The Market,Production,Price and Development of Gallium AITranslate

central south university
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The applications,market,production,price and development of gallium were reviewed.The production of metal gallium in Russia and Khasakstan is described.

KeyWords AITranslate

gallium application market production price

1铃木康生.ガリウム[J].工业レアソタル,2000,(116):24.[ZK)

2胜野泰光.化合物半体と结晶材料GaAs,GaP,InP[J].工业レアソタル,2000,(116):21-21.

3SKVORTSOV A YU,et al.Method for Extraction of Gal lium from AlkaliAluminium-Containing Solutions[P].Russian Patent:2049824,1995-12-10.

4SKVORTSOV A YU,et al.Method for Combined Process ing of Gallium-ContainingAluminate Solutions[P].Russian Patent:2049825,199 5-12-10.

5SKVORTSOV A YU,et al.Method of Gallium Extraction from A lkalineSolutions[P].Russian Patent:2051113,1995-12-27.

6LAHIRI S,et al.Gallium Recovery-technological Alt ernatives[J].Bulletin ofElectrochemistry,1996,12(5~6):342.

1王新萍,曾德启.平果铝土矿伴生镓的综合利用前景[J].轻金属,2012(6):6-8. 被引量:1

2黄中省.富镓物中镓的浸出、分离试验研究[J].稀有金属与硬质合金,2016,44(4):5-10. 被引量:2

3赵汀,秦鹏珍,王安建,王高尚,李建武,刘超,刘毅飞.镓矿资源需求趋势分析与中国镓产业发展思考[J].地球学报,2017,38(1):77-84. 被引量:22

4陈浩林,谢克强,黄海艺,纪文涛.水浸法富集黄磷电尘灰中镓的预处理研究[J].昆明理工大学学报:自然科学版,2020,45(2):9-15. 被引量:1

5陈浩林,谢克强,张燕,梁可,杨坤,高亮,符德正.Ga_(2)O_(3)真空碳热还原实验研究[J].真空科学与技术学报,2023,43(1):60-65.

6苏毅,李国斌,罗康碧.金属镓提取研究进展[J].湿法冶金,2003,22(1):9-13. 被引量:12

7Paraffin wax as a diluent for extraction and separation of trivalent gallium, indium, and thallium with 2,6-bis-(l'-phenyl-3'-methyl-5'-oxopyrazole-4') pyridineacyl[J].稀有金属:英文版,2003,22(2):86-90. 被引量:1

8苏毅,李国斌,罗康碧,毕莉.高纯金属镓制备技术研究进展[J].稀有金属,2003,27(4):495-499. 被引量:15

1黄靖,王英滨,周冠轩,马真乾.混合酸溶-电感耦合等离子体发射光谱法测定粉煤灰样品中的微量元素镓[J].环境化学,2020(5):1427-1433. 被引量:2

2彭波,俞洁,高锦章.4-(2-吡啶偶氮)间苯二酚光度法测定Ga^(3+)、In^(3+)的研究[J].西北师范大学学报:自然科学版,2005,41(1):51-54. 被引量:1

3熊利芝,何则强,刘文萍,麻成金,戴永年.Preparation of high-purity bismuth by sulphur deleadization in vacuum distillation[J].中国有色金属学会会刊:英文版,2004,14(6):1210-1214. 被引量:5

4何则强,肖卓炳,熊利芝,麻成金,刘文萍,戴永年.精铋的真空蒸馏硫化除铅[J].真空科学与技术学报,2006,26(1):32-35. 被引量:12

5颜秀文,丘泰,张振忠,李晓云.Ga-Ag-Sn液态合金与Cu的结合界面分析[J].稀有金属,2006,30(3):310-312. 被引量:1

6佘旭.高纯镓电解精炼的研究[J].稀有金属,2007,31(6):871-874. 被引量:2

7邢学永,李斯加.金属钒的制备研究进展[J].四川有色金属,2009(1):11-14. 被引量:7

8熊利芝,戴永年,尹周澜,陈启元.真空蒸馏加剂除铅制备高纯铋[J].吉首大学学报:自然科学版,2009,30(3):95-101. 被引量:4

9吴恩辉,杨绍利.从攀枝花钒钛磁铁矿中回收镓的研究进展[J].中国有色冶金,2010,39(1):45-47. 被引量:8

10李海涛,曲文卿,庄鸿寿.真空电子器件用Ga基堵漏钎料的研究[J].真空电子技术,2011,24(3):55-58. 被引量:1

1简讯[J].中国金属通报,1999,0(29):15-15.

2仇振琢,翟凤丽.各国金属镓品质浅析[J].有色金属:冶炼部分,1989(1):43-45.

3谭军.三门峡铝业高科技项目——金属镓近日成功下线[J].功能材料信息,2009(4):37-37.

4韩杰华,高贵超.强化金属镓生产提高企业综合经济效益[J].轻金属,1999(8):12-14. 被引量:11

5三门峡铝业高科技项目金属镓成功下线[J].中国金属通报,2009(21):6-6.

6潘雄.我国拟计划将稀有金属镓铟纳入收储范围[J].功能材料信息,2009(2):46-47.

7孔祥海,胡瑛.持续发展招招领先——中铝山东分公司发展循环经济纪实[J].中国有色金属,2008(6):52-53.

8张建.镓价狂飙缘为何[J].中国金属通报,2001,0(14):6-7.

9邵志博.中国氧化铝工业的发展方向[J].世界有色金属,1999(3):8-12. 被引量:12

10江涛宏.2006年上半年锗、铟、镓市场简评[J].中国金属通报,2006,0(21):15-16.

Basic Information:

DOI:

Chinese Library Classification Number:F407.3[经济管理—产业经济];TG146.431[金属学及工艺—金属材料]

Citation Information:

The applications,market,production,price and development of gallium were reviewed.The production of metal gallium in Russia and Khasakstan is described.

quote

GB/T 7714-2015 [1] ZHAO Qin-sheng. The Market,Production,Price and Development of Gallium[J]. Rare Metals and Cemented Carbides, 2001(4): 42-44.
MLA [1] ZHAO Qin-sheng. "The Market,Production,Price and Development of Gallium." Rare Metals and Cemented Carbides, no. 4, 2001, pp. 42-44.
APA [1] ZHAO Qin-sheng. (2001). The Market,Production,Price and Development of Gallium. Rare Metals and Cemented Carbides(4), 42-44.
IEEE [1] ZHAO Qin-sheng, "The Market,Production,Price and Development of Gallium," Rare Metals and Cemented Carbides, no. 4, pp. 42-44, 2001. keywords: {gallium;application,market;production;price}