Study on Preparation and Properties of New Cu-based Composite AITranslate

College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Copper-coated carbon fiber-graphite-copper matrix composite,carbon nanotube-graphite-copper matrix composite and graphite-copper matrix composite were prepared by powder metallurgy.The properties of the composites,such as density,resistivity,Vickers hardness and bend strength,were tested,the microstructure is observed and then the comprehensive performance was compared with each other.The results show that carbon fiber-graphite-copper matrix composite is of the most excellent performance in the three composites.

KeyWords AITranslate

copper-based composite graphite carbon fiber carbon nanotube

1王文芳,许少凡,应美芳,王成福,褚道葆,颐家山,陈发华.用镀铜石墨粉制备铜-石墨复合材料[J].机械工程材料,1999,23(2):41-43. 被引量:34

2孙巍,李文珍.碳纳米管增强铜基复合材料的制备技术研究[J].铸造技术,2008,29(1):29-32. 被引量:15

3许少凡,顾斌,李政,王成福.镀铜碳纤维-镀铜石墨-铜基复合材料的制备与性能研究[J].兵器材料科学与工程,2006,29(5):1-4. 被引量:8

4许少凡,凤仪,颜士钦,应美芳,王成福.碳纤维对中铜-石墨复合材料组织与性能的影响[J].合肥工业大学学报:自然科学版,1997,20(6):10-15. 被引量:4

5高强,吴渝英,张国定,洪锓,肖学明.碳纤维对铜-石墨复合材料性能的影响[J].中国有色金属学报,2000,10(S1):97-101. 被引量:27

6凤仪,应美芳,王成福.碳纤维不同分布的碳纤维-铜复合材料的电导率[J].复合材料学报,1998,15(4):38-42. 被引量:21

7董仕节,史耀武.铜基复合材料的研究进展[J].国外金属热处理,1999,20(6):9-11. 被引量:19

8许少凡,王文芳,凤仪,颜士钦,应美芳,王成福.碳纤维-中铜-石墨复合材料的摩擦磨损性能研究[J].摩擦学学报,1998,18(3):254-258. 被引量:25

9徐金城,李晓龙,夏龙,杨华,于辉.短碳纤维增强铜基复合材料的制备及其性能的研究[J].兰州大学学报:自然科学版,2004,40(4):28-32. 被引量:18

10李政,许少凡.碳纤维对镀铜石墨-铜基复合材料性能的影响[J].热加工工艺,2004,33(4):41-41. 被引量:9

1毕红梅,梁英,史克英.氧化铜/碳纳米管复合物的制备及其微观结构的研究[J].黑龙江八一农垦大学学报,2011,23(6):78-80. 被引量:2

2杨正海,张永振,陈拂晓,上官宝,李雪飞,田磊.载流摩擦用铜碳粉末冶金材料概述[J].材料导报,2012,26(3):106-110. 被引量:6

3杜建文,程继贵,詹海林,叶楠敏.轧膜成形制备石墨/Cu复合材料及其性能研究[J].粉末冶金工业,2014,24(3):29-33. 被引量:1

4于竹丽,朱和国.铜基复合材料的导电性研究现状[J].材料导报:纳米与新材料专辑,2015,29(2):345-349. 被引量:6

5范涛,申珣,王虎,刘翊安,张程,陈泽雷,赵东方,唐伟忠,贾成厂.球磨工艺对原位合成SiCp增强铜复合材料组织及性能的影响[J].粉末冶金技术,2016,34(4):264-267. 被引量:4

6张俊峰,邓璘.列车制动用Cu基粉末闸片材料摩擦磨损性能分析[J].粉末冶金工业,2017,27(2):38-41. 被引量:8

7杨淑贞,马海英,张晓旭.铜基粉末冶金刹车闸瓦材料的摩擦磨损性能研究[J].铸造技术,2017,38(9):2093-2095.

8杨淑贞,马海英,张晓旭.铜基粉末冶金刹车闸瓦材料摩擦磨损性能研究[J].铸造技术,2017,38(10):2369-2370. 被引量:2

9刘建秀,宋阳,樊江磊,吴深,张驰,贾德晋,李育文.碳纤维增强铜基复合材料研究进展[J].材料科学与工程学报,2018,36(2):342-346. 被引量:8

10韩东艳,贾爱芹,邱文.拉拔压下量对车用Al2O3/Cu复合材料组织和硬度的影响[J].热加工工艺,2018,47(16):133-135.

1舒鑫,刘洋赈,李卫.铜基复合材料的载流摩擦磨损研究进展[J].特种铸造及有色合金,2022,42(4):419-424.

