Effects of Electroless Nickel Plating on Electrochemical Properties of AB_3-typed Hydrogen Storage Alloy AITranslate
Abstract AITranslate
AB3-typed hydrogen storage alloy(Mm0.78Mg0.22Ni2.48 Mn0.09Al0.23Co0.47,Mm=82.3%La+17.7%Nd)was modified by electroless nickel plating to improve its electrochemical and kinetic properties.Alloy phase composition was analyzed by XRD,and the results show that the phase composition of the alloy has no change after electroless nickel plating.Electrochemical test results show that the alloy electrode has significantly increased discharge specific capacity after electroless nickel plating with the maximum327.7mA·h/g,and its cycle stability is also greatly improved with increased capacity retention rate from original 83.3% to 93.3% after 50charge/discharge cycles.Electroless nickel plating can improve alloy electrochemical properties,and thereby exchange current density i0,limiting current density iL,corrosion potential Ecorrand electrochemical reactivity of the alloy electrode are significantly improved.
KeyWords AITranslate
1K. Young,D.F. Wong,S. Yasuoka,J. Ishida,J. Nei,J. Koch.Different failure modes for V-containing and V-free AB 2 metal hydride alloys[J]. Journal of Power Sources . 2014
2Weiqing Jiang,Changsheng Qin,Rongrong Zhu,Jin Guo.Annealing effect on hydrogen storage property of Co-free La 1.8 Ti 0.2 MgNi 8.7 Al 0.3 alloy[J]. Journal of Alloys and Compounds . 2013
3Xianyun Peng,Baozhong Liu,Yanping Fan,Xilin Zhu,Qiuming Peng,Zhi Zhang.Microstructures and electrochemical hydrogen storage characteristics of La 0.7 Ce 0.3 Ni 4.2 Mn 0.9? x Cu 0.37 (Fe 0.43 B 0.57 ) x ( x = 0–0.20) alloys[J]. Journal of Power Sources . 2013
4Yanping Fan,Baozhong Liu,Baoqing Zhang,Liqiang Ji,Yongguang Wang,Zhi Zhang.Microstructures and electrochemical properties of LaNi 3.55 Co 0.2? x Mn 0.35 Al 0.15 Cu 0.75 (Fe 0.43 B 0.57 ) x ( x = 0–0.20) hydrogen storage alloys[J]. Materials Chemistry and Physics . 2013 (2-3)
5Xianyun Peng,Baozhong Liu,Yanping Fan,Liqiang Ji,Baoqing Zhang,Zhi Zhang.Microstructures and electrochemical characteristics of La 0.7 Ce 0.3 Ni 4.2 Mn 0.9? x Cu 0.37 (V 0.81 Fe 0.19 ) x hydrogen storage alloys[J]. Electrochimica Acta . 2013
6Pawel Slepski,Kazimierz Darowicki,Ewa Janicka,Agnieszka Sierczynska.Application of electrochemical impedance spectroscopy to monitoring discharging process of nickel/metal hydride battery[J]. Journal of Power Sources . 2013
7Weiqing Jiang,Xiaohua Mo,Jin Guo,Yinyan Wei.Effect of annealing on the structure and electrochemical properties of La 1.8 Ti 0.2 MgNi 8.9 Al 0.1 hydrogen storage alloy[J]. Journal of Power Sources . 2013
8Chenxi Jiang,Haiyan Wang,Yazhi Wang,Xiangrong Chen,Yougen Tang,Zuming Liu,Hualin Xie.Enhanced electrochemical performance of Mg 2 Ni alloy prepared by rapid quenching in magnetic field[J]. Journal of Power Sources . 2013
9Wenzhuo Shen,Shumin Han,Yuan Li,Jing Yang,Kun Xiao.Electrochemical performance of polyaniline electroless deposited La–Mg–Ni-based hydrogen storage alloys[J]. Materials Chemistry and Physics . 2011 (2-3)
10Sheng-Han Lin,Wu-Tsan Wu,Jing-Shan Do.High-rate discharge characteristics of metal hydride modified by electroless nickel plating based on experimental design approach[J]. International Journal of Hydrogen Energy . 2011 (3)
1周楠,丁毅,马立群,董振伟.镁对La_(1-x)Mg_xNi_(2.5)Co_(0.5)(x=0~0.4)合金循环过程中电化学性能的影响[J].中国稀土学报,2012,30(3):380-384.
