Research on Effects of Tempering Process on Microstructure and Corrosion Resistance of AlFeCrCoCu High-entropy Alloy AITranslate
Abstract AITranslate
The microstructure was studied of AlFeCrCoCu high-entropy alloy prepared by vacuum arc melting.Effects were investigated of tempering process on alloy microstructure,hardness and corrosion resistance in 3.5% NaCl solution.The results show that the alloy has dendrite microstructure,the dendrite is Al,Fe,Cr,Co-rich BCC phase and intergranular microstructure is Cu-rich FCC phase.Alloy melting point is about 1 380 ℃,and intergranular Cu-rich phase begins phase transition at about 1 050 ℃.With the increase of tempering temperature,the grains begin to grow up until develop into coarse grains at about 1 000℃.The alloy exhibits a superior resistance to temper softening.Electrochemical test results show that the alloy has better corrosion resistance than 304 stainless steel,and 800 ℃ temper microstructure has the highest corrosion resistance.
KeyWords AITranslate
1Jien-Wei Yeh.Alloy Design Strategies and Future Trends in High-Entropy Alloys[J]. JOM . 2013 (12)
2Xing-Wu Qiu,Yun-Peng Zhang,Li He,Chun-ge Liu.Microstructure and corrosion resistance of AlCrFeCuCo high entropy alloy[J]. Journal of Alloys and Compounds . 2013
3任明星,李邦盛,傅恒志.固溶体型高熵合金的形成条件(英文)[J].中国有色金属学报:英文版,2013,23(4):991-995. 被引量:21
4Y. Zhang,X. Yang,P. Liaw.Alloy Design and Properties Optimization of High-Entropy Alloys[J]. JOM . 2012 (7)
5C.P. Lee,Y.Y. Chen,C.Y. Hsu,J.W. Yeh,H.C. Shih.Enhancing pitting corrosion resistance of Al x CrFe 1.5 MnNi 0.5 high-entropy alloys by anodic treatment in sulfuric acid[J]. Thin Solid Films . 2008 (3)
6Yuan-Sheng Huang,Ling Chen,Hong-Wei Lui,Ming-Hong Cai,Jien-Wei Yeh.Microstructure, hardness, resistivity and thermal stability of sputtered oxide films of AlCoCrCu 0.5 NiFe high-entropy alloy[J]. Materials Science & Engineering A . 2006 (1)
7Jien-Min Wu,Su-Jien Lin,Jien-Wei Yeh,Swe-Kai Chen,Yuan-Sheng Huang,Hung-Cheng Chen.Adhesive wear behavior of Al x CoCrCuFeNi high-entropy alloys as a function of aluminum content[J]. Wear . 2005 (5)
8Akihisa Inoue.Stabilization of metallic supercooled liquid and bulk amorphous alloys[J]. Acta Materialia . 2000 (1)
9Revie R,Winston U.Corrosion handbook. . 2005
1崔普昌,张益铭,傅生,栾添,农智升.热处理对AlCrFeNiTi高熵合金组织和硬度的影响[J].稀有金属与硬质合金,2017,45(1):52-57. 被引量:3
2王志新,周家臣,马明星,卢金斌,朱达川,张德良.退火对AlCoCrFeMnTi高熵合金相组成与显微形貌的影响[J].金属热处理,2020,45(4):144-148. 被引量:9
3赵路路,林乃明,邹娇娟,谢瑞珍,袁烁.高熵合金的耐蚀性与耐磨性研究进展[J].热加工工艺,2020,49(6):1-7. 被引量:4
4李承泽,尤俊华,白鹤山,张维维,刘苏杰.高熵合金的热处理综述[J].材料热处理学报,2020,41(5):1-12. 被引量:7
5蔡志海,GUO Yu,柳建,LIU Jun,GUO Jie,DU Xian,HUANG Shaofu.Progress in Light-weight High Entropy Alloys[J].武汉理工大学学报:材料科学英文版,2021,36(5):737-753. 被引量:2
6李美艳,张琪,韩彬,王稼林.多主元高熵合金组织性能及塑性变形的研究进展[J].材料热处理学报,2019,40(1):1-8. 被引量:4
1崔小杰,苏新磊,刘岩,李月,赵定国,王书桓,张鹏杰.气雾化工艺对高熵合金粉体粒径的影响[J].特种铸造及有色合金,2022,42(4):441-445. 被引量:1
2王逸飞,张艳,王振旭,陈景润,陈德旭,张静,杨诗雨.热处理对氮间隙固溶CoCrFeMnNi高熵合金组织及性能的影响[J].特种铸造及有色合金,2022,42(1):55-59.
3贾彦军.多主元高熵合金组织性能及塑性变形分析[J].科技视界,2019,0(22):52-53.
