Yttrium aluminum garnet (YAG) ceramic fibers were prepared by sol-gel with aluminum chloride,aluminum powder,yttrium oxide and acetic acid as raw materials. Boric acid was added into YAG precursor sol to study the effects of boric acid on the spinnability of sol,and crystallization temperature and microstructure of YAG fibers. The results indicate that addition of boric acid has no effect on the sol spinnability. Upon 2 h calcination at 1 000 ℃ ,YAG gel fibers are fully crystallized into YAG. The addition of boric acid can improve the fiber crystallization and decrease the crystallization temperature. Larger grains and intergranular voids can be observed on the surface of the fibers with boric acid.
KeyWords AITranslate
1谭宏斌,张伟,郭从盛.溶胶-凝胶法制备钇铝石榴石纤维[J].有色金属:冶炼部分,2011(3):39-41. 被引量:7
2谭宏斌,袁新强,付蕾.钇铝石榴石纤维的应用与制备[J].中国陶瓷,2011,47(4):17-20. 被引量:4
3谭毅.钇铝石榴石长纤维制备研究[J].中国陶瓷,2011,47(5):28-29. 被引量:3
4Shojaie-Bahaabad M, Taheri-Nassaj E, Naghizadeh R. An alumina-YAG nanostructured fiber prepared from an a- queous sol-gel precursor : preparation, rheological beha vior and spinnability[J]. Ceramics International, 2008,34 (8):1 893-1 902.
1谭毅.钇铝石榴石长纤维制备研究[J].中国陶瓷,2011,47(5):28-29. 被引量:3
2李呈顺,张玉军,张景德,龚红宇.溶胶–凝胶法制备多晶钇铝石榴石纤维[J].硅酸盐学报,2009,37(7):1165-1170. 被引量:6
3李呈顺,张玉军,张景德,龚红宇.钇铝石榴石纤维的制备和应用研究进展[J].硅酸盐通报,2009,28(1):132-137. 被引量:10
4黄剑清,潘安健.硼改性酚醛泡沫的耐高温性能[J].玻璃钢/复合材料,2007(6):26-28. 被引量:16
5吴建亭.高强高模聚乙烯醇纤维的生产工艺初探[J].维纶通讯,2011,31(2):22-23.
6李欣达,兰嫒,唐静文,杨燕平,何小云,陆帅羽,张玥,余木火.DMSO/离子液体复合溶剂湿法纺丝制备纤维素纤维的凝固条件[J].材料科学与工程学报,2015,33(4):474-478. 被引量:3
7吴建亭.高强高模聚乙烯醇纤维的生产工艺初探[J].合成纤维工业,2010,33(5):54-55. 被引量:4
8潘雯.建筑保温材料用酚醛泡沫的改性与性能[J].工程塑料应用,2016,44(9):100-103. 被引量:2
9戚发金,朱宪忠,王苏,王海波.气相法制备优质白光LED用YAG荧光粉[J].中国照明电器,2005(4):1-3. 被引量:1
10王思齐,马海燕,陆烨邦,赵化祎.冷却速率对聚合物熔纺纤维结构及性能的影响[J].纺织导报,2017,0(1):51-53. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TQ343.41[化学工程—化纤工业]
Citation Information:
Yttrium aluminum garnet (YAG) ceramic fibers were prepared by sol-gel with aluminum chloride,aluminum powder,yttrium oxide and acetic acid as raw materials. Boric acid was added into YAG precursor sol to study the effects of boric acid on the spinnability of sol,and crystallization temperature and microstructure of YAG fibers. The results indicate that addition of boric acid has no effect on the sol spinnability. Upon 2 h calcination at 1 000 ℃ ,YAG gel fibers are fully crystallized into YAG. The addition of boric acid can improve the fiber crystallization and decrease the crystallization temperature. Larger grains and intergranular voids can be observed on the surface of the fibers with boric acid.
quote
| GB/T 7714-2015 | [1] TAN Hong-bin. Effects of Boric Acid Addition on Microstructure of Yttrium Aluminum Garnet[J]. Rare Metals and Cemented Carbides, 2013(5): 25-27. |
| MLA | [1] TAN Hong-bin. "Effects of Boric Acid Addition on Microstructure of Yttrium Aluminum Garnet." Rare Metals and Cemented Carbides, no. 5, 2013, pp. 25-27. |
| APA | [1] TAN Hong-bin. (2013). Effects of Boric Acid Addition on Microstructure of Yttrium Aluminum Garnet. Rare Metals and Cemented Carbides(5), 25-27. |
| IEEE | [1] TAN Hong-bin, "Effects of Boric Acid Addition on Microstructure of Yttrium Aluminum Garnet," Rare Metals and Cemented Carbides, no. 5, pp. 25-27, 2013. keywords: {yttrium aluminum garnet fiber;sol-gel;boric acid;spinnability;crystallization temperature;microstructure} |