Study on Preparation of Thicker 93W-4.9Ni-2.1Fe Tungsten Heavy Alloy Sheets by Powder Rolling-Stacking Sintering AITranslate

School of Materials Engineering, Nanjing Institute of Technology;School of Materials Engineering, Nanjing Institute of Technology;School of Materials Engineering, Nanjing Institute of Technology;School of Materials Engineering, Nanjing Institute of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The thicker 93W-4.9Ni-2.1Fe tungsten heavy alloy sheets were prepared by powder rolling-stacking sintering. The comparison of microstructure and properties was conducted between single sintered tungsten alloy sheets and stacking sintered ones (i. e. thicker tungsten alloy sheets),and the influences of cold-rolling on microstructure and properties of stacking sintered alloy sheets were studied. The results show that the thicker tungsten heavy alloy sheets can be prepared with homogeneous microstructure and well combined layers by powder rolling-stacking sintering, and their relative density, hardness and tensile strength are comparable with those of single sintered alloy sheets. Moreover,the mechanical properties of stacking sintered alloy sheets are improved significantly by cold-rolling. Therefore, powder rolling-stacking sintering is effective for preparation of the thicker tungsten heavy alloy sheets.

KeyWords AITranslate

thicker tungsten heavy alloy sheet powder rolling stacking sintering microstructure mechanical property

1周伟,高翔,周永贵,罗丰华.95W-5(Ni/Fe)合金的延、脆性断裂行为及热处理影响[J].粉末冶金材料科学与工程,2010,15(2):141-144. 被引量:3

2刘桂荣,王玲,王广达,杨海兵.钨合金轧制变形强化的组织与性能研究[J].兵器材料科学与工程,2010,33(5):39-41. 被引量:13

3范景莲,刘涛,彭石高,祁美贵,田家敏.稀土Y在90W-7Ni-3Fe合金中的存在形态和分布特征[J].稀有金属材料与工程,2011,40(8):1438-1441. 被引量:4

4刘书祯,李杰,程艳明.微波加热在钨工业中的应用现状[J].稀有金属与硬质合金,2012,40(1):51-54. 被引量:3

5Liu W, Ma Y,Zhang J. Properties and microstructural e volution of W-Ni-Fe alloy via microwave sintering[J] International Journal of Refractory Metals and Hard Ma lerials, 2012,35 : 138-142.

6Xiang D, Ding I., Li Y,et a l. Microstructure and mechan- ical properties of fine-grained W-7Ni-3Fe heavy alloy by spark plasma s!ntering [J ]. Materials Science and Engineering A, 2012,551 = 95-99.

7Hu K,Li X,Yang C,et al. Densification and microstru- cture evolution during SPS consolidation process in W- Ni-Fe system[J]. Transactions of Nonferrous Metals Society of China,2011,21:493- 501.

8Chanadee T, Niyomwas S, Wannasin J. Novel synthesis of tungsten alloys from metal oxide by self propagating high temperature synthesis reaction[J]. Procedia Engin- eering, 2012,32 : 628-634.

9范景莲.钨合金及其制备新技术[M].北京:冶金工业出版社,2007.

10肖海滨,陈玉华,张晓燕,朱玉斌.W-Ni-Fe高比重合金板材冷轧变形行为及其显微组织特征研究[J].稀有金属,2007,31(4):425-429. 被引量:8

1孙文,章晓波.高密度钨合金烧结新工艺研究现状[J].稀有金属与硬质合金,2014,42(2):36-40. 被引量:3

2武杰,孙毅,王晖.烧结和热处理对WNiFe合金板材轧制性能的影响[J].热加工工艺,2016,45(20):239-241. 被引量:2

3崔利群,韩胜利,施麒,李达人,胡建召,刘祖岩.钨铜粉末轧制的有限元模拟研究[J].粉末冶金材料科学与工程,2019,24(5):406-412. 被引量:1

1邹树梁,颜亮,唐德文,谢宇鹏,张德.高密度W-Ni-Fe合金制备与应用研究进展[J].南华大学学报:自然科学版,2015,29(1):53-59. 被引量:3

2武杰,孙毅,王晖.烧结和热处理对WNiFe合金板材轧制性能的影响[J].热加工工艺,2016,45(20):239-241. 被引量:2

3田野,孙大智,李萍,梁辰,华睿.高压扭转对难熔金属粉末钨致密固结及强韧化的影响研究[J].稀有金属与硬质合金,2016,44(5):37-42. 被引量:1

4张浩,石科学,郑晓斐.高密度钨合金部件断裂失效分析[J].铸造技术,2020,41(6):557-559.

