daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synthesis of pH-Responsive Polymer Sponge Coatings and Freestanding Films via Vapor-Phase Deposition AITranslate

University of Southern California; University of Southern California; University of Southern California
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Porous polymer materials are desired for a variety of applications such as catalysis, filtration, sensing, optics, and biological engineering. In this work, we present a modified initiated chemical vapor deposition (iCVD) process to synthesize spongelike stimuli-responsive poly(methacrylic acid) (PMAA) polymer coatings and freestanding films characterized by micron-sized pores, pore interconnectivity, and varying heights. The carboxylic acid functional group in the PMAA sponge allows for pH-responsive behavior ideal for biomedical applications and separations. Thermal annealing was used to control the dissolution of sponge coatings in different pH environments. Ethylene glycol diacrylate was introduced during the fabrication process to form freestanding sponges with pH-responsive swelling behavior, and glycidyl methacrylate was introduced during the fabrication process to increase the durability of sponge coatings. Hierarchical structures with a bottom sponge layer and a top pillared layer were fabricated in situ by varying processing conditions. The sponge structures were coated with a fluorinated polymer to fabricate superhydrophobic structures with self-cleaning properties. Our fabrication process offers an all-dry one-pot method to synthesize polymer sponges with different functionalities for a range of applications in drug delivery, sensor, and separation applications.

KeyWords AITranslate

porous polymers functional coatings freestanding films pHresponsive initiated chemical vapor deposition Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01151

Chinese Library Classification Number:

Citation Information:

Porous polymer materials are desired for a variety of applications such as catalysis, filtration, sensing, optics, and biological engineering. In this work, we present a modified initiated chemical vapor deposition (iCVD) process to synthesize spongelike stimuli-responsive poly(methacrylic acid) (PMAA) polymer coatings and freestanding films characterized by micron-sized pores, pore interconnectivity, and varying heights. The carboxylic acid functional group in the PMAA sponge allows for pH-responsive behavior ideal for biomedical applications and separations. Thermal annealing was used to control the dissolution of sponge coatings in different pH environments. Ethylene glycol diacrylate was introduced during the fabrication process to form freestanding sponges with pH-responsive swelling behavior, and glycidyl methacrylate was introduced during the fabrication process to increase the durability of sponge coatings. Hierarchical structures with a bottom sponge layer and a top pillared layer were fabricated in situ by varying processing conditions. The sponge structures were coated with a fluorinated polymer to fabricate superhydrophobic structures with self-cleaning properties. Our fabrication process offers an all-dry one-pot method to synthesize polymer sponges with different functionalities for a range of applications in drug delivery, sensor, and separation applications.

quote

GB/T 7714-2015 [1] Stacey Bacheller, Golnaz Dianat, Malancha Gupta. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01151.
MLA [1] Stacey Bacheller, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01151.
APA [1] Stacey Bacheller, Golnaz Dianat, & Malancha Gupta. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01151
IEEE [1] Stacey Bacheller, Golnaz Dianat, and Malancha Gupta, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01151. keywords: {porous polymers;functional coatings;freestanding films;pHresponsive;initiated chemical vapor deposition;Show More}