4张雷,陈红梅,陶小马,欧阳义芳.Al基五元高熵合金的热力学研究[J].中国有色金属学报,2019,29(11):2601-2608. 被引量:3
5彭勇,雷卫宁,张扬,张文杰,邓瑶,李小平.电弧熔敷用高熵合金粉芯丝材熔敷层的摩擦磨损行为[J].电焊机,2020,50(1):34-41. 被引量:2
6张骁,刘亮,商剑,赵作福,张越,齐锦刚,王冰.热处理对双FCC相CoCrFeNiCu高熵合金组织与性能的影响[J].金属热处理,2021,46(2):157-160. 被引量:4
7徐洪洋,孟雯露,卢金斌,马明星.基于第一性原理的CrCuFeNiTi高熵合金涂层的相及稳定性分析[J].金属热处理,2021,46(7):60-64. 被引量:3
8全韬,郭伟波,钱铖.粉末冶金Al_(1)Co_(25)Cr_(18)Fe_(23)Ni_(23)Ta_(10)共晶高熵合金摩擦磨损性能研究[J].硬质合金,2021,38(3):156-164.
9陈明宣,马强,孟君晟,李成硕,史晓萍.高熵合金涂层的研究进展[J].金属热处理,2021,46(9):7-14. 被引量:4
10张微,刘亮,商剑,赵作福,张越,齐锦刚,王冰.磁控溅射AlCrFeNiTi高熵合金薄膜的组织和表面形貌[J].电镀与涂饰,2021,40(19):1489-1493. 被引量:3
1刘亮,张越,赵作福,商剑.热处理对CoCrFeNiMo高熵合金组织与硬度的影响[J].金属热处理,2016,41(8):29-32. 被引量:11
2罗晓艳,刘贵仲,吴鹏,钟文华.多主元AlFeCoNiCrV合金退火状态下硬度及电化学性能的研究[J].材料导报:纳米与新材料专辑,2010,24(2):546-548.
3孙日伟,张伟强,付华萌.固态渗铝对AlCoCrFeNi高熵合金组织的影响[J].金属热处理,2015,40(9):160-163. 被引量:8
4唐群华,程虎,戴品强.轧制及退火后Al_(0.3)CoCrFeNi高熵合金的组织和力学性能[J].材料热处理学报,2015,36(12):72-77. 被引量:5
5罗晓艳,刘贵仲,高原.多主元AlFeCoNiCrTiV_(0.5)高熵合金退火态的硬度及电化学性能[J].机械工程材料,2011,35(4):87-90. 被引量:5
6徐文臣,黄凯,武世峰,宗影影,单德彬.Mo含量对含β相TiAl合金组织和力学性能的影响(英文)[J].中国有色金属学报:英文版,2017,27(4):820-828. 被引量:4
7黄照军,程晓农,顾冬青,赵国平,李孟伟.Cu-Zn-Sn-Mn低熔点合金的设计[J].铸造,2010,59(12):1349-1351.
8管彦朋,李亚江,王娟.1000 MPa及以上级高强钢焊接性研究现状[J].机械制造文摘:焊接分册,2015(3):30-34. 被引量:5
9吕雪飞,甘树坤.化学处理液中的La及BTA对铜合金表面性能的影响[J].表面技术,2012,41(5):70-72. 被引量:3
10谢红波,刘贵仲,郭景杰.Mn、V、Mo、Ti、Zr元素对AlFeCrCoCu-X高熵合金组织与高温氧化性能的影响[J].中国有色金属学报,2015,25(1):103-110. 被引量:28
Basic Information:
DOI:
Chinese Library Classification Number:TG156.5[金属学及工艺—热处理]
Citation Information:
The microstructure was studied of AlFeCrCoCu high-entropy alloy prepared by vacuum arc melting.Effects were investigated of tempering process on alloy microstructure,hardness and corrosion resistance in 3.5% NaCl solution.The results show that the alloy has dendrite microstructure,the dendrite is Al,Fe,Cr,Co-rich BCC phase and intergranular microstructure is Cu-rich FCC phase.Alloy melting point is about 1 380 ℃,and intergranular Cu-rich phase begins phase transition at about 1 050 ℃.With the increase of tempering temperature,the grains begin to grow up until develop into coarse grains at about 1 000℃.The alloy exhibits a superior resistance to temper softening.Electrochemical test results show that the alloy has better corrosion resistance than 304 stainless steel,and 800 ℃ temper microstructure has the highest corrosion resistance.
quote
| GB/T 7714-2015 | [1] XIE Hong-bo, LIU Gui-zhong, GUO Jing-jie, et al. Research on Effects of Tempering Process on Microstructure and Corrosion Resistance of AlFeCrCoCu High-entropy Alloy[J]. Rare Metals and Cemented Carbides, 2015(4): 51-56. |
| MLA | [1] XIE Hong-bo, et al., "Research on Effects of Tempering Process on Microstructure and Corrosion Resistance of AlFeCrCoCu High-entropy Alloy." Rare Metals and Cemented Carbides, no. 4, 2015, pp. 51-56. |
| APA | [1] XIE Hong-bo, LIU Gui-zhong, GUO Jing-jie, MAO Wei-qian, & HAO Cong-min. (2015). Research on Effects of Tempering Process on Microstructure and Corrosion Resistance of AlFeCrCoCu High-entropy Alloy. Rare Metals and Cemented Carbides(4), 51-56. |
| IEEE | [1] XIE Hong-bo, LIU Gui-zhong, GUO Jing-jie, MAO Wei-qian, and HAO Cong-min, "Research on Effects of Tempering Process on Microstructure and Corrosion Resistance of AlFeCrCoCu High-entropy Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 51-56, 2015. keywords: {AlFeCrCoCu high-entropy alloy;tempering process;microstructure;hardness;corrosion resistance} |