Orthogonal Design to Optimize the Technological Parameters of Preparing Aluminum-based Composite Photocatalyst AITranslate
Abstract AITranslate
Aluminum-based composite photocatalyst was prepared by coating flake aluminum powders with TiO2 and using sol-gel method.The influences of technological parameters on the photocatalysis property were studied by orthogonal experiments.The samples were analyzed and characterized by XRD.The results show that the photocatalysis property is significantly affected by calcination temperature.The degradation rate of methylene blue is up to 93.5% through 3 h UV-lamp irradiation when hydrolysis temperature is 30 ℃,pH value 4.5,molar ratio of water to tetrabutyl titanate 50,and calcination temperature 600 ℃.
KeyWords AITranslate
1Fujishima A, Honda K. Electrochemical photolysis of water at an semiconductor electrode[J]. Nature, 1972, 238:37-38.
2Hoffmann M R, Martin S T, Choi W, et al. environmental applications of semiconductor photocatalysis [J] Chemical Reviews, 1995,95 (1) :69-96.
3彭峰,任艳群.TiO_2-SnO_2复合纳米膜的制备及其光催化降解甲苯的活性[J].催化学报(英文),2003,24(4):243-247. 被引量:48
4李和平,袁曹龙,张玉强,曹忠.金属共掺杂纳米TiO_2对甲基橙的催化降解[J].印染,2006,32(24):9-13. 被引量:15
5李婷,武晓伟,施亦东,陈衍夏.纳米TiO_2的分散及其在织物上整理工艺的研究[J].印染助剂,2007,24(7):34-37. 被引量:5
6蔡铁军,岳明,王贤文,邓谦,彭振山,周文辉.复合催化剂NdPW_(12)O_(40)/TiO_2的制备、表征及光催化性能[J].催化学报(英文),2007,28(1):10-16. 被引量:16
7张建臣,郭坤敏,马兰,赵红阳.TiO_2/AC复合光催化剂对苯和丁醛的气相光催化降解机理[J].催化学报(英文),2006,27(10):853-856. 被引量:15
8陆必志,陈振兴,黄巧萍,刘辉.纳米片状铝粉的制备及其发展动态[J].涂料技术与文摘,2004,25(1):1-4. 被引量:6
9蔡河山,刘国光,黎晓霞,吕文英,余林.不同气氛下TiO2纳米晶的光催化性能研究[J].化工新型材料,2008,36(4):39-41. 被引量:1
10李云雁,胡传荣.试验设计与数据处理[M].北京:化学工业出版社,2004.87~91
1殷国祥,孙勇,杨宁,赵如龙,郭中正,鲁俐.片状铝粉的SiO_2包覆着色研究[J].金属功能材料,2010,17(4):33-37. 被引量:5
2于丽敏,蒋文全,傅钟臻.含Fe低CoAB_5型贮氢合金的性能与结构[J].稀有金属,2005,29(6):856-859. 被引量:3
3邹隽,叶建红,王剑阳,杨慧.正交试验设计在Cr12MoV工艺试验中的应用[J].模具制造,2005,5(7):59-61. 被引量:1
4殷国祥,孙勇,杨宁,赵如龙,郭中正,鲁俐.片状铝粉包覆着色的研究[J].南方金属,2009(6):22-25. 被引量:3
5王胜民,何明弈,章全奎.机械镀锌-铝复合镀层的结构分析[J].电镀与涂饰,2005,24(11):5-7. 被引量:6
6田春益.45#钢厚板窄间隙焊接工艺研究[J].现代焊接,2015,0(12):33-35. 被引量:1
7牛宗伟,徐明玉.湿法超声机械镀锌-铝层的结构分析[J].电镀与精饰,2014,36(10):5-8. 被引量:2
8张林,刘欣,彭道衡.热锻模型腔整体焊接修复的工艺研究[J].现代焊接,2016,0(10):54-58.
9杨永顺,宁晓兵,杨茜,陈超群.基于正交试验法的铝基复合材料制备工艺研究[J].热加工工艺,2013,42(8):121-124. 被引量:4
10杨振国,朱基木,吴连生,金忠(告羽),陈天岭.二次过热器炉管的腐蚀损伤分析与表征[J].腐蚀与防护,2004,25(2):87-90. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TG132.5[一般工业技术—材料科学与工程]
Citation Information:
Aluminum-based composite photocatalyst was prepared by coating flake aluminum powders with TiO2 and using sol-gel method.The influences of technological parameters on the photocatalysis property were studied by orthogonal experiments.The samples were analyzed and characterized by XRD.The results show that the photocatalysis property is significantly affected by calcination temperature.The degradation rate of methylene blue is up to 93.5% through 3 h UV-lamp irradiation when hydrolysis temperature is 30 ℃,pH value 4.5,molar ratio of water to tetrabutyl titanate 50,and calcination temperature 600 ℃.
quote
| GB/T 7714-2015 | [1] LU Shuang, YE Hong-qi, GAO Ying, et al. Orthogonal Design to Optimize the Technological Parameters of Preparing Aluminum-based Composite Photocatalyst[J]. Rare Metals and Cemented Carbides, 2010(3): 9-12. |
| MLA | [1] LU Shuang, et al., "Orthogonal Design to Optimize the Technological Parameters of Preparing Aluminum-based Composite Photocatalyst." Rare Metals and Cemented Carbides, no. 3, 2010, pp. 9-12. |
| APA | [1] LU Shuang, YE Hong-qi, GAO Ying, & HAN Kai. (2010). Orthogonal Design to Optimize the Technological Parameters of Preparing Aluminum-based Composite Photocatalyst. Rare Metals and Cemented Carbides(3), 9-12. |
| IEEE | [1] LU Shuang, YE Hong-qi, GAO Ying, and HAN Kai, "Orthogonal Design to Optimize the Technological Parameters of Preparing Aluminum-based Composite Photocatalyst," Rare Metals and Cemented Carbides, no. 3, pp. 9-12, 2010. keywords: {aluminum-based composite photocatalyst;flake aluminum powder;TiO2;sol-gel method;coating;orthogonal experiment} |