2霸书红,闫明辉,周龙,程秀莲,王桂萍,万新国,杜雪峰.纳米CuO/CNTs的制备及对高氯酸钾基烟火药发光强度的影响[J].含能材料,2014,22(1):80-83. 被引量:7

3张永振,杨正海,上官宝.载流摩擦的研究现状与挑战[J].自然杂志,2014,36(4):256-263. 被引量:18

4孙建荣,李长生,唐华,华希俊.含NbSe_2的铜基电接触复合材料的制备及其真空摩擦学性能研究[J].无机材料学报,2014,29(9):936-940.

5吴海华,李腾飞,肖林楠,熊盼.鳞片石墨粉末选择性激光烧结成型工艺研究[J].激光与光电子学进展,2016,53(10):182-187. 被引量:17

6刘建秀,宋阳,樊江磊,吴深,张驰,贾德晋,李育文.碳纤维增强铜基复合材料研究进展[J].材料科学与工程学报,2018,36(2):342-346. 被引量:8

7许海,李钊,王俊峰,陈金水,肖翔鹏.SPS烧结原位制备Al2O3-TiC增强Cu基复合材料的组织与性能[J].材料热处理学报,2018,39(5):10-16. 被引量:1

8姚萍屏,肖叶龙,张忠义,周海滨,贡太敏,赵林,邓敏文.高速列车粉末冶金制动材料的研究进展[J].中国材料进展,2019,38(2):116-125. 被引量:16

9付昌星,张晓旭.离合器用30CrMnSiA钢制动片和铜基粉末冶金摩擦片的温摩擦磨损性能分析[J].粉末冶金工业,2019,29(3):41-45. 被引量:5

10代世勋,张竹林.石墨与BN添加对车离合器用铜基摩擦材料磨损性能的影响[J].粉末冶金工业,2019,29(3):57-61. 被引量:8

1杜金晶,王斌,曹卓坤,姚广春,梁李斯.镀铜碳纤维增强铝基泡沫材料准静态压缩力学性能及吸能特性[J].有色金属工程,2016,6(3):1-4. 被引量:3

2杜金晶,王斌,曹卓坤,姚广春,梁李斯.镀铜碳纤维增强铝基泡沫材料结构的特性表征[J].材料导报,2016,30(6):82-85.

3乐青,周灵平,朱家俊,李德意.电子封装用碳纤维/铜复合材料制备与性能研究[J].真空电子技术,2015,28(5):36-39 51. 被引量:2

4李政,许少凡.碳纤维对镀铜石墨-铜基复合材料性能的影响[J].热加工工艺,2004,33(4):41-41. 被引量:9

5杨正伟,程振财,卢裕高,杨琪.碳纤维/铜复合涂层材料研究[J].上海工程技术大学学报,2013,27(2):151-153. 被引量:1

6钟涛生,邹伟,付求涯.用粉末冶金法制备C_fAl复合材料研究[J].热处理,2009,24(6):53-55. 被引量:4

7张林光,谢敬佩,刘舒,孙浩亮,王文炎.短碳纤维表面镀铜的研究[J].河南科技大学学报:自然科学版,2014,35(2):1-6. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TB333[一般工业技术—材料科学与工程]

Citation Information:

Copper-coated carbon fiber-graphite-copper matrix composite,carbon nanotube-graphite-copper matrix composite and graphite-copper matrix composite were prepared by powder metallurgy.The properties of the composites,such as density,resistivity,Vickers hardness and bend strength,were tested,the microstructure is observed and then the comprehensive performance was compared with each other.The results show that carbon fiber-graphite-copper matrix composite is of the most excellent performance in the three composites.

quote

GB/T 7714-2015 [1] SONG Ying-ying, LI Jia-jie, ZHANG Biao. Study on Preparation and Properties of New Cu-based Composite[J]. Rare Metals and Cemented Carbides, 2010(3): 13-15.
MLA [1] SONG Ying-ying, et al., "Study on Preparation and Properties of New Cu-based Composite." Rare Metals and Cemented Carbides, no. 3, 2010, pp. 13-15.
APA [1] SONG Ying-ying, LI Jia-jie, & ZHANG Biao. (2010). Study on Preparation and Properties of New Cu-based Composite. Rare Metals and Cemented Carbides(3), 13-15.
IEEE [1] SONG Ying-ying, LI Jia-jie, and ZHANG Biao, "Study on Preparation and Properties of New Cu-based Composite," Rare Metals and Cemented Carbides, no. 3, pp. 13-15, 2010. keywords: {copper-based composite;graphite;carbon fiber;carbon nanotube}