The Latest and Future Development of Nitride Phosphor Used in White LED AITranslate

Hunan Institute of Rare Earth Metal Materials Institute of Metals and Alloys;Hunan Institute of Rare Earth Metal Materials Institute of Metals and Alloys;Hunan Institute of Rare Earth Metal Materials Institute of Metals and Alloys;Hunan Institute of Rare Earth Metal Materials Institute of Metals and Alloys
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

:The latest development of nitride phosphor used in white LED is reviewed, and the problems and trends are analyzed. The nitride phosphor M2Si5 N8 : Eu(M= Ca, Sr,Ba) is emphatically introduced. Appli- cation prospect of new nitride phosphor is pointed out. Preparation of high purity metal materials such as Eu,Ca,Sr and synthesis of nitride powders are critical for the development of new nitride phosphor.

KeyWords AITranslate

nitride phosphor white LED the latest development development trend

1张凯,刘河洲,胡文彬.白光LED用荧光粉的研究进展[J].材料导报,2005,19(9):50-53. 被引量:63

2吴占超,刘杰,侯万国.白色发光二极管用蓝色荧光粉的研究进展[J].材料导报:纳米与新材料专辑,2009,23(2):105-108. 被引量:4

3印琰,杨宝东,朱月华,王海波.白光LED用荧光粉的发展现状[J].中国照明电器,2009(3):6-10. 被引量:34

4Feldmann C,Justel T, Ronda C R, et al. Inorganic luminescent materials: 100 years of research and application[J]. Adv Funct Mater, 2003,13 : 511-516.

5Sreekanth Chakradhar R P, Nagabhushana B M,Ramesh K P, et al. Solution combustio derived nanocrystalline Zn2SiO4 : Mn phosphors: A spectroscopic view[J]. J Chem Phys,2004,121 : 10 250-10 259.

6Hattori Y, Isobe T, Takahashi H, et al. Photoluminescenee properties of Eu^2+-aetivated sialon S-phase BaAl- Si5O2N7 [J]. J Lumin, 2005,113 (1,2) : 69 -78.

7ChenG, CravenM, KimA, et al, Performance of high- power Ⅲ-nitride light emitting diodes[J]. Physic Status Solid A,2008,205(2):1 086-1 092.

8Xie R J, Hirosaki N, Mitomom,et al. Strong green emission from alpha-SiAlON activated by divalent ytterbimn under blue light irradiation[J]. J Phys Chem: B, 2005,9 (19) :9 490-9 494.

9Hhiosaki N, Kocer C,Ogata S,et a l. Ab initio characterization of the mechanical and electronic properties of beta -SiAION (Si6-z AlzOx N8-x;z= 0-5 ) [J]. Physical review B,2005,71:104 105(1)-104 105(12).

10韩建伟,黄淋毅,王昌铃,石士考,刘行仁.白光LED用几种Eu^(2+)激活的红色荧光体的性能[J].照明工程学报,2009,20(3):18-23. 被引量:2

1刘吉波,杨涛,王志坚,苏正夫,成维.废旧稀土荧光灯资源的回收方法研究现状[J].稀有金属与硬质合金,2014,42(2):29-31. 被引量:3

2成维,黄美松,杨露辉,贾帅广,杨涛,包新军.高纯金属铕的制备工艺研究[J].有色金属:冶炼部分,2014(6):55-57. 被引量:7

3张文涛,田学敏,王玉龙,龙剑平.RCa_2Mg_2(VO_4)_3(R=Li,K,Na)荧光粉的制备及发光性能研究[J].电子元件与材料,2015,34(11):31-34. 被引量:3

4何军,廖森,韦庆敏.LED荧光粉发展现状及趋势探讨[J].民营科技,2017(1):37-38.

5李海速,刘在洲,张保,夏冰,贾泳,向康.455nm蓝激光激发YAG∶Ce^(3+)荧光轮光源输出特性研究[J].光学与光电技术,2018,16(5):60-65.

6刘志航.LED半导体照明的核心技术与发展趋势[J].科技资讯,2017,15(32):75-75. 被引量:4

7林金填,陈磊,蔡金兰,邱镇民,冉崇高.Ca替代Sr对Sr_2Si_5N_8:Eu^(2+)荧光粉结构、光谱及热猝灭性能的影响[J].照明工程学报,2019,30(1):38-42.

8张先恒,赵二雄,苗旭晨,陈国华,刘玉宝.金属铕纯度控制的研究[J].稀土,2019,40(1):121-127. 被引量:5

9Wenjie Wu,Kefu Chao,Wenquan Liu,Lesi Wei,Dahai Hu,Taiyang Wang,O. Tegus.Enhanced orange emission by doping CeB_6 in CaAlSiN_3:Ce^(3+) phosphor for application in white LEDs[J].稀土学报:英文版,2018,0(12):1250-1255. 被引量:6

1刘朋朋,沈佳,徐玉,邹军,石明明,徐慧,陈启.一种驱蚊灯的光电性能研究[J].灯与照明,2019,0(3):53-57.