5张俊,杨晓青,李志翔.钨粉粒度和烧结温度对添加La_(2)O_(3)的钨合金性能和组织的影响[J].稀有金属与硬质合金,2021,49(2):24-28. 被引量:1

6王苗,李荣,曹卜元,任尚远,刘高建.粉末轧制成形技术研究进展[J].粉末冶金工业,2023,33(2):103-108.

1林永新.粉末轧制钛板的工业生产[J].钛工业进展,1994(4):6-6.

2张忠伟,汪凌云,黄光胜,牛禧.金属带材粉末轧制的研究[J].轻合金加工技术,2005,33(4):40-43. 被引量:6

3王东玺.粉末轧制成型技术的研究[J].黑龙江科技信息,2011(19):64-64. 被引量:1

4崔利群,李达人,韩胜利.辊缝与轧制速度对粉末轧制钛铝多孔板性能的影响[J].材料导报:纳米与新材料专辑,2016,30(2):568-570. 被引量:2

5王兴庆,吕海波.粉末冶金法制取Fe-Al金属间化合物的研究[J].上海大学学报:自然科学版,2000,6(6):511-515. 被引量:11

6许光明,王哲锋,崔建忠.铝锡合金电磁搅拌中电磁场的模拟分析[J].材料导报,2003,17(1):66-68. 被引量:1

7刘明俊,夏伟,周照耀.一种基于数值模拟的金属粉末轧制力能参数计算方法[J].现代制造工程,2012(11):58-62. 被引量:3

8姚志涛,王迎春,程兴旺,李树奎,王富耻.Y_2O_3对93W-4.9Ni-2.1Fe合金力学性能及断裂过程的影响[J].兵器材料科学与工程,2008,31(3):45-47.

9孙文,章晓波.高密度钨合金烧结新工艺研究现状[J].稀有金属与硬质合金,2014,42(2):36-40. 被引量:3

10于洋,王尔德,胡连喜,张宝友,于杰.形变强化对93W-4.9Ni-2.1Fe合金组织及性能的影响[J].材料科学与工艺,2005,13(4):442-444. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

The thicker 93W-4.9Ni-2.1Fe tungsten heavy alloy sheets were prepared by powder rolling-stacking sintering. The comparison of microstructure and properties was conducted between single sintered tungsten alloy sheets and stacking sintered ones (i. e. thicker tungsten alloy sheets),and the influences of cold-rolling on microstructure and properties of stacking sintered alloy sheets were studied. The results show that the thicker tungsten heavy alloy sheets can be prepared with homogeneous microstructure and well combined layers by powder rolling-stacking sintering, and their relative density, hardness and tensile strength are comparable with those of single sintered alloy sheets. Moreover,the mechanical properties of stacking sintered alloy sheets are improved significantly by cold-rolling. Therefore, powder rolling-stacking sintering is effective for preparation of the thicker tungsten heavy alloy sheets.

quote

GB/T 7714-2015 [1] ZHANG Xiao-bo, SUN Wen, CHEN Yong-ming, et al. Study on Preparation of Thicker 93W-4.9Ni-2.1Fe Tungsten Heavy Alloy Sheets by Powder Rolling-Stacking Sintering[J]. Rare Metals and Cemented Carbides, 2013(5): 28-31.
MLA [1] ZHANG Xiao-bo, et al., "Study on Preparation of Thicker 93W-4.9Ni-2.1Fe Tungsten Heavy Alloy Sheets by Powder Rolling-Stacking Sintering." Rare Metals and Cemented Carbides, no. 5, 2013, pp. 28-31.
APA [1] ZHANG Xiao-bo, SUN Wen, CHEN Yong-ming, & SHEN Chong. (2013). Study on Preparation of Thicker 93W-4.9Ni-2.1Fe Tungsten Heavy Alloy Sheets by Powder Rolling-Stacking Sintering. Rare Metals and Cemented Carbides(5), 28-31.
IEEE [1] ZHANG Xiao-bo, SUN Wen, CHEN Yong-ming, and SHEN Chong, "Study on Preparation of Thicker 93W-4.9Ni-2.1Fe Tungsten Heavy Alloy Sheets by Powder Rolling-Stacking Sintering," Rare Metals and Cemented Carbides, no. 5, pp. 28-31, 2013. keywords: {thicker tungsten heavy alloy sheet;powder rolling;stacking sintering;microstructure;mechanical property}