The latest Development of Ti-containing Catalysts AITranslate

Beijing Normal University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With review of the role of Ti-containing catalysts in the modern catalytical industry and its impetus to the development of modern industry,the paper briefly describes the latest development of Ti- containing catalysts.The paper also introduces the related new achievements made by Chinese catalyst researchers and related literatures and references.

KeyWords AITranslate

Ti-containing catalysts photocatalysis modern chemical industry

1苏文悦,付贤智,魏可镁.SO_4^(2_)表面修饰对TiO_2结构及其光催化性能的影响[J].物理化学学报,2001,17(1):28-31. 被引量:79

2高远,徐安武,祝静艳,刘汉钦.RE/TiO_2用于NO_2^-光催化氧化的研究[J].催化学报(英文),2001,22(1):53-56. 被引量:92

3李芳柏,古国榜,李新军,万洪富.WO_3/TiO_2纳米材料的制备及光催化性能[J].物理化学学报,2000,16(11):997-1002. 被引量:96

4颜秀茹,李晓红,霍明亮,郭伟巍,巩永进.纳米SnO_2@TiO_2的制备及其光催化性能[J].物理化学学报,2001,17(1):23-27. 被引量:31

5张玉红,熊国兴,杨维慎,傅贤智.溶胶-凝胶法制备复合M_xO_(y-)TiO_2光催化剂[J].物理化学学报,2001,17(3):273-277. 被引量:30

6王娅娟,李斌,魏培海,张延昌,冯绪胜,杨孔章.溶胶-凝胶法制备TiO_2/玻璃膜和光催化降解玫瑰红B的研究[J].应用化学,2001,18(1):36-39. 被引量:29

7成英之,张渊明,唐渝.WO_3-TiO_2薄膜型复合光催化剂的制备和性能[J].催化学报(英文),2001,22(2):203-205. 被引量:87

8余家国,赵修建,陈文梅,林立,张艾丽.TiO_2/SiO_2纳米薄膜的光催化活性和亲水性[J].物理化学学报,2001,17(3):261-264. 被引量:29

9崔玉民,单德杰,朱亦仁.TiO_2薄膜光催化氧化I^-的研究[J].无机化学学报,2001,17(3):401-406. 被引量:22

10朱宁,b唐涛,陈辉,于广谦,冯之榴,黄葆同.有机/无机纳米杂化材料载体化钛催化剂的聚合研究 Ⅱ.间同聚苯乙烯制备[J].应用化学,2001,18(1):9-11. 被引量:1

1新型高分子合成压敏胶粘剂[J].化工文摘,2001(4):56-56.

2唐晓东,诸林.论化工专业《工业催化〉课程设置[J].石油高等教育,2000(2):81-83.

3用于苯酚氧化的高效Ti/分子筛催化剂[J].石油化工,2008,37(6):644-644.

4倪天民.用高活性含钛催化剂制备PET[J].聚酯工业,2005,18(4):62-63.

5吴燕妮,崔秀兰,刘双平,郭海福.稀土催化剂的应用[J].内蒙古石油化工,2002,28(3):68-71. 被引量:3

6姜鸿基,李彦锋,叶正芳,彭嘉选.纳米TiO_2光催化剂的制备及在降解有机物方面的研究进展[J].功能材料,2002,33(4):360-362. 被引量:30

7国外高分子合成与加工应用[J].国内外石油化工快报,2003(11):24-28.

8倪天民.用高活性含钛催化剂生产PET的方法[J].聚酯工业,2005,18(4):63-63.

9关于举行浙江省粘接技术协会成立30周年庆典暨粘接材料技术创新与行业发展论坛的通知[J].中国胶粘剂,2015,24(5):44-44.

10杨志兰,刘桂艳.三层法FCCL用合成树脂粘合剂的研究进展[J].武汉生物工程学院学报,2006,0(2):107-110. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TQ426[化学工程]

Citation Information:

With review of the role of Ti-containing catalysts in the modern catalytical industry and its impetus to the development of modern industry,the paper briefly describes the latest development of Ti- containing catalysts.The paper also introduces the related new achievements made by Chinese catalyst researchers and related literatures and references.

quote

GB/T 7714-2015 [1] ZHANG Wen-pu. The latest Development of Ti-containing Catalysts[J]. Rare Metals and Cemented Carbides, 2001(4): 39-41.
MLA [1] ZHANG Wen-pu. "The latest Development of Ti-containing Catalysts." Rare Metals and Cemented Carbides, no. 4, 2001, pp. 39-41.
APA [1] ZHANG Wen-pu. (2001). The latest Development of Ti-containing Catalysts. Rare Metals and Cemented Carbides(4), 39-41.
IEEE [1] ZHANG Wen-pu, "The latest Development of Ti-containing Catalysts," Rare Metals and Cemented Carbides, no. 4, pp. 39-41, 2001. keywords: {Ti-containing catalysts;photocatalysis;modern chemical industry}