Synthesis of New Benzimidazole Corrosion Inhibitor Applied in Cemented Carbide AITranslate
Abstract AITranslate
Three kinds of benzimidazole ramification including 2-(o/i/p)-nitrobenzimidazole were synthesized by one step with o-phenylenediamine and nitrobenzaldehyde as the materials.And they were applied in cemented carbide anticorrosion.The results show that the optimal synthesis technical parameters are as follows:the ratio of o-phenylenediamine to nitrobenzaldehyde is 1.2,reaction temperature 60 ℃,heating duration 20 min.The melting point analysis results show that the synthetic product is the target product.The corrosion inhibition rate of the new corrosion inhibitor is up to 95.6%,better than that of the similar domestic products.
KeyWords AITranslate
1G.Mori,吴建国,陈满元.Cr3C2、TiC和TaC添加剂对硬质合金耐腐蚀性的影响[J].国外难熔金属与硬质材料,2003,19(2):10-15. 被引量:11
2张伟,蒋勇.耐腐蚀硬质合金的性能与选用[J].粉末冶金技术,1994,12(3):235-235. 被引量:2
1王娴.苯并咪唑类缓蚀剂缓蚀机理以及研究趋势[J].清洗世界,2012,28(6):27-33. 被引量:2
2娴文.苯并咪唑类缓蚀剂缓释机理以及研究趋势[J].精细化工原料及中间体,2012(7):24-27.
1刘雪,孟艳斌,马雪梅,胡志勇.具有表面活性的杂环缓蚀剂的合成及性能评价[J].化学通报,2016,79(2):164-169. 被引量:2
2李伟光,袁斌,何冠宁,贾群坡.新型苯并三氮唑基咪唑啉缓蚀剂的合成及性能研究[J].应用化工,2017,46(9):1752-1756. 被引量:5
1苏铁军,习伟,邓仕英.一种苯并咪唑衍生物对盐酸中N80钢的缓蚀作用[J].广东化工,2014,41(18):36-37. 被引量:1
2李杰兰,梁成浩,黄乃宝,贾广鹏.苯并咪唑衍生物缓蚀剂研究进展[J].腐蚀科学与防护技术,2011,23(2):191-195. 被引量:11
3左秀丽,舒建华,王志民,何天稀.高氯油田水溶液中咪唑类缓蚀剂的性能[J].腐蚀与防护,2015,36(2):148-151. 被引量:5
4苏铁军,李克华,罗运柏,习伟.盐酸介质中APPB对A3钢的缓蚀作用[J].腐蚀与防护,2015,36(7):629-634. 被引量:1
5张宝文,何伟,M.Grote,A.Kettrup.邻位酸性取代基甲(月替)衍生物的合成及其在分析化学上的应用Ⅳ.钢中钴的直接分光光度测定[J].冶金分析,1989,9(4):13-16. 被引量:2
6苏铁军,罗运柏,李克华,李凡修,邓仕英,习伟.苯并咪唑-N-曼尼希碱对盐酸中N80钢的缓蚀性能[J].中国腐蚀与防护学报,2015,35(5):415-422. 被引量:15
7王青,马雪梅,石海燕,原珊,郭建峰,梁栋,胡志勇.苯并咪唑衍生物在1mol/LHCl溶液中对45#碳钢缓蚀行为的研究[J].中国腐蚀与防护学报,2015,35(1):49-54. 被引量:8
8石墨烯在金属防腐领域取得新突破[J].中国粉体工业,2014(1):48-48.
9王娴.苯并咪唑类缓蚀剂缓蚀机理以及研究趋势[J].清洗世界,2012,28(6):27-33. 被引量:2
10林一坚.再结晶织构与形变织构间位向关系的研究[J].上海钢研,1997(3):1-4. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG174.42[金属学及工艺—金属表面处理]
Citation Information:
Three kinds of benzimidazole ramification including 2-(o/i/p)-nitrobenzimidazole were synthesized by one step with o-phenylenediamine and nitrobenzaldehyde as the materials.And they were applied in cemented carbide anticorrosion.The results show that the optimal synthesis technical parameters are as follows:the ratio of o-phenylenediamine to nitrobenzaldehyde is 1.2,reaction temperature 60 ℃,heating duration 20 min.The melting point analysis results show that the synthetic product is the target product.The corrosion inhibition rate of the new corrosion inhibitor is up to 95.6%,better than that of the similar domestic products.
quote
| GB/T 7714-2015 | [1] TANG Kai, YAN Jie, SUN Ya-li, et al. Synthesis of New Benzimidazole Corrosion Inhibitor Applied in Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2010(3): 16-18. |
| MLA | [1] TANG Kai, et al., "Synthesis of New Benzimidazole Corrosion Inhibitor Applied in Cemented Carbide." Rare Metals and Cemented Carbides, no. 3, 2010, pp. 16-18. |
| APA | [1] TANG Kai, YAN Jie, SUN Ya-li, & LI Li. (2010). Synthesis of New Benzimidazole Corrosion Inhibitor Applied in Cemented Carbide. Rare Metals and Cemented Carbides(3), 16-18. |
| IEEE | [1] TANG Kai, YAN Jie, SUN Ya-li, and LI Li, "Synthesis of New Benzimidazole Corrosion Inhibitor Applied in Cemented Carbide," Rare Metals and Cemented Carbides, no. 3, pp. 16-18, 2010. keywords: {benzimidazole;cemented carbide anticorrosion;corrosion inhibitor;corrosion inhibition rate} |