46(8):105-108.

2张广森,季文彬,戴士杰,武星辰.微波烧结Ti(C,N)-WC-Al_(2)O_(3)/Ti(C,N)-WC叠层陶瓷的微观结构和力学性能[J].硅酸盐学报,2022,50(12):3212-3221.

3杨雄,于新,彭欣,左锐,林孝良,高荣根.基于正交试验和BP神经网络的Ti(C,N)基金属陶瓷成分及性能研究[J].硬质合金,2023,40(1):50-58.

1赵鸣,姜曌,陈华,张志远,李保卫.玻璃陶瓷增韧研究进展[J].中国陶瓷,2020,56(4):1-6. 被引量:3

2袁智慧,牛永平,汪小伟,杜三明.环氧树脂增韧机理及研究进展[J].热固性树脂,2019,34(6):65-70. 被引量:8

3李沛欣,袁凌,潘磊,刘伟超,周文明,闫文娟.MW级风电叶片用环氧类结构胶的研究进展[J].中国胶粘剂,2020,29(4):57-65. 被引量:1

4高磊,李慧芸.基于选择性激光改性的双陶瓷层热障涂层界面增韧方法[J].红外与激光工程,2020,49(1):171-178.

5崔文博.环氧树脂增韧固化剂的合成与性能研究[J].化工管理,2019(36):114-115. 被引量:4

6廖依敏,陈明辉,王福会,朱圣龙.自修复金属搪瓷高温防护涂层[J].表面技术,2020,49(1):25-34. 被引量:5

7董慧民,闫丽,安学锋,钱黄海,苏正涛,益小苏.ESTM-fabric/3266复合材料低速冲击响应及冲击后压缩行为研究[J].材料工程,2020,48(1):41-47. 被引量:3

8马新伟,夏佳军,郑泽鹏,侯岷杰.四元镁质胶凝材料增强与增韧机理研究[J].沈阳建筑大学学报:自然科学版,2020,36(1):116-123.

Basic Information:

DOI:

Chinese Library Classification Number:TG148[金属学及工艺—金属材料]

Citation Information:

The recent research progress of the methods such as self-toughening,particle toughening and whisker toughening adopted to improve the toughness of Ti(C,N)-based cermets and their comprehensive properties is reviewed.The related toughening mechanism is expounded,and the problems existing in toughening technologies of cermet materials and their future development directions are briefly described.

quote

GB/T 7714-2015 [1] DONG Ding-qian, YANG Wei, SHI Kai-hua, et al. Research Status and Prospect of Toughening Methods of Ti(C,N)-based Cermets[J]. Rare Metals and Cemented Carbides, 2020(2): 57-62.
MLA [1] DONG Ding-qian, et al., "Research Status and Prospect of Toughening Methods of Ti(C,N)-based Cermets." Rare Metals and Cemented Carbides, no. 2, 2020, pp. 57-62.
APA [1] DONG Ding-qian, YANG Wei, SHI Kai-hua, LIAO Jun, & ZHANG Li. (2020). Research Status and Prospect of Toughening Methods of Ti(C,N)-based Cermets. Rare Metals and Cemented Carbides(2), 57-62.
IEEE [1] DONG Ding-qian, YANG Wei, SHI Kai-hua, LIAO Jun, and ZHANG Li, "Research Status and Prospect of Toughening Methods of Ti(C,N)-based Cermets," Rare Metals and Cemented Carbides, no. 2, pp. 57-62, 2020. keywords: {Ti(C,N)-based cermet;fracture toughness;toughening method;toughening mechanism;research progress}