Ti-Based Gilding Materials and Its Latest Development AITranslate

Department of Metallurgical Science and Engineering, Central South University;Department of Metallurgical Science and Engineering, Central South University;Department of Metallurgical Science and Engineering, Central South University;Department of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Brief description is made of the application and properties of various gilding materials.Emphasizes are put on the basic information and achievement in the deveopment of TiN-based gilding materials,the synthesis of new gilding material-TiO powder and latest development of TiO-based PM gilding materials.

KeyWords AITranslate

gilding material titanium nitride TiO

1马光.提高仿金饰品材料性能的几个途径[J].稀有金属材料与工程,1989(5):74-76. 被引量:3

2唐多光,周自强,葛建生,陆庆桃.抗变色仿金合金的研究[J].金属科学与工艺,1991,10(1):77-82. 被引量:18

3VERSHINA A K,et.al.Structure and Decorative Prope rties of TiO Coatings Depositedfrom Separated Low Temperature Plasma Fluxes[J ].Fiz Khim Obrab Mater,1996,(5):45.

4YOSHIO,et al.Decorative Golden Sintered Alloy [P]US Pat 4589917,1986-05-20.

5YOSHIO,et al.Sintered Alloy of Golden Color[P].EP P at 0520465,1992-11-30.

1艾小玲.仿金材料的熔铸技术[J].武汉汽车工业大学学报,1999,21(2):40-42.

2薛涛.仿金材料的熔铸[J].五金科技,1992(3):15-15.

3董玉祥,张金龙.仿金材料防腐蚀和抗变色钝化工艺[J].上海工业大学学报,1991,12(6):557-559.

4李庆奎,赵红亮,钟晖,钟海云.一氧化钛基金属陶瓷仿金材料的制备及性能研究[J].稀有金属,2005,29(3):279-284. 被引量:1

5许贤超,雷广孝.铜基稀土仿金材料的研究及应用[J].四川有色金属,1992(3):22-25. 被引量:2

6李庆奎,石广新,钟晖,钟海云.非化学计量一氧化钛的颜色研究[J].稀有金属,2005,29(2):187-190. 被引量:1

7万传庚,Krits.,P.高温钎料PdCu-Ti在氧化铝陶瓷上的润湿性及界面反应[J].焊接学报,1994,15(4):209-213. 被引量:20

8王碧文,王涛.仿金材料及焊接工艺研究[J].有色金属:冶炼部分,2000(1):34-38.

9沈燕,陆原,罗海燕,丘俊强,韦天元.高抗变色铜基仿金合金的研究[J].广西大学学报:自然科学版,1995,20(2):134-138. 被引量:3

10汤孝平,曹玉民,李庆奎,钟海云.一氧化钛基金属陶瓷粘结相的研究[J].稀有金属与硬质合金,2002,30(1):9-12. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]

Citation Information:

Brief description is made of the application and properties of various gilding materials.Emphasizes are put on the basic information and achievement in the deveopment of TiN-based gilding materials,the synthesis of new gilding material-TiO powder and latest development of TiO-based PM gilding materials.

quote

GB/T 7714-2015 [1] LI Qing-kui, ZHONG Hai-yun, LI Jian, et al. Ti-Based Gilding Materials and Its Latest Development[J]. Rare Metals and Cemented Carbides, 2001(4): 36-38.
MLA [1] LI Qing-kui, et al., "Ti-Based Gilding Materials and Its Latest Development." Rare Metals and Cemented Carbides, no. 4, 2001, pp. 36-38.
APA [1] LI Qing-kui, ZHONG Hai-yun, LI Jian, & DAI Yan-yang. (2001). Ti-Based Gilding Materials and Its Latest Development. Rare Metals and Cemented Carbides(4), 36-38.
IEEE [1] LI Qing-kui, ZHONG Hai-yun, LI Jian, and DAI Yan-yang, "Ti-Based Gilding Materials and Its Latest Development," Rare Metals and Cemented Carbides, no. 4, pp. 36-38, 2001. keywords: {gilding material;titanium nitride;TiO}