2李国辉,黄红霞,王新颖,谢文强.聚苯胺对La_(0.94)Mg_(0.06)Ni_(3.49)Co_(0.73)Mn_(0.12)Al_(0.20)储氢合金电化学性能的影响[J].稀有金属与硬质合金,2016,44(6):44-48.
3一种对AB_3型储氢合金进行表面改性的方法[J].金属功能材料,2014,21(2):40-40.
4王姗姗,韩选利,张良,钟吕玲,李斌强.LaMg_2Ni_(2.7)Co_(2.1)Mn_(2.7)Cu_(1.5)滴涂TiO_2复合电极的制备及电化学性能[J].稀有金属材料与工程,2016,45(4):1008-1011. 被引量:1
5刘智雄,唐欣,朱铁夫,田美云,肖李宝.GH4169的钎焊性改进研究[J].热加工工艺,2014,43(19):184-185. 被引量:2
6李国辉,黄红霞,王新颖,李银.AB_3型Mm_(0.78)Mg_(0.22)Ni_(2.48)Mn_(0.09)Al_(0.23)Co_(0.47)储氢合金的表面氟化处理[J].表面技术,2014,43(5):76-80. 被引量:1
7王新颖,黄红霞,李国辉,谢文强.浅议储氢合金的研究现状及发展[J].稀有金属与硬质合金,2015,43(5):39-43. 被引量:3
8樊星,韩选利,齐白羽.AB_3型LaMg_2Ni_(9-x-y-z)Co_xMn_yCu_z储氢合金的制备及电化学性能研究[J].稀有金属材料与工程,2011,40(6):1025-1028. 被引量:2
9樊星,韩选利,齐白羽.化学法制备LaMg_2Ni_(9-x-y-z)Co_xMn_yCu_z系列储氢合金及电化学性能研究[J].化学工程与装备,2010(1):18-21. 被引量:2
10贺忠臣,丁毅,秦铁男,马立群,袁亮.热处理温度与6063铝合金化学镀镍层的耐蚀性[J].腐蚀与防护,2010,31(3):231-233. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:TG139.7[一般工业技术—材料科学与工程]
Citation Information:
AB3-typed hydrogen storage alloy(Mm0.78Mg0.22Ni2.48 Mn0.09Al0.23Co0.47,Mm=82.3%La+17.7%Nd)was modified by electroless nickel plating to improve its electrochemical and kinetic properties.Alloy phase composition was analyzed by XRD,and the results show that the phase composition of the alloy has no change after electroless nickel plating.Electrochemical test results show that the alloy electrode has significantly increased discharge specific capacity after electroless nickel plating with the maximum327.7mA·h/g,and its cycle stability is also greatly improved with increased capacity retention rate from original 83.3% to 93.3% after 50charge/discharge cycles.Electroless nickel plating can improve alloy electrochemical properties,and thereby exchange current density i0,limiting current density iL,corrosion potential Ecorrand electrochemical reactivity of the alloy electrode are significantly improved.
quote
| GB/T 7714-2015 | [1] LI Guo-hui, HUANG Hong-xia, WANG Xin-ying, et al. Effects of Electroless Nickel Plating on Electrochemical Properties of AB_3-typed Hydrogen Storage Alloy[J]. Rare Metals and Cemented Carbides, 2015(4): 57-61 71. |
| MLA | [1] LI Guo-hui, et al., "Effects of Electroless Nickel Plating on Electrochemical Properties of AB_3-typed Hydrogen Storage Alloy." Rare Metals and Cemented Carbides, no. 4, 2015, pp. 57-61 71. |
| APA | [1] LI Guo-hui, HUANG Hong-xia, WANG Xin-ying, & XIE Wen-qiang. (2015). Effects of Electroless Nickel Plating on Electrochemical Properties of AB_3-typed Hydrogen Storage Alloy. Rare Metals and Cemented Carbides(4), 57-61 71. |
| IEEE | [1] LI Guo-hui, HUANG Hong-xia, WANG Xin-ying, and XIE Wen-qiang, "Effects of Electroless Nickel Plating on Electrochemical Properties of AB_3-typed Hydrogen Storage Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 57-61 71, 2015. keywords: {AB3-typed hydrogen storage alloy;electroless nickel plating;surface modification;electrochemical property} |