Study on Selective Reduction of Nitrogen Oxides on AgO/Al_2O_3 Catalyst AITranslate

School of Chemistry and Materials Science, Liaoning University of Petroleum and Chemical Technology;School of Chemistry and Materials Science, Liaoning University of Petroleum and Chemical Technology;School of Chemistry and Materials Science, Liaoning University of Petroleum and Chemical Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Selective reduction was studied of nitrogen oxides on AgO/Al2O3 catalyst prepared by impregnation and hydrothermal coprecipitation.The results show that preparation methods of the catalyst play an important role in its catalytic effect.Prepared by hydrothermal coprecipitation,AgO/Al2O3 catalyst is more active than that by impregnation.The catalyst systems with different reducing agents have different reduction performance.AgO/Al2O3 catalyst prepared by hydrothermal coprecipitation has better water and sulfur resistance and high selective reduction activity due to strong interaction between AgO and high specific surface area Al2O3.Oxygen adsorbed on the catalyst surface greatly promotes selective oxidation of nitrogen oxides.

KeyWords AITranslate

AgO/Al2O3 catalyst impregnation hydrothermal coprecipitation selective reduction nitrogen oxide

1E.F. Iliopoulou,A.P. Evdou,A.A. Lemonidou,I.A. Vasalos.Ag/alumina catalysts for the selective catalytic reduction of NO x using various reductants[J]. Applied Catalysis A, General . 2004 (1)

2Junhua Li,Jiming Hao,Lixin Fu,Zhiming Liu,Xiangyu Cui.The activity and characterization of sol–gel Sn/Al 2 O 3 catalyst for selective catalytic reduction of NO x in the presence of oxygen[J]. Catalysis Today . 2004 (3)

3Hong He,Changbin Zhang,Yunbo Yu.A comparative study of Ag/Al 2 O 3 and Cu/Al 2 O 3 catalysts for the selective catalytic reduction of NO by C 3 H 6[J]. Catalysis Today . 2004 (3)

4Zhiming Liu,Jiming Hao,Lixin Fu,Tianle Zhu,Junhua Li,Xiangyu Cui.Promoting effect of sol-gel method and pre-treatment on the activity of SnO2/Al2O3 catalyst for NO reduction by propene[J]. Reaction Kinetics and Catalysis Letters . 2003 (1)

5Masaaki Haneda,Yoshiaki Kintaichi,Hideaki Hamada.Effect of SO 2 on the catalytic activity of Ga 2 O 3 –Al 2 O 3 for the selective reduction of NO with propene in the presence of oxygen[J]. Applied Catalysis B, Environmental . 2001 (4)

6Masaaki Haneda,Yoshiaki Kintaichi,Hiromichi Shimada,Hideaki Hamada.Selective Reduction of NO with Propene over Ga 2 O 3 –Al 2 O 3 : Effect of Sol–Gel Method on the Catalytic Performance[J]. Journal of Catalysis . 2000 (1)

7Erol Seker,John Cavataio,Erdogan Gulari,Paisan Lorpongpaiboon,Somchai Osuwan.Nitric oxide reduction by propene over silver/alumina and silver–gold/alumina catalysts: effect of preparation methods[J]. Applied Catalysis A, General . 1999 (1)

8Laiyuan Chen,Tatsuro Horiuchi,Toshihiko Osaki,Toshiaki Mori.Catalytic selective reduction of NO with propylene over Cu-Al 2 O 3 catalysts: influence of catalyst preparation method[J]. Applied Catalysis B, Environmental . 1999 (4)

9Masaaki Haneda,Yoshiaki Kintaichi,Hideaki Hamada.Promotional effect of H 2 O on the activity of In 2 O 3 ‐doped Ga 2 O 3 –Al 2 O 3 for the selective reduction of nitrogen monoxide[J]. Catalysis Letters . 1998 (1)

10Held W,Konig A,Thomas R,et al.Catalytic NOx reduction in net oxidizing exhaust gas. SAE Transactions . 1990

1齐延,邱爽,张志刚,郭耘,卢冠忠,郭杨龙.尿素基水热共沉淀法铈锆固溶体的制备及应用[J].中国稀土学报,2005,23(S1):51-54. 被引量:8

2黄亚丽.关于实验室法制氧气的催化剂选择[J].三明学院学报,2000,18(S4):77-78.

3沈建忠,池毓习,罗文英,曹运连,官丽华,邹明旺,周文富.TiCl_3在乙酸异戊酯合成中的催化研究[J].三明学院学报,1998,16(2):47-50.

4杨洪,宁黔冀,赵海涛.均匀共沉淀-水热法制备纤维状羟基磷酸钙/壳聚糖复合粉体[J].化学研究与应用,2005,17(2):186-189. 被引量:4

5郭海福,秦海莉,樊宏伟,崔秀兰,林明丽,成大农,赵薇.尼泊金酯的合成及催化剂选择[J].精细石油化工,1999,16(1):34-37. 被引量:42

6谢婷,陈文华,李智利.含氟吡咯-硫脲有机催化剂促进硫醚的选择性氧化过程[J].化学试剂,2013,35(3):264-266.

7王文南,陈继东,张曼征.液相法催化加氢制邻氨基酚的研究[J].湖北化工,1996,13(2):12-13. 被引量:2

8赵俊凤,孙小丽,李吉来,黄旭日.铂钌团簇活化甲醇C―H和O―H键的理论研究[J].物理化学学报,2015,31(6):1077-1085. 被引量:2

9刘双培,郭栋才,梅焕谋.烷基糖苷的制备和应用[J].湖南化工,1997,27(3):4-7. 被引量:13

10郭海福,赵薇.对羟基苯甲酸丁酯的合成及催化剂选择[J].内蒙古工学院学报,1993,12(4):66-71. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:O643.36[理学—物理化学]

Citation Information:

Selective reduction was studied of nitrogen oxides on AgO/Al2O3 catalyst prepared by impregnation and hydrothermal coprecipitation.The results show that preparation methods of the catalyst play an important role in its catalytic effect.Prepared by hydrothermal coprecipitation,AgO/Al2O3 catalyst is more active than that by impregnation.The catalyst systems with different reducing agents have different reduction performance.AgO/Al2O3 catalyst prepared by hydrothermal coprecipitation has better water and sulfur resistance and high selective reduction activity due to strong interaction between AgO and high specific surface area Al2O3.Oxygen adsorbed on the catalyst surface greatly promotes selective oxidation of nitrogen oxides.

quote

GB/T 7714-2015 [1] XU Zhen-chong, WU Shuang, ZHOU Ming-dong. Study on Selective Reduction of Nitrogen Oxides on AgO/Al_2O_3 Catalyst[J]. Rare Metals and Cemented Carbides, 2015(4): 62-66 74.
MLA [1] XU Zhen-chong, et al., "Study on Selective Reduction of Nitrogen Oxides on AgO/Al_2O_3 Catalyst." Rare Metals and Cemented Carbides, no. 4, 2015, pp. 62-66 74.
APA [1] XU Zhen-chong, WU Shuang, & ZHOU Ming-dong. (2015). Study on Selective Reduction of Nitrogen Oxides on AgO/Al_2O_3 Catalyst. Rare Metals and Cemented Carbides(4), 62-66 74.
IEEE [1] XU Zhen-chong, WU Shuang, and ZHOU Ming-dong, "Study on Selective Reduction of Nitrogen Oxides on AgO/Al_2O_3 Catalyst," Rare Metals and Cemented Carbides, no. 4, pp. 62-66 74, 2015. keywords: {AgO/Al2O3 catalyst;impregnation;hydrothermal coprecipitation;selective reduction;nitrogen oxide}