Research on Self-propagation High-temperature Synthesis of Ti_2SnC Material AITranslate

College of Materials and Chemical of Central Plains Institute of Technology;College of Materials and Chemical of Central Plains Institute of Technology;College of Materials and Chemical of Central Plains Institute of Technology;College of Materials and Chemical of Central Plains Institute of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The Ti2 SnC material was prepared by self-propagation high-temperature synthesis(SHS)with2Ti/Sn/C and Ti/Sn/TiC as the raw materials.Effects of the two raw materials on Ti2SnC synthesis were investigated.The results show that with the two raw materials,Ti2 SnC can be synthesized by SHS,and the products contain a small amount of TiC and Sn.With 2Ti/Sn/C as the raw powder material,the synthesized Ti2 SnC has well-developed lath grains of about 10μm length and about 2μm width.With Ti/Sn/TiC as the raw material,the synthesized Ti2 SnC has fine granular grains of about 1~5μm granularity.

KeyWords AITranslate

Ti2SnC self-propagation high-temperature synthesis microstructure reaction mechanism

1Fanai Meng,Baoyan Liang,Mingzhi Wang.Investigation of formation mechanism of Ti 3 SiC 2 by self-propagating high-temperature synthesis[J]. International Journal of Refractory Metals and Hard Materials . 2013

2Shi-Bo Li,Guo-Ping Bei,Hong-Xiang Zhai,Yang Zhou,Cui-Wei Li.Synthesis of Ti 2 SnC at low-temperature using mechanically activated sintering process[J]. Materials Science & Engineering A . 2007 (1)

3J.Y. Wu,Y.C. Zhou,J.Y. Wang.Tribological behavior of Ti 2 SnC particulate reinforced copper matrix composites[J]. Materials Science & Engineering A . 2006 (1)

4Guanghua Liu,Kexin Chen,Heping Zhou,Junming Guo,Kegang Ren,J.M.F. Ferreira.Layered growth of Ti 2 AlC and Ti 3 AlC 2 in combustion synthesis[J]. Materials Letters . 2006 (3)

5Shi-Bo Li,Guo-Ping Bei,Hong-Xiang Zhai,Yang Zhou.Synthesis of Ti 2 SnC from Ti/Sn/TiC powder mixtures by pressureless sintering technique[J]. Materials Letters . 2006 (29)

6Yanchun Zhou,Hongying Dong,Xiaohui Wang,Chengke Yan.Preparation of Ti2SnC by solid–liquid reaction synthesis and simultaneous densification method[J]. Materials Research Innovations . 2002 (5-6)

7M.W. Barsoum,G. Yaroschuk.Fabrication and characterization of M 2 SnC (M = Ti, Zr, Hf and Nb)[J].Scripta Materialia.1997(10)

1蔡璋文,李啸轩,王春晓,朱春城.三元层状陶瓷Ti_2SnC的研究进展[J].材料导报,2018,32(A01):99-104. 被引量:1

1宋丽红,慕利斌.三元层状氮化物Ti2InN材料的合成及电学性质研究[J].真空科学与技术学报,2020,40(12):1225-1228.

1贝国平,李世波,翟洪祥,周洋.Ti_2SnC的合成及其反应机制的研究[J].航空材料学报,2007,27(3):47-50. 被引量:8

2梁宝岩,关耀君,刘嘉霖,徐世帅.自蔓延高温烧结制备钛锡碳结合剂金刚石复合材料[J].金刚石与磨料磨具工程,2015,35(1):35-38. 被引量:2

3许浩,黄振莺,王雅正.Ti_2SnC块体材料的制备及摩擦学性能研究[J].稀有金属材料与工程,2015,44(S1):825-828. 被引量:2

4张少冲,严有为.自蔓延高温合成技术的局限性及其对策[J].材料导报,2004,18(F10):198-200. 被引量:1

5郎晓川,谢宏伟,翟玉春,邹祥宇.熔盐电解法制备TiC粉末的研究[J].稀有金属与硬质合金,2013,41(5):1-4. 被引量:5

6金正中,李琳,傅正义.自蔓延高温合成技术及其制备新材料的研究[J].现代技术陶瓷,2001,22(2):27-32. 被引量:2

7陈怡元,邹正光,龙飞.碳源对自蔓延高温合成TiC粉末的影响[J].桂林工学院学报,2006,26(4):534-537. 被引量:9

8梁宝岩,张旺玺,史冬丽,穆云超.SHS技术在金刚石表面镀覆Ni-TiC复合涂层的研究[J].金刚石与磨料磨具工程,2016,36(3):50-53. 被引量:5

9王华彬,韩杰才,杜善义.自蔓延高温合成技术应用的新进展[J].功能材料,1997,28(2):115-121. 被引量:13

10胡继林,刘鑫,胡传跃,郭文明.TiC制备技术及其增强SiC基复合材料的研究进展[J].中国陶瓷,2013,49(12):1-5. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TQ174.6[化学工程—陶瓷工业]

Citation Information:

The Ti2 SnC material was prepared by self-propagation high-temperature synthesis(SHS)with2Ti/Sn/C and Ti/Sn/TiC as the raw materials.Effects of the two raw materials on Ti2SnC synthesis were investigated.The results show that with the two raw materials,Ti2 SnC can be synthesized by SHS,and the products contain a small amount of TiC and Sn.With 2Ti/Sn/C as the raw powder material,the synthesized Ti2 SnC has well-developed lath grains of about 10μm length and about 2μm width.With Ti/Sn/TiC as the raw material,the synthesized Ti2 SnC has fine granular grains of about 1~5μm granularity.

quote

GB/T 7714-2015 [1] LIANG Bao-yan, ZHANG Wang-xi, WANG Yan-zhi, et al. Research on Self-propagation High-temperature Synthesis of Ti_2SnC Material[J]. Rare Metals and Cemented Carbides, 2015(4): 43-46.
MLA [1] LIANG Bao-yan, et al., "Research on Self-propagation High-temperature Synthesis of Ti_2SnC Material." Rare Metals and Cemented Carbides, no. 4, 2015, pp. 43-46.
APA [1] LIANG Bao-yan, ZHANG Wang-xi, WANG Yan-zhi, & XU Shi-shuai. (2015). Research on Self-propagation High-temperature Synthesis of Ti_2SnC Material. Rare Metals and Cemented Carbides(4), 43-46.
IEEE [1] LIANG Bao-yan, ZHANG Wang-xi, WANG Yan-zhi, and XU Shi-shuai, "Research on Self-propagation High-temperature Synthesis of Ti_2SnC Material," Rare Metals and Cemented Carbides, no. 4, pp. 43-46, 2015. keywords: {Ti2SnC;self-propagation high-temperature synthesis;microstructure;reaction mechanism}