Facile Synthesis of Hyperbranched Copolymers via an [A2 + B3] Click Polymerization Synthesized Reducible Hyperbranched Template AITranslate

Southern University of Science and Technology; University of South China; Southern University of Science and Technology; Southern University of Science and Technology; Lanzhou University; Southern University of Science and Technology; Lanzhou University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Synthesis of multifunctional hyperbranched polymers (HPs) with simultaneously precisely modulated degrees of branch (DBs) and multibiorelevant signal-triggered sensitivities generally suffers from multistep preparation and purification procedures and uncontrolled DB. To develop a facile yet robust approach toward multifunctional HPs with a precisely modulated DB, we reported herein the synthesis of a reducible hyperbranched polymer template (HPT) with a fixed DB via an [A2 + B3]-based click polymerization and its further mediation of reversible addition–fragmentation chain transfer (RAFT) polymerization for the facile preparation of well-defined multifunctional HPs with a uniform DB, predetermined polymer compositions, and well-modulated molecular weights (MWs) and low dispersity (Đ) indexes. The breakthrough of this study is the design of a bioreducible HPT-based multimacro chain transfer agent (multimacro-CTA) with a fixed DB of 0.45 via click polymerization between an A2 unit containing a central trithiocarbonate group for further conduction of RAFT polymerization of any vinyl-based monomers, two disulfide links for reduction sensitivity, and two azide groups and a branched B3 unit with three highly reactive alkynyl functions. The resulting HPT was further adopted as a multimacro-CTA to mediate RAFT polymerization of a previously reported acidic pH cleavable oligo(ethylene glycol) monomethyl ether methacrylate (OEGMA) monomer, α-OEGMA, affording reduction and acidic pH dual sensitive HPT-P(α-OEGMA). Notably, the resulting polymer panel of HPT-P(α-OEGMA)s could self-assemble into stabilized unimolecular micelles with MW-dependent mean hydrodynamic size in a range from 18.9 to 27.0 nm. The drug-loaded HPT-P(α-OEGMA) micelles incubated in a reducing or an acidic pH condition showed accelerated drug release due to the reduction-triggered cleavage of the disulfide links or an acidic pH induced breakage of the acetal links for polymer degradation. Therefore, the universal HPT platform provides a facile yet robust approach toward well-defined multifunctional HPs with a uniform DB, well-controlled MWs, and low Đ indexes for biomedical applications.

KeyWords AITranslate

hyperbranched polymer degree of branch reduction sensitivity acidic pH sensitivity click polymerization controlled drug release
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01153

Chinese Library Classification Number:

Citation Information:

Synthesis of multifunctional hyperbranched polymers (HPs) with simultaneously precisely modulated degrees of branch (DBs) and multibiorelevant signal-triggered sensitivities generally suffers from multistep preparation and purification procedures and uncontrolled DB. To develop a facile yet robust approach toward multifunctional HPs with a precisely modulated DB, we reported herein the synthesis of a reducible hyperbranched polymer template (HPT) with a fixed DB via an [A2 + B3]-based click polymerization and its further mediation of reversible addition–fragmentation chain transfer (RAFT) polymerization for the facile preparation of well-defined multifunctional HPs with a uniform DB, predetermined polymer compositions, and well-modulated molecular weights (MWs) and low dispersity (Đ) indexes. The breakthrough of this study is the design of a bioreducible HPT-based multimacro chain transfer agent (multimacro-CTA) with a fixed DB of 0.45 via click polymerization between an A2 unit containing a central trithiocarbonate group for further conduction of RAFT polymerization of any vinyl-based monomers, two disulfide links for reduction sensitivity, and two azide groups and a branched B3 unit with three highly reactive alkynyl functions. The resulting HPT was further adopted as a multimacro-CTA to mediate RAFT polymerization of a previously reported acidic pH cleavable oligo(ethylene glycol) monomethyl ether methacrylate (OEGMA) monomer, α-OEGMA, affording reduction and acidic pH dual sensitive HPT-P(α-OEGMA). Notably, the resulting polymer panel of HPT-P(α-OEGMA)s could self-assemble into stabilized unimolecular micelles with MW-dependent mean hydrodynamic size in a range from 18.9 to 27.0 nm. The drug-loaded HPT-P(α-OEGMA) micelles incubated in a reducing or an acidic pH condition showed accelerated drug release due to the reduction-triggered cleavage of the disulfide links or an acidic pH induced breakage of the acetal links for polymer degradation. Therefore, the universal HPT platform provides a facile yet robust approach toward well-defined multifunctional HPs with a uniform DB, well-controlled MWs, and low Đ indexes for biomedical applications.

quote

GB/T 7714-2015 [1] Yuping Liu, Wei Ma, Zhen Dong, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01153.
MLA [1] Yuping Liu, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01153.
APA [1] Yuping Liu, Wei Ma, Zhen Dong, Nanting Qiu, Liwei Ma, ZhongRen Chen, & Hua Wei. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01153
IEEE [1] Yuping Liu, Wei Ma, Zhen Dong, Nanting Qiu, Liwei Ma, ZhongRen Chen, and Hua Wei, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01153. keywords: {hyperbranched polymer;degree of branch;reduction sensitivity;acidic pH sensitivity;click polymerization;controlled drug release}