Research on Effects of Deformation Methods on Density and Reinforcement Mechanism of Molybdenum Powders AITranslate

College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The molybdenum powders were put into the tube and heated to 500℃,and then two pass A-route equal channel angular pressing(ECAP)or hot pressing experiments were carried out.Particle morphology,pore distribution and microhardness were compared of the molybdenum powders from different pressing methods.The results show that after two pass ECAP,pore distribution of the sample is more uniform,and both particle deformation degree and microhardness are higher.After hot pressing,pore distribution of the sample is nonuniform,its density at the upper end is higher than that at the down end,and its particle deformation degree is small.During hot pressing,pressing force cannot result in brittle fracture of the particles,so the sample has lower microhardness than the sample processed by equal channel angular pressing.

KeyWords AITranslate

molybdenum powder equal channel angular pressing density pore microhardness

1陈振华,陈鼎,编著.现代粉末冶金原理[M]. 化学工业出版社, 2012

2Thermal stability of ultrafine grains size of pure copper obtained by equal-channel angular pressing[J]. Journal of Materials Science . 2010 (9)

3Ruslan Z. Valiev,Terence G. Langdon.Principles of equal-channel angular pressing as a processing tool for grain refinement[J]. Progress in Materials Science . 2006 (7)

4M. Haouaoui,I. Karaman,K. T. Harwig,H. J. Maier.Microstructure evolution and mechanical behavior of bulk copper obtained by consolidation of micro- and nanopowders using equal-channel angular extrusion[J]. Metallurgical and Materials Transactions A . 2004 (9)

5Valiev RZ,Enikeev NA,Langdon TG.Towards superstrength of nanostructured metals and alloys produced by SPD. Metallic Materials . 2011

1安耿,周莎,张晓,席莎,刘仁智.钼管材制备技术及应用研究进展[J].中国钼业,2021,45(6):7-11.

1唐长国,陈文涛,朱金华.钨合金高应变率导致的塑性降低及微观机理[J].西安交通大学学报,1997,31(3):28-32. 被引量:6

2仝健民,李继红,王春.静态、铝热自蔓延高温合成(SHS)陶瓷涂层的组织结构研究[J].表面工程,1996(1):20-23. 被引量:9

3欧阳鸿武,何世文,刘咏,韦嘉.装粉方式对钛粉压制成形影响的数值模拟[J].粉末冶金材料科学与工程,2004,9(3):184-191. 被引量:1

4欧阳鸿武,何世文,韦嘉,刘咏.装粉方式对钛粉压制成形影响的数值模拟[J].中国有色金属学报,2004,14(8):1318-1323. 被引量:3

5李威威,左孝青,董晓蓉,杨皓.多孔NiTi形状记忆合金的制备工艺[J].热加工工艺,2016,45(8):58-62. 被引量:3

6马旭梁,李莉,朱成武,王香,郑玉峰.多孔NiTi形状记忆合金的制备及性能[J].材料工程,2011,39(3):6-10. 被引量:7

7丁锐,李相波,王佳,许立坤.冷喷涂Cu-Cu_2O涂层微观结构与沉积特性[J].真空科学与技术学报,2013,33(6):586-592. 被引量:3

8谷曼,焦明华,孙龙,吴玉程.不同压制工艺下的粉末颗粒变形三维细观模拟研究[J].热加工工艺,2015,44(5):125-128. 被引量:2

9刘咏,黄伯云,贺跃辉,王彬.热压反应合成 TiAl 合金的密度及孔隙分布[J].中南工业大学学报,1998,29(5):446-449. 被引量:10

10焦彤,张宝■,张海涛,刘长林.90W和93W钨合金动加载下微(细)观响应分析[J].中国有色金属学报,2001,11(z1):92-97. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG379[金属学及工艺—金属压力加工]

Citation Information:

The molybdenum powders were put into the tube and heated to 500℃,and then two pass A-route equal channel angular pressing(ECAP)or hot pressing experiments were carried out.Particle morphology,pore distribution and microhardness were compared of the molybdenum powders from different pressing methods.The results show that after two pass ECAP,pore distribution of the sample is more uniform,and both particle deformation degree and microhardness are higher.After hot pressing,pore distribution of the sample is nonuniform,its density at the upper end is higher than that at the down end,and its particle deformation degree is small.During hot pressing,pressing force cannot result in brittle fracture of the particles,so the sample has lower microhardness than the sample processed by equal channel angular pressing.

quote

GB/T 7714-2015 [1] SONG Qun-chao, LI Ping, WANG Xue, et al. Research on Effects of Deformation Methods on Density and Reinforcement Mechanism of Molybdenum Powders[J]. Rare Metals and Cemented Carbides, 2015(4): 47-50.
MLA [1] SONG Qun-chao, et al., "Research on Effects of Deformation Methods on Density and Reinforcement Mechanism of Molybdenum Powders." Rare Metals and Cemented Carbides, no. 4, 2015, pp. 47-50.
APA [1] SONG Qun-chao, LI Ping, WANG Xue, HUA Rui, & XUE Ke-min. (2015). Research on Effects of Deformation Methods on Density and Reinforcement Mechanism of Molybdenum Powders. Rare Metals and Cemented Carbides(4), 47-50.
IEEE [1] SONG Qun-chao, LI Ping, WANG Xue, HUA Rui, and XUE Ke-min, "Research on Effects of Deformation Methods on Density and Reinforcement Mechanism of Molybdenum Powders," Rare Metals and Cemented Carbides, no. 4, pp. 47-50, 2015. keywords: {molybdenum powder;equal channel angular pressing;density;pore;microhardness}