Abstract AITranslate
The influences of extractant saponification value,solution acidity and Al concentration on the distribution ratio and separation factor of RE and Al in the chloronaphthenic acid system were studied.The results show that in the feed solution with high Al concentration,RE is separated effectively from Al by the above extraction system even under high solution acidity,where no emulsification occurs in the extraction process.And the optimal technological parameters of the extraction separation process are as follows:extractant saponification value 0.35 mol/L,Al concentration 12.5 mmol/L and pH=0.10.Under the above conditions,the distribution ratios of Al and RE are 0.53 and 0.05,respectively,and the separation factor of RE and Al is up to 10.6.
KeyWords AITranslate
1贾江涛,廖春生,严纯华,曾东海,冯余清,周静,田北超.萃取法Ca/La在线分离工艺[J].稀土,1999,20(4):12-15. 被引量:15
2严纯华,张亚文,廖春生.萃取法稀土料液浓缩技术[P].CN 1129256A,1996.
3李永绣,何小彬,辜子英,胡平贵.RECl_3与NH_4HCO_3的沉淀反应及伴生杂质的共沉淀行为[J].稀土,1999,20(2):19-22. 被引量:31
4曾天元.关于我国稀土提取分离的进展、存在问题和改进途径初探[J].有色冶炼,1996,25(4):13-18. 被引量:12
5袁承业.稀土萃取剂的化学结构与性能问题.科学通报,1977,22(11):465-479.
1李治国,柳召刚,孙祥.混合稀土料液中环烷酸萃取分离稀土和铝的研究[J].有色金属:冶炼部分,2019,0(11):38-41. 被引量:4
1种轲李尧,朱炳龙,余人杰,童霏,秦恒飞,潘君丽,周全法.用微乳液从废催化剂浸出液中分离铝[J].湿法冶金,2021,40(1):20-25.
2孙亮,李玉虎,宋健清,张敏.焙烧制度对稀土精矿中铁、铝等杂质浸出行为的影响[J].有色金属科学与工程,2021,12(4):27-32. 被引量:1
3蓝桥发,邱小英,柯兆华,黄金.萃淋树脂法制备超高纯氯化钕工艺研究[J].有色金属:冶炼部分,2021(10):42-49.
4杨少波.一种新型萃取剂在稀土料液除铝铁中的应用[J].福建冶金,2023,52(1):30-33.
1曾青云,曾清全,常卿卿.环烷酸体系萃取分离稀土和铝的实验研究[J].有色金属科学与工程,2012,3(2):17-19. 被引量:7
2李剑虹,张兴.环烷酸改性合成氯代环烷酸萃取体系分离稀土和铝的红外光谱分析[J].有色金属,2011,63(2):305-307. 被引量:2
3李洪桂,赵中伟.钨冶金强碱性阴离子交换过程的某些问题的理论分析[J].中国钨业,2010,25(5):35-39. 被引量:3
4张兴.稀土和铝在皂化氯代环烷酸体系中分配比及分离系数的研究[J].稀土,2011,32(2):93-97. 被引量:2
5周嘉郁,张一敏,包申旭,段继华.电容去离子技术分离石煤酸浸液中的钒和铝[J].有色金属:冶炼部分,2016(8):43-47.
6穆光杰.N503串级萃取分离Ga、In[J].稀有金属,1991,15(1):13-17. 被引量:1
7杨学民,刘越生.论炼钢过程中的泡沫化和乳化现象[J].炼钢,1993,9(6):40-45. 被引量:5
8李庸华,郭锦勇,等.D999系列新功能树脂分离铂铼的研究[J].有色金属,2002,54(B07):109-113. 被引量:1
9王新成.70t电炉泡沫渣工艺技术的改进[J].工业加热,2006,35(1):53-55.
10成本诚,洪涌.α-氯代羧酸对某些金属的萃取[J].中国有色金属学报,1993,3(3):38-42.
Basic Information:
DOI:
Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]
Citation Information:
The influences of extractant saponification value,solution acidity and Al concentration on the distribution ratio and separation factor of RE and Al in the chloronaphthenic acid system were studied.The results show that in the feed solution with high Al concentration,RE is separated effectively from Al by the above extraction system even under high solution acidity,where no emulsification occurs in the extraction process.And the optimal technological parameters of the extraction separation process are as follows:extractant saponification value 0.35 mol/L,Al concentration 12.5 mmol/L and pH=0.10.Under the above conditions,the distribution ratios of Al and RE are 0.53 and 0.05,respectively,and the separation factor of RE and Al is up to 10.6.
quote
| GB/T 7714-2015 | [1] LI Jian-hong, ZHANG Xing, XU Ying, et al. Research on the Distribution Ratio and Separation Factor of Rare Earth and Aluminium in Chloronaphthenic Acid Extraction System[J]. Rare Metals and Cemented Carbides, 2010(3): 5-8. |
| MLA | [1] LI Jian-hong, et al., "Research on the Distribution Ratio and Separation Factor of Rare Earth and Aluminium in Chloronaphthenic Acid Extraction System." Rare Metals and Cemented Carbides, no. 3, 2010, pp. 5-8. |
| APA | [1] LI Jian-hong, ZHANG Xing, XU Ying, & WU Wen-yuan. (2010). Research on the Distribution Ratio and Separation Factor of Rare Earth and Aluminium in Chloronaphthenic Acid Extraction System. Rare Metals and Cemented Carbides(3), 5-8. |
| IEEE | [1] LI Jian-hong, ZHANG Xing, XU Ying, and WU Wen-yuan, "Research on the Distribution Ratio and Separation Factor of Rare Earth and Aluminium in Chloronaphthenic Acid Extraction System," Rare Metals and Cemented Carbides, no. 3, pp. 5-8, 2010. keywords: {chloronaphthenic acid;extraction separation;rare earth;aluminum;distribution ratio;separation factor} |