Production,Properties and Applications of Low-cost Titanium Powder Products AITranslate
Abstract AITranslate
This paper describes the production,properties,and applications of a new high-quality powder produced from titanium dioxde by metal hydride reduction.The powder contains no residual chloride,as is suitable for corrosion-proof medical and other applications.
KeyWords AITranslate
1FROES F H,et al.Metal Handbook:Production of Titanium Powder(Vol7)[M].OH:ASM Metals Park,1993.164.
2FROES F H,et al.Powder Metallurgy of Titanium All oys[J].International Material Reviews,1990,35:162.
3CARLSON H A,et al.Method for Electrolyging Water with Dual Directional Membrane[P].US Patent:5296109,1994-02-22.
4MOXSON V,et al.Production,Characterigation and Ap plications of Low Cost Titanium Powder Products,Non-Aerospuce Applications of T ita nium[M].Warrendale,Pennsylvania,TMS,1998.127.
1徐宝强,戴永年,宋宁,杨斌.海绵钛制备方法的研究现状[J].材料导报,2004,18(7):52-54. 被引量:11
2洪艳,曲涛,沈化森,王兆林,车小奎.氢化脱氢法制备钛粉工艺研究[J].稀有金属,2007,31(3):311-315. 被引量:23
3洪艳,沈化森,曲涛,胡永海,车小奎.钛冶金工艺研究进展[J].稀有金属,2007,31(5):694-700. 被引量:9
4黄光明,雷霆,方树铭,李红梅.氢化脱氢制备钛粉的研究进展[J].钛工业进展,2010,27(6):6-9. 被引量:8
5万贺利,徐宝强,杨斌,刘大春,戴永年.真空钙热还原法制备金属钛粉的研究[J].真空科学与技术学报,2012,32(6):539-544. 被引量:9
6冯虎成,刘松利.金属钛制备方法的研究进展及趋势[J].攀枝花学院学报,2013,30(1):108-110. 被引量:3
7邹黎明,谢焕文,刘辛,王蕾,蔡一湘.钛及钛合金粉末制备技术的研究及应用现状[J].材料研究与应用,2015,9(4):222-225. 被引量:5
1刘畅,李慧,张汉鑫,梁精龙.钛粉制备工艺的研究进展及发展趋势[J].稀有金属与硬质合金,2020(1):35-39. 被引量:2
2闫洪.2004年云南金属材料与加工年评[J].云南冶金,2005,34(2):40-49.
3方树铭,雷霆,朱从杰,周林.海绵钛生产工艺和技术方案的选择及分析[J].轻金属,2007(4):43-49. 被引量:13
4陈晋,张世敏,彭金辉,陈菓,黄孟阳,雷鹰.微波加热在钛冶金中的应用[J].钢铁钒钛,2008,29(3):68-72. 被引量:13
5闫丽静.钛制备方法研究现状[J].中国西部科技,2008,7(32):35-36. 被引量:4
6孙莹,王宁,袁继维,田元江,李惠文.海绵钛生产中铜丝除钒废弃物的回收实验与分析[J].矿物学报,2009,29(1):124-128. 被引量:3
7宋建勋,徐宝强,杨斌,林大志.镁热还原法制取金属钛的实验研究[J].轻金属,2009(12):43-48. 被引量:11
8杨明,杨钢,唐仁杰,张玲.海绵钛生产技术进展[J].云南冶金,2010,39(1):45-49. 被引量:8
9刘毅,金志浩.Ti_2AlN可加工陶瓷的快速制备及压痕行为研究[J].西安交通大学学报,2011,45(10):104-108. 被引量:2
10李开华.镁热法生产海绵钛技术发展现状[J].材料导报:纳米与新材料专辑,2011,25(2):225-228. 被引量:14
1吴引江.低成本粉末钛及其合金的发展[J].钛工业进展,1998,15(6):10-11. 被引量:4
2Bonfe,L,徐万仁.西德玛高炉的高质量低成本铁水炉料结构[J].世界钢铁,1999(3):34-38. 被引量:2
3曹太平.最先进的低成本炼钢法(摘译)[J].太钢译文,1997(2):24-28.
4白丙中.高质量保护渣与连铸机多炉连浇[J].首钢科技,1990(5):22-25.
5兰涛.粉末冶金钛材的新发展[J].钛工业进展,1989(3):26-27.
6贾翃.我国钛粉末及其制品的生产与应用概况[J].钛工业进展,1998,15(2):1-4. 被引量:4
7张小明.钛粉末注射成形的开发[J].钛工业进展,1990(4):6-7.
8王长华.残留有色金属杂质对结构钢性能的影响[J].冶金译丛,1997(3):65-67.
9Froes,FH,黎刚蕊.低成本钛粉的生产[J].轻金属,1999(6):46-49. 被引量:3
10张国才.连续气相还原生产钛粉末[J].钛合金信息,2000(1):5-7. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF123.23[冶金工程—粉末冶金]
Citation Information:
This paper describes the production,properties,and applications of a new high-quality powder produced from titanium dioxde by metal hydride reduction.The powder contains no residual chloride,as is suitable for corrosion-proof medical and other applications.
quote
| GB/T 7714-2015 | [1] HUANG Jin-chang. Production,Properties and Applications of Low-cost Titanium Powder Products[J]. Rare Metals and Cemented Carbides, 2001(4): 45-48. |
| MLA | [1] HUANG Jin-chang. "Production,Properties and Applications of Low-cost Titanium Powder Products." Rare Metals and Cemented Carbides, no. 4, 2001, pp. 45-48. |
| APA | [1] HUANG Jin-chang. (2001). Production,Properties and Applications of Low-cost Titanium Powder Products. Rare Metals and Cemented Carbides(4), 45-48. |
| IEEE | [1] HUANG Jin-chang, "Production,Properties and Applications of Low-cost Titanium Powder Products," Rare Metals and Cemented Carbides, no. 4, pp. 45-48, 2001. keywords: {titanium;powder;production;property;application} |