2李鸿亚,胡志方,江洪林,尹延西.高纯金属钪锭的制备[J].有色金属:冶炼部分,2017(12):43-46.

3张立志,周桓竹,樊思宁,秦振伟.发光材料中稀土元素回收的研究[J].科技创新与生产力,2018(7):50-52.

4刘伟程.LED半导体照明技术存在的问题及优化策略分析[J].电子技术与软件工程,2019(5):114-114. 被引量:5

5Robert Tomala,Dariusz Hreniak,Wieslaw Strek.Laser induced broadband white emission of Y2Si2O7 nanocrystals[J].稀土学报:英文版,2019,37(11):1196-1199. 被引量:2

6李国玲,李吉刚,傅凯,李星国.等离子体在提纯金属过程中微痕量杂质元素迁移机制的影响规律[J].中国稀土学报,2019,37(6):647-654. 被引量:3

7庞才良,赖小辉,陈林.熔盐法制备NaCa2Mg2(VO4)3:Eu3+白色荧光粉[J].萍乡学院学报,2019,36(6):34-37.

8彭康亮,陈林,孙朝中,杨雪晴,宋杰光.熔盐法制备Ca5Mg4(VO4)6绿色荧光粉及其发光性能研究[J].硅酸盐通报,2020,39(3):969-973. 被引量:1

9卡依尔江·卡哈尔.废荧光灯的环境污染对策探讨[J].新疆环境保护,2020,42(1):47-50.

10赵丹,赵丹丹,薛亚丽.一种新型蓝色发光材料Na13Sr2Ta2(PO4)9:Tm3+的合成及性能研究[J].聊城大学学报:自然科学版,2020,33(5):66-73. 被引量:1

1龚朝阳,李泉,程璇,张颖.先驱体转化法制备硅基氮氧化物荧光粉的初步研究[J].陶瓷学报,2016,37(2):191-194. 被引量:1

2杨晓婵(摘译).超高纯金属[J].现代材料动态,2006(2):11-12.

3张琦,李文,林燕,彭兆城,王欣泽,孔海南.酵母菌性能优化关键技术研究进展[J].酿酒科技,2013(4):80-87. 被引量:6

4王衍行,祖成奎,赵华,何坤,赵慧峰,陈江,韩滨.长波红外玻璃的研究[J].功能材料,2010,41(A02):196-200. 被引量:6

5彭文利,谈娟娟,谢美燕.鞋类新型材料的应用及发展趋势[J].西部皮革,2009,31(10):18-20. 被引量:1

6朱永康.乐山筹建国家硅材料质检中心[J].中国橡胶,2010(17):47-47.

7朱永康.乐山筹建国家硅材料质检中心[J].橡胶科技市场,2010(20):36-36.

8内蒙古锦洋化工水合肼项目开工[J].氯碱工业,2013(12):19-19.

9杭氧联合德国MESSER公司攻克技术壁垒研制成功首台国产稀有气体氪氙提取装置[J].气体分离,2011,0(6):42-42.

10邓涛.旋流电解技术及其应用[J].世界有色金属,2012(12):34-37. 被引量:17

Basic Information:

DOI:

Chinese Library Classification Number:TQ133.3[化学工程—无机化工]

Citation Information:

:The latest development of nitride phosphor used in white LED is reviewed, and the problems and trends are analyzed. The nitride phosphor M2Si5 N8 : Eu(M= Ca, Sr,Ba) is emphatically introduced. Appli- cation prospect of new nitride phosphor is pointed out. Preparation of high purity metal materials such as Eu,Ca,Sr and synthesis of nitride powders are critical for the development of new nitride phosphor.

quote

GB/T 7714-2015 [1] HUANG Mei-song, ZHANG Ke-xiang, ZHANG Yao-bin, et al. The Latest and Future Development of Nitride Phosphor Used in White LED[J]. Rare Metals and Cemented Carbides, 2012(1): 34-37.
MLA [1] HUANG Mei-song, et al., "The Latest and Future Development of Nitride Phosphor Used in White LED." Rare Metals and Cemented Carbides, no. 1, 2012, pp. 34-37.
APA [1] HUANG Mei-song, ZHANG Ke-xiang, ZHANG Yao-bin, & CHEN Yun-zhi. (2012). The Latest and Future Development of Nitride Phosphor Used in White LED. Rare Metals and Cemented Carbides(1), 34-37.
IEEE [1] HUANG Mei-song, ZHANG Ke-xiang, ZHANG Yao-bin, and CHEN Yun-zhi, "The Latest and Future Development of Nitride Phosphor Used in White LED," Rare Metals and Cemented Carbides, no. 1, pp. 34-37, 2012. keywords: {nitride phosphor;white LED;the latest development;